Production method of antireflection film, antireflection film and coating composition
Abstract
A production method of an antireflection film comprises, in order, a step of applying a coating composition obtained by mixing the following components (A) to (D) on a base material to form a coating film, a step of drying the coating film to volatilize the solvent therefrom, and a step of curing the coating film to form a cured layer, wherein a multilayer structure having different refractive indexes is formed from the coating composition: (A) a compound having at least one structure selected from a fluorine-containing hydrocarbon structure and a polysiloxane structure and at least one basic functional group, (B) an inorganic fine particle, (C) a curable binder containing no fluorine atom in the molecule, and (D) a solvent, provided that the mass ratio of [component (A)+component (B)]/[component (C)] is from 1/199 to 60/40.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| CN 106,459,320 A | Low volatile organic compound-containing polymers with release properties | — | 0 |