Control of amount and uniformity of oxidation at the interface of an emitter region of a monocrystalline silicon wafer and a polysilicon layer formed by chemical vapor deposition
Abstract
A method of controlling the quantity and uniformity of distribution of bonded oxygen atoms at the interface between the polysilicon and the monocrystalline silicon includes carrying out, after having loaded the wafer inside the heated chamber of the reactor and evacuated the chamber of the LPCVD reactor under nitrogen atmosphere, a treatment of the wafer with hydrogen at a temperature generally between 500 and 1200° C. and at a vacuum generally between 0.1 Pa and 60000 Pa. The treatment is performed at a time generally between 0.1 and 120 minutes, to remove any and all the oxygen that may have combined with the silicon on the surface of the monocrystalline silicon during the loading inside the heated chamber of the reactor even if it is done under a nitrogen flux. After such a hydrogen treatment, another treatment is carried out substantially under the same vacuum conditions and at a temperature generally between 700 and 1000° C. with nitrogen protoxide (N 2 O) for a time generally between 0.1 and 120 minutes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.