Non-oriented electrical steel sheet and motor core comprising same
Abstract
A non-oriented electrical steel sheet includes a steel sheet base material and an insulation film on the steel sheet base material. The steel sheet base material includes, by wt %, 2.0 to 6.5% Si, 0.1 to 1.3% Al, 0.3 to 2.0% Mn, more than 0 to 0.03% Sn, more than 0 to 0.02% Sb, and a balance of Fe and inevitable impurities, and satisfies Formula 1: 0.030 ≥ [Sn]+[Sb] ≥ 0.005. The non-oriented electrical steel sheet satisfies Formula 2: 0.1 ≥ [Mn film]/[Mn50] before stress relief annealing and Formula 3: 10 ≥ [Mn film]/[Mn50] ≥ 1 after stress relief annealing, wherein [Sn] and [Sb] are contents, in wt %, of Sn and Sb, [Mn film] is an average Mn amount in the insulation film, and [Mn50] is a Mn amount at a depth of 50 μ m from an interface toward an inside of the steel sheet base material.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 0.
Claims (15 — 3 Independent, 12 Dependent)
- Claim 1Independent Claim
A non-oriented electrical steel sheet comprising: a steel sheet base material which includes, by weight: 2.0 to 6.5% of Si, 0.1 to 1.3% of Al, 0.3 to 2.0% of Mn, more than 0 to 0.03% or less of Sn, and more than 0 to 0.02% or less of Sb, with a balance of Fe and other inevitable impurities and satisfies the following Formula 1, and an insulating coating film positioned on the steel sheet base material, wherein the non-oriented electrical steel sheet satisfies the following Formula 2 before stress relief annealing and satisfies the following Formula 3 after stress relief annealing: 0.03 ≥ [Sn] + [Sb] ≥ 0.005 [Formula 1] 0.1 ≥ [Mn coating film] / [Mn 50] [Formula 2] 10 ≥ [Mn coating film] / [Mn 50] ≥ 1 [Formula 3] wherein [Sn] and [Sb] are contents, in wt %, of Sn and Sb, respectively, [Mn coating film] is an average Mn content, in wt %, in the insulating coating film, and [Mn50] is a Mn content, in wt %, at a depth of 50 μ m from an interface between the steel sheet base material and the insulating coating film toward an inside of the steel sheet base material.
- Claim 2Depends on #1
The non-oriented electrical steel sheet of claim 1, wherein: the steel sheet base material further includes 0.005 wt % or less of one or more of C, N, S, Ti, Nb, and V.
- Claim 3Depends on #1
The non-oriented electrical steel sheet of claim 1, wherein: the steel sheet base material further includes one or more of 0.01 to 0.2 wt % of Cu, 0.100 wt % or less of P, 0.002 wt % or less of B, 0.01 wt % or less of Mo, 0.005 wt % or less of Mg, and 0.005 wt % or less of Zr.
- Claim 4Depends on #1
The non-oriented electrical steel sheet of claim 1, wherein: an average crystal grain particle diameter before the stress relief annealing is 60 μ m or less.
- Claim 5Depends on #1
The non-oriented electrical steel sheet of claim 1, wherein: iron loss W10/800, in W/kg, after the stress relief annealing satisfies the following Formula 4: W 10 / 800 ≤ 25 + 60 × t [Formula 4] wherein t is a thickness, in mm, of the steel sheet.
- Claim 6Depends on #1
The non-oriented electrical steel sheet of claim 1, wherein: the stress relief annealing is performed at a temperature of 800 ° C to 900 ° C under an atmosphere which includes one or more of nitrogen, hydrogen, and carbon monoxide and has a dew point of 0 ° C or lower.
- Claim 7Independent Claim
A method for manufacturing a non-oriented electrical steel sheet, the method comprising: hot rolling a slab which includes, by weight: 2.0 to 6.5% of Si, 0.1 to 1.3% of Al, 0.3 to 2.0% of Mn, more than 0 to 0.03% or less of Sn, and more than 0 to 0.02% or less of Sb, with a balance of Fe and other inevitable impurities and satisfies the following Formula 1, thereby manufacturing a hot rolled sheet; removing scale present on a surface of the hot rolled sheet; cold rolling the descaled hot rolled sheet to manufacture a cold rolled sheet; and annealing the cold rolled sheet, wherein the removing of scale includes projecting shot balls in an amount of 15 to 35 kg per minute per m 2 onto the steel sheet to remove scale: 0.03 ≥ [Sn] + [Sb] ≥ 0.005 [Formula 1] wherein [Sn] and [Sb] are contents, in wt %, of Sn and Sb, respectively.
- Claim 8Depends on #7
The method for manufacturing a non-oriented electrical steel sheet of claim 7, wherein: the shot balls have an average particle size of 0.1 to 1 mm and are projected for 1 to 60 seconds.
