Disclosed are methods of purifying nanodiamonds and a method of making essentially pure nanodiamonds each involving mixing nanodiamonds with at least one salt to form a mixture; heating the mixture at a temperature from 200 ° C. to 1,000 ° C. for a time from 10 minutes to 10 hours; and combining a liquid with the heated mixture and centrifuging at a speed of 30 rcf to 25,000 rcf for a time from 10 seconds to 60 minutes to provide purified nanodiamonds. With the methods of the invention, pure NDs can be produced by one-step processing after air oxidation, without the need for any further centrifugation acts. Furthermore, the developed salt-assisted air oxidation method enables facile scale-up manufacturing of clean NDs, with a rounded shape transformed from original shard-like shape, which is impossible to achieve using any existing purification method.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for purifying nanodiamonds, comprising: mixing the nanodiamonds with at least one salt to form a mixture; heating the mixture at a temperature of 400 ° C. to 600 ° C. for a period of 1 hour to 5 hours; and combining an organic liquid with the heated mixture and centrifuging at a speed from 500 rcf to 5,000 rcf for a period from 1 minute to 15 minutes to provide purified nanodiamonds, wherein the at least one salt is selected from one or more of sodium chloride, magnesium chloride, potassium chloride, calcium chloride, and ammonium chloride, wherein the organic liquid is selected from the group consisting of methanol and ethanol.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the nanodiamonds have a size below 1 μ m.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the nanodiamonds are mixed with 0.1 to 100 times by weight of the at least one salt.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the purified nanodiamonds comprise at least 99.9% by weight nanodiamonds and less than 0.1% by weight impurities.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the purified nanodiamonds are not agglomerated.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the nanodiamonds are mixed with 0.5 to 50 times by weight of the at least one salt.

  7. Claim 7Independent Claim

    A method for preparing pure nanodiamonds, the method comprising: mixing unprocessed nanodiamonds with at least one salt to form a mixture; heating the mixture at a temperature of 400 ° C. to 600 ° C. in air for a period of 1 hour to 5 hours; and combining an organic liquid with the heated mixture and centrifuging at a speed of 500 rcf to 5,000 rcf for a period from 1 minute to 15 minutes to provide the pure nanodiamonds having less than 0.01% impurities by weight, wherein the at least one salt is selected from one or more of sodium chloride, magnesium chloride, potassium chloride, calcium chloride, or ammonium chloride.

  8. Claim 8Depends on #7

    The method of claim 7, wherein the unprocessed nanodiamonds have a size below 1 μ m.

Technical Overview & Description

TECHNICAL FIELD The present invention relates to methods of making and purifying nanodiamonds. BACKGROUND ART Nanoscale diamond particles (with a size below 1 μ m), generally known as nanodiamonds (NDs), have several outstanding material qualities, offering a wide range of potential for basic science and industrial applications. In particular, a number of optically addressable impurity defects, such as nitrogen-vacancy (NV) centers residing in the diamond lattice, have been deployed for next-generation quantum technologies due to their unique spin properties. Currently, there are mainly two methods for the large-scale fabrication of NDs: “ bottom-up ” detonation NDs and “ top-down ” milling of bulk high-pressure high-temperature (HPHT) diamond. It is well known that the raw ND powders (i.e., detonation or HPHT) contain a considerable amount of unwanted impurities [e.g., ultrasmall ( < 10 nm)-sized NDs, disordered carbons, metal, and metal oxides], which are naturally introduced during synthesis and processing. However, previous reports have demonstrated that the non-diamond phases present at the surface of NDs are detrimental to the properties of embedded quantum defects (e.g., NV centers). Therefore, the removal of these impurities becomes a critical step before the ultimate applications of the NDs. For example, the fluorescence lifetime and spin-coherence time (T 2 ) of NV centers in NDs could be significantly improved by cleaning the surface quenchers (e.g., fluorescent graphitic carbon). This has proven to be quite beneficial for potential applications in photonics, quantum sensing, and imaging. Moreover, a sufficiently clean and uniform surface of NDs, desired for favorable nanobiointeractions, is a prerequisite for potential biomedical applications in drug delivery, biolabeling, and biosensing. At present, the most commonly used method of removing non-diamond carbons involves the surface oxidization of raw NDs in the presence of air at 400-600 ° C. for several

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (2)

PatentTitleYearCitations

Non-Patent Literature (10)

  • S. Stehlik et al.
  • “
  • Size and nitrogen inhomogeneity in detonation and laser synthesized primary nanodiamond particles revealed via salt-assisted deaggregation,
  • ”
  • Carbon 2021, 171, 230-239; available online Sep. 9, 2020. (Year: 2020).
  • English machine translation of JP H09328307 A. (Year: 1997).
  • M. Mobin, A.U. Malik and Sultan Ahmad.
  • “
  • High Temperature Interactions of Metal Oxides with NaCl,
  • ”