Prestressing a flat glass by generating a gradient in the surface composition
Abstract
The invention relates to glass articles, in particular flat glasses, in the case of which the surface material has gradient material properties as a result of targeted process control which in turn lead to compressive prestressing of the surface. The invention also relates to a method for producing the glass articles and the use thereof.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.
Claims (20 — 3 Independent, 17 Dependent)
- Claim 1Independent Claim
A glass article, comprising: three portions comprising an upper side surface glass, a core glass, and an underside surface glass, the upper side surface glass and the underside surface glass being present in each case to a depth of < 20 nm and the core glass is present in any event at 500 nm depth, a sum of proportions of tin oxide and bismuth oxide in the underside surface glass is greater than a sum of proportions of tin oxide and bismuth oxide in the upper side surface glass, the core glass having a CTE K calculated according to the following general formulas (13) and (14a) in a range from 2.5 to 5.0 ppm/K: E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ i = 1 m z i, j, (13) CTE K = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 a) CTE o = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 b) wherein m is a number of cation types which occur, E pot,j, is a potential well depth tabulated for a j th cation type, and z j,I is a number of cations of the j th type in i th constituent phase; the upper side surface glass having a CTE O that is calculated according to the formula (14b) for the upper side surface glass and the following formulas (15) and (16) which is lower by at least 0.6 ppm/K in comparison with the CTE K of the core glass calculated according to the formulas (13) and (14a): E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ j = 1 m z i, j = ∑ j = 1 m (∑ i = 1 n c i · z i, j) · E pot, j ∑ j = 1 m (∑ i = 1 n c i · z i, j), (15) ∑ i = 1 n c i · z i, j = k j · x j; (16) and wherein according to the following formula (10) a compressive prestress σ O on the upper side surface of at least 50 MPa is produced when the values of the core glass calculated according to the following formulas (31), (29), and (37) are used for E/(1 − μ) and T G and a difference CTE K − CTE O between the CTE values calculated for core glass and upper side surface glass is used for Δ CTE: σ O = E 1 - μ · (T G - T ambient) · Δ CTE, (10) μ = 0.17 + Δ μ f + Δ μ χ, (29) E = (0.683888667 (2 · (1 + μ) · f · E pot _ · z V m o l) - 39.4242404) GPa, (31) 1 V A - T G = (0.002665819 · f W + 0.001119212) · 1 K, (37) wherein T G is an annealing point of the glass, VA is a working point of the glass, E is a modulus of elasticity of the glass, μ is Poisson's ratio of the glass, T ambient is an ambient temperature, Δ μ f = - [(1 + μ) (1 - 2 μ) 3 1 f] Δ f, and f = Angle condition number p. A. - (2 3) (3 D angle degrees of freedom number p. A. - angle degrees of freedom number p. A.) Angle condition number p. A..
- Claim 2Depends on #1
The glass article of claim 1, wherein the core glass has a composition which is characterized by a system of constituent phases which comprises the constituent phase reedmergnerite in a proportion of 10 to 50 mol %, the constituent phase potassium reedmergnerite in a proportion of 0 to 30 mol %, the constituent phase anorthite in a proportion of 0 to 20 mol %, the constituent phase diboron trioxide in a proportion of 0 to 20 mol %, and the constituent phase silicon dioxide in a proportion of 20 to 75 mol %.
- Claim 3Depends on #2
The glass article of claim 2, wherein the composition of the core glass is characterized by the following constituent phases: Constituent phase Min (mol %) Max (mol %) Reedmergnerite 10 50 Potassium reedmergnerite 0 30 Cordierite 0 20 Anorthite 0 20 Diopside 0 20 Diboron trioxide 0 20 Silicon dioxide 20 75.
- Claim 4Depends on #2
The glass article of claim 2, wherein the composition of the core glass is characterized by the following constituent phases: Constituent phase Min (mol %) Max (mol %) Reedmergnerite 10 50 Potassium reedmergnerite 0 30 Albite 0 50 Anorthite 0 20 Diboron trioxide 0 20 Silicon dioxide 20 75.
- Claim 5Depends on #2
The glass article of claim 2, wherein a ratio of a proportion of the constituent phase silicon dioxide in the upper side surface glass to a proportion of the constituent phase silicon dioxide in the core glass lies in a range from 1.1:1 to 2.0:1.
- Claim 6Depends on #2
The glass article of claim 2, wherein a proportion of the constituent phase silicon dioxide in the upper side surface glass is at least 50 mol %.
- Claim 7Depends on #2
The glass article of claim 2, wherein a proportion of the constituent phase anorthite in the upper side surface glass is at most 5 mol %.
- Claim 8Depends on #2
The glass article of claim 2, wherein a proportion of the constituent phase reedmergnerite in the upper side surface glass is at most 10 mol %.
