Forging method for high-silver aluminum alloy and high-silver aluminum alloy forged part
Abstract
Disclosed is a forging method for a high-silver aluminum alloy and a high-silver aluminum alloy forged part are provided. The forging method comprises the following steps: heating the high-silver aluminum alloy to 440° C. to 500° C., and holding for 8 to 16 hours to obtain a blank; preheating a contact portion of a forging anvil, a tong or a die with the blank to 300° C. to 480° C., and holding in the process of transferring the blank to a press; carrying out six-upsetting six-stretching multidirectional forging deformation on the blank, thus obtaining a forging blank, wherein the final forging temperature is 360° C. to 400° C.; and carrying out forming forging treatment on the forging blank, and then carrying out solid solution treatment, residual stress elimination and artificial aging treatment in sequence.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (4)
Non-Patent Literature (3)
- English translation of CN 104015011 (originally published September 3, 2014), obtained from PE2E search.
- English translation of CN 110434264 (originally published November 12, 2019), obtained from PE2E search.
- English translation of CN 115608897 (originally published January 17, 2023), obtained from PE2E search.