US 2002176984 A1#36980673 Most CitedPendingUnited States (USPTO)Application
Silicon penetration device with increased fracture toughness and method of fabrication
2Forward Citations (#36980673 Global)
0.1/yrCitation Velocity (#48389583 Global)
1.13Citation PageRank (#35065615 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets
Abstract
A silicon penetration device with increased fracture toughness and method of fabrication thereof are provided. The method comprises strengthening silicon penetration devices by thermally growing a silicon oxide layer on the penetration device and then subsequently stripping the silicon oxide. The method also includes strengthening silicon penetration devices through the sputtering of thin film coatings on the silicon penetration devices.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.