- Claim 9Depends on #2
The glass article of claim 2, wherein a working point VA calculated according to the following formula (35) from the composition of the core glass in constituent phases lies in a range from 1200 ° C. to 1350 ° C.: V A = 0.989573825 · E pot _ · ° C kJ / mol - 387.9923613 ° C. (35)
- Claim 10Depends on #2
The glass article of claim 2, wherein a quotient of the elastic modulus and the variable (1 − μ) calculated according to the formulas (31) and (29) from the composition of the core glass lies in a range from 80 GPa to 100 GPa.
- Claim 11Depends on #1
The glass article of claim 1, wherein the CTE O calculated according to the formulas (14b), (15), and (16) of the upper side surface glass is 1.2 to 3.0 ppm/K.
- Claim 12Depends on #1
The glass article of claim 1, wherein a thickness of the glass article lies in a range from 0.1 mm to 30 mm.
- Claim 13Independent Claim
A method for producing a glass article, comprising: melting glass raw materials; forming a glass article from the glass melt; and cooling the glass article; wherein the glass article comprises three portions comprising an upper side surface glass, a core glass, and an underside surface glass, the upper side surface glass and the underside surface glass being present in each case to a depth of < 20 nm and the core glass is present in any event at 500 nm depth, a sum of proportions of tin oxide and bismuth oxide in the underside surface glass is greater than a sum of proportions of tin oxide and bismuth oxide in the upper side surface glass, the core glass having a CTE K calculated according to the following formulas (13) and (14a) in a range from 2.5 to 5.0 ppm/K: E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ i = 1 m z i, j, (13) CTE Glass = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 a) CTE O = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 b) wherein m is a number of cation types which occur, E pot,j, is a potential well depth tabulated for a j th cation type, and z j,I is a number of cations of the j th type in an i th constituent phase; the upper side surface glass having a CTE O that is calculated according to the formula (14b) for the upper side surface glass and the following formulas (15) and (16) which is lower by at least 0.6 ppm/K in comparison with the CTE K of the core glass calculated according to the formulas (13) and (14a): E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ i = 1 m z i, j = ∑ j = 1 m (∑ i = 1 n c i · z i, j) · E pot, j ∑ j = 1 m (∑ i = 1 n c i · z i, j), (15) ∑ i = 1 n c i · z i, j = k j · x j; (16) and wherein according to the following formula (10) a compressive prestress σ O on the upper side surface of at least 50 MPa is produced when the values of the core glass calculated according to the following formulas (31), (29), and (37) are used for E/(1 − μ) and T G and a difference CTE K -CTE O between the CTE values calculated for core glass and upper side surface glass is used for Δ CTE: σ O = E 1 - μ · (T G - T ambient) · Δ CTE, (10) μ = 0.17 + Δ μ f + Δ μ χ, (29) E = (0.683888667 (2 · (1 + μ) · f · E pot _ · z V m o l) - 39.4242404) GPa, (31) 1 V A - T G = (0.002665819 · f W + 0.001119212) · 1 K, (37) wherein T G is an annealing point of the glass, VA is a working point of the glass, E is a modulus of elasticity of the glass, μ is Poisson's ratio of the glass, T ambient is an ambient temperature, Δ μ f = - [(1 + μ) (1 - 2 μ) 3 1 f] Δ f, and f = Angle condition number p. A. - (2 3) (3 D angle degrees of freedom number p. A. - angle degrees of freedom number p. A.) Angle condition number p. A.; wherein the glass melt contains 30 to 60 mmol water per liter glass in a dissolved form.
- Claim 14Depends on #13
The method of claim 13, wherein the method comprises flat glass forming by a float method in which the glass melt is added onto a surface of a float bath composed of molten metal by flowing onto the surface of the float bath.
- Claim 15Depends on #14
The method of claim 14, wherein a dwell time which the glass has in a forming region of the float bath at a viscosity in the range 10 3 dPas to 10 8 dPas lies in a range from 5 to 60 minutes.
- Claim 16Depends on #15
The method of claim 15, wherein the dwell time lies in a range from 1 minute to 10 minutes per mm thickness of the glass article.
- Claim 17Depends on #15
The method of claim 15, wherein a glass temperature in a portion of the flowing-on glass lies in a range from VA K +10 ° C. to VA K +140 ° C., wherein VA K is a working point of the glass calculated from a composition of the glass.
- Claim 18Depends on #15
The method of claim 15, wherein the float bath is operated in a reducing protective gas atmosphere.
- Claim 19Depends on #18
The method of claim 18, wherein a float bath pressure lies between 0.05 mbar and 0.3 mbar and/or a hydrogen content in the gas atmosphere lies between 2 vol-% and 15 vol-%.
