Method for producing cathode active material and method for manufacturing nonaqueous electrolyte battery
Abstract
A method for producing a cathode active material which produces a spinel type lithium manganese oxide expressed by a general formula: Li 1+x Mn 2−x−y Me y PO 4 , as the cathode active material, (here, x is expressed by a relation of 0≦x≦0.15 and y is expressed by a relation of 0<y<0.3, and Me is at least one kind of element selected from between Co, Ni, Fe, Cr, Mg and Al). The method comprises a mixing step of mixing raw materials of the spinel type lithium manganese oxide to obtain a precursor; and a sintering step of sintering the precursor obtained in the mixing step to obtain the spinel type lithium manganese oxide. The sintering temperature in the sintering step is located within a range of 800° C. or higher and 900° C. or lower. Accordingly. even when manganese which is inexpensive and abundant in resources is employed as a main material, an excellent cathode performance can be maintained under the environment.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 16.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