- Claim 9Depends on #7
The method for manufacturing a non-oriented electrical steel sheet of claim 7, wherein: a material of the shot balls is an Fe-based alloy.
- Claim 10Depends on #7
The method for manufacturing a non-oriented electrical steel sheet of claim 7, wherein: the annealing of the cold rolled sheet is performed at a temperature of 700 to 1100 ° C for 10 to 1000 seconds.
- Claim 11Depends on #7
The method for manufacturing a non-oriented electrical steel sheet of claim 7, further comprising: annealing the hot rolled sheet, before the removing of scale.
- Claim 12Depends on #7
The method for manufacturing a non-oriented electrical steel sheet of claim 7, further comprising: performing stress relief annealing, after the annealing of the cold rolled sheet.
- Claim 13Independent Claim
A motor core comprising: a rotor formed by laminating a plurality of non-oriented electrical steel sheets and a stator formed by laminating a plurality of non-oriented electrical steel sheets, wherein the non-oriented electrical steel sheet in the rotor includes, by weight: 2.0 to 6.5% of Si, 0.1 to 1.3% of Al, 0.3 to 2.0% of Mn, more than 0 to 0.03% or less of Sn, and more than 0 to 0.02% or less of Sb, with a balance of Fe and other inevitable impurities, and satisfies the following Formulae 1 and 2, and the non-oriented electrical steel sheet in the stator includes, by weight: 2.0 to 6.5% of Si, 0.1 to 1.3% of Al, 0.3 to 2.0% of Mn, more than 0 to 0.03% or less of Sn, and more than 0 to 0.02% or less of Sb, with a balance of Fe and other inevitable impurities, and satisfies the following Formulae 1 to 3: 0.03 ≥ [Sn] + [Sb] ≥ 0.005 [Formula 1] 0.1 ≥ [Mn coating film] / [Mn 50] [Formula 2] 10 ≥ [Mn coating film] / [Mn 50] ≥ 1 [Formula 3] wherein [Sn] and [Sb] are contents of Sn and Sb, respectively, [Mn coating film] is an average Mn content, in wt %, in the insulating coating film, and [Mn50] is a Mn content, in wt %, at a depth of 50 μ m from the interface between the steel sheet base material and the insulating coating film toward an inside of the steel sheet base material.
- Claim 14Depends on #13
The motor core of claim 13, wherein: the non-oriented electrical steel sheets included in the stator and the rotor are derived from the same coil.
- Claim 15Depends on #13
The motor core of claim 13, wherein: a difference in contents of Si, Al, and Mn between the non-oriented electrical steel sheets included in the stator and the rotor is 0.20 wt % or less.
Technical Overview & Description
CROSS-REFERENCE OF RELATED APPLICATIONS This application is the U.S. National Phase under 35 U.S.C. § 371 of International Patent Application No. PCT/KR2022/020963, filed on Dec. 21, 2022, which in turn claims the benefit of Korean Application No. 10-2021-0184608, filed on Dec. 22, 2021, the disclosures of which applications are incorporated by reference herein. TECHNICAL FIELD An embodiment of the present disclosure relates to a non-oriented electrical steel sheet and a motor core including the same. Specifically, an embodiment of the present disclosure relates to a non-oriented electrical steel sheet which has improved adhesiveness of an insulating coating film by appropriately adjusting contents of Sn and Sb and increasing a shot ball projection amount when removing scale to prevent Mn diffusion into an insulating coating film during stress relief annealing, and a motor core including the same. BACKGROUND ART A non-oriented electrical steel sheet is mainly used in a motor which converts electrical energy into mechanical energy, and in order to exhibit high efficiency in this process, the non-oriented electrical steel sheet is required to have excellent magnetic properties. In particular, in recent years, as environmentally-friendly technology has been gaining attention, it is considered to be very important to increase the efficiency of motors, which accounts for more than a half of total electrical energy consumption, and to this end, the demand for a non-oriented electrical steel sheet having excellent magnetic properties is also increasing. The magnetic properties of the non-oriented electrical steel sheet is mainly evaluated by iron loss and magnetic flux density. Iron loss refers to energy loss occurring at certain magnetic flux density and frequency, and magnetic flux density refers to a magnetization degree obtained under the certain magnetic field. As the iron loss is lower, a motor having higher energy efficiency may be manufactured under the same condit
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (22)
Non-Patent Literature (3)
- Japanese Office Action dated Sep. 30, 2025 issued in Japanese Patent Application No. 2024-538215.
- The Extended European Search Report dated Sep. 29, 2025 issued in European Patent Application No. 22911927.6.
- International Search Report and Written Opinion dated Mar. 24, 2023 issued in International Patent Application No. PCT/KR2022/020963 (with English translation).