- Claim 20Independent Claim
A method for producing a glass article, comprising: melting glass raw materials; forming a glass article from the glass melt; and cooling the glass article; wherein the glass article comprises three portions comprising an upper side surface glass, a core glass, and an underside surface glass, the upper side surface glass and the underside surface glass being present in each case to a depth of < 20 nm and the core glass is present in any event at 500 nm depth, a sum of proportions of tin oxide and bismuth oxide in the underside surface glass is greater than a sum of proportions of tin oxide and bismuth oxide in the upper side surface glass, the core glass having a CTE K calculated according to the following formulas (13) and (14a) in a range from 2.5 to 5.0 ppm/K: E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ j = 1 m z i, j, (13) CTE K = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 a) CTE O = (50116.33042 (kJ Mol) E pot _ - 26.1724514) ppm / K, (14 b) wherein m is a number of cation types which occur, E pot,j, is a potential well depth tabulated for a j th cation type, and z j,I is a number of cations of the j th type in i th constituent phase; the upper side surface glass having a CTE O that is calculated according to the formula (14b) for the upper side surface glass and the following formulas (15) and (16) which is lower by at least 0.6 ppm/K in comparison with the CTE K of the core glass calculated according to the formulas (13) and (14a): E pot _ = ∑ i = 1 n c i · ∑ j = 1 m z i, j · E pot, j ∑ i = 1 n c i · ∑ j = 1 m z i, j = ∑ j = 1 m (∑ i = 1 n c i · z i, j) E pot, j ∑ j = 1 m (∑ i = 1 n c i · z i, j) j, (15) ∑ i = 1 n c i · z i, j = k j · x j; (16) and wherein according to the following formula (10) a compressive prestress σ O on the upper side surface of at least 50 MPa is produced when the values of the core glass calculated according to the following formulas (31), (29), and (37) are used for E/(1 − μ) and T G and a difference CTE K − CTE O between the CTE values calculated for core glass and upper side surface glass is used for Δ CTE: σ O = E 1 - μ · (T G - T a m b i e n 𝔱) · Δ CTE, (10) μ = 0. 1 7 + Δ μ f + Δ μ χ, (29) E = (0. 6 8 3 8 8 8 6 6 7 (2 · (1 + μ) · f · E pot _ · z V m o l) - 3 9. 4 2 4 2 4 04) GPa, (31) 1 V A - T G = (0. 0 0 2 665819 · f W + 0. 0 0 1 1 1 9212) · 1 K, (37) wherein T G is an annealing point of the glass, VA is a working point of the glass, E is a modulus of elasticity of the glass, μ is Poisson's ratio of the glass, T ambient is an ambient temperature, Δ μ f = - [(1 + μ) (1 - 2 μ) 3 1 f] Δ f, and f = Angle condition number p. A. - (2 3) (3 D angle degrees of freedom number p. A. - angle degrees of freedom number p. A.) Angle condition number p. A.; wherein the method comprises flat glass forming by a float method in which the glass melt is added onto a surface of a float bath composed of molten metal by flowing onto the surface of the float bath, wherein a dwell time which the glass has in a forming region of the float bath at a viscosity in the range 10 3 dPas to 10 8 dPas lies in a range from 5 to 60 minutes.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS This application claims priority to German Patent Application No. 10 2021 115 903.2, filed Jun. 18, 2021, which is incorporated herein by reference. BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to glass articles, for example, flat glasses, in the case of which the surface material has gradient material properties as a result of targeted process control which in turn lead to compressive prestressing of the surface. The invention also relates to a method for producing the glass articles as well as the use thereof. 2. Description of the Related Art Glasses which are compressively prestressed on the surface are required for many applications, in particular for applications in the field of safety glass or generally for glasses which are more resistant to mechanical effects than unprestressed glasses. There are various methods of compressive prestressing of the surfaces of glass products. In the case of what is known as chemical prestressing, see i.a. Arun K. Varshneya, Chemical Strengthening of Glass: Lessons Learned and Yet To Be Learned, International Journal of Applied Glass Science 1 [2]131-142 (2010), smaller ions located in the glass surface, e.g. sodium ions, are replaced by larger ions, e.g. potassium ions. This results in a greater space requirement of the surface relative to the core material. As a result of the connection to the core material, the surface is prevented from undergoing this expansion and is compressed to the original dimension, which results in corresponding compressive stresses. The chemical prestressing process typically takes place at high temperatures, but still significantly below the annealing point. In the case of what is known as thermal prestressing, see i.a. Werner Kiefer, Thermisches Vorspannen von Glasern niedriger Warmeausdehnung, Glastechnische Berichte 57 (1984), No. 9, pp. 221-228, the glass product, for example, a flat glass, is heated to a temperatur
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (10)
| Patent | Title | Year | Citations |
|---|---|---|---|
| EP 3,838,859 A1 | Thermally prestressable borosilicate glasses | — | 0 |
Non-Patent Literature (10)
- Yang et al. (
- “
- Cathodoluminescence and depth profiles in tin in float glass,
- ”
- J. Phys. D: Appl. Phys. 27 (1994) 1457-1762.) (Year: 1994).
- European Office Action dated Nov. 8, 2022 for European Patent Application No. 22179158.5 (7 pages).
- “
- Chemical Strengthening of Glass: Lessons Learned and Yet to Be Learned
- ”
- , Arun K. Varshneya, International Journal of Applied Glass Science 1 [2] 131-142, 2010 (12 pages).