Mechanochemical ammonia synthesis method
Abstract
A mechanochemical ammonia synthesis method according to an embodiment includes: (a) ball-milling Fe particles with balls under a nitrogen (N 2 ) atmosphere; and (b) ball-milling the Fe particles ball-milled under the nitrogen (N 2 ) atmosphere, with balls under a hydrogen (H 2 ) atmosphere.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.
Claims (19 — 1 Independent, 18 Dependent)
- Claim 1Independent Claim
A mechanochemical ammonia synthesis method, comprising: (a) performing first ball-milling on Fe particles with balls in a nitrogen (N 2) atmosphere; and (b) performing second ball-milling on the first ball-milled Fe particles with balls under a hydrogen (H 2) atmosphere.
- Claim 2Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein in the step (a), collisions with the balls create, on the Fe particles, active defects providing sites allowing nitrogen (N 2) to be adsorbed and dissociated into nitrogen atoms (N*).
- Claim 3Depends on #2
The mechanochemical ammonia synthesis method of claim 2, wherein in the step (a), Fe (N*) particles having nitrogen atoms (N*) adsorbed at the active defects are formed.
- Claim 4Depends on #3
The mechanochemical ammonia synthesis method of claim 3, wherein the nitrogen atoms (N*) adsorbed on the Fe particles in the step (a) are hydrogenated in the step (b) to produce NH* or NH 2 * intermediates, or ammonia (NH 3).
- Claim 5Depends on #4
The mechanochemical ammonia synthesis method of claim 4, wherein the step (b) is repeated until all of the NH* or NH 2 * intermediates are converted to ammonia.
- Claim 6Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein by the first ball milling, a density of the active defects on the Fe particles increases.
- Claim 7Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the step (a) is conducted at a temperature in a range of 20 ° C. to 100 ° C.
- Claim 8Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the step (a) is conducted at a pressure in a range of 1 bar to 20 bars.
- Claim 9Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the first and second ball-milling are conducted in a ball-milling container, and in the step (a), the first ball milling is conducted at a rotation speed of the ball-milling container, in a range of 200 rpm to 1,000 rpm.
- Claim 10Depends on #1
The mechanochemical ammonia synthesis method of claim 1, further comprising, between the step (a) and the step (b), a step of converting the nitrogen (N 2) atmosphere to the hydrogen (H 2) atmosphere.
- Claim 11Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the step (b) is conducted at a temperature in a range of 40 ° C. to 100 ° C.
- Claim 12Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the step (b) is conducted at a pressure in a range of 1 bar to 20 bars.
- Claim 13Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the first and second ball-milling are conducted within a ball-milling container, and in the step (b), the ball milling is conducted at a rotation speed of the ball-milling container, in a range of 200 rpm to 1,000 rpm.
- Claim 14Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein the balls are Fe-containing balls.
- Claim 15Depends on #1
The mechanochemical ammonia synthesis method of claim 1, wherein in the step (a), the Fe particles have a diameter in a range of 10 nm to 100 μ m.
- Claim 16Depends on #3
The mechanochemical ammonia synthesis method of claim 3, wherein in the step (b), the Fe (N*) particles have a diameter smaller than a diameter of the Fe particles.
- Claim 17Depends on #1
The mechanochemical ammonia synthesis method of claim 1, further comprising step (c) of separating ammonia produced, after the step (b).
- Claim 18Depends on #17
The mechanochemical ammonia synthesis method of claim 17, wherein the Fe particles after the step (c) grow to larger particles by Ostwald ripening.
- Claim 19Depends on #17
The mechanochemical ammonia synthesis method of claim 17, wherein the step (a) and the step (b) are repeated reusing the Fe particles regenerated after the step (c).
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS This is the U.S. National Stage of International Application No. PCT/KR2020/019127, filed Dec. 24, 2020, which claims the benefit of Korean Application No. 10-2020-0080499, filed Jun. 30, 2020. TECHNICAL FIELD The present disclosure relates to an ammonia synthesis method. BACKGROUND ART Ammonia (NH 3 ) is one of the most important industrial materials in fertilizers, explosives, plastics and other chemicals. Around 140 million tons of ammonia were produced annually worldwide in 2019, making ammonia one of the world's top 10 chemicals. The latest ammonia synthesis method is the Haber-Bosch process that synthesizes ammonia from nitrogen (N 2 ) and hydrogen (H 2 ) at 400-500 ° C. and at 100 bar or more. The reaction of the Haber-Bosch process, 0.5N 2 +1.5H 2 ↔ NH 3 ( Δ H= − 46.22 kJ mol − 1 ), is an exothermic reaction, and therefore in theory, according to Le Chatelier's principle, decreasing the temperature facilitates the conversion to NH 3 . However, high dissociation energy of N 2 and strong adsorption energy of hydrogen inhibit the formation of ammonia, thus making the Haber-Bosch process unfeasible under ambient conditions. Therefore, for the thermodynamic equilibrium being in favor of NH 3 at low temperatures and the ease of low-temperature processing, the science community is constantly looking for ways to synthesize ammonia at milder conditions than the Haber-Bosch process. However, unfortunately, the ammonia synthesis today has the same basic structure as it did 100 years ago. Thermodynamically considering the enthalpy of reaction, the activation energy for N 2 dissociation inevitably requires a high binding energy of the intermediates. The high temperature of the Haber-Bosch process used in industry is to promote the dissociation of stable N 2 molecules and the desorption of strongly adsorbed intermediates (N*, NH* and NH 2
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (7)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Machine Translation, CN-109835917-A, Chen P, Jun. 4, 2019 (Year: 2019).
- Machine Translation, JP-2020142189-A, Kataoka M, Sep. 10, 2020 (Year: 2020).
- International Stainless Steel Forum,
- “
- Basic facts about stainless steel
- ”
- (Year: 2025).
- Gao et al.,
- “
- Production of ammonia via a chemical looping process based on metal imides as nitrogen carriers,