US 2003201263 A1#15205407 Most CitedPendingUnited States (USPTO)Application

Welding material and a method of producing welded joint

7Forward Citations (#15205407 Global)
0.3/yrCitation Velocity (#25530063 Global)
1.78Citation PageRank (#17436741 Global)
7Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

In the present invention, an iron based alloy which contains by mass %: 0.20% or less of C; 6.0 to 16.0% of Cr; 6.0 to 16.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 0-170° C., inclusive of 0° C. and exclusive of 170° C., is used as a welding material. With respect to a weld metal, the weld metal has a iron alloy composition which contains by mass %: 0.20% or less of C; 3.0 to 13.0% of Cr; 3.0 to 13.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 50-360° C., inclusive of both 50° C. and 360° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 7.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