Methods and systems for welding copper using blue laser
Abstract
A visible light laser system and operation for welding materials together. A blue laser system that forms essentially perfect welds for copper based materials. A blue laser system and operation for welding conductive elements, and in particular thin conductive elements, together for use in energy storage devices, such as battery packs.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.
Claims (6 — 1 Independent, 5 Dependent)
- Claim 1Independent Claim
A method of forming a weld in copper based materials, the method comprising: a. placing a work piece in a laser system; wherein the work piece comprises placing a first piece of copper based material in contact with a second piece of copper material, the first piece of copper based material comprises a plurality of layers of copper foil; b. directing a laser beam at the work piece, whereby a weld is formed between the first piece of copper based material and the second piece of copper based material; wherein the weld comprises a HAZ and a resolidification zone; and, c. wherein a microstructure of the copper based material, the HAZ and the resolidification zone show no discernable difference in the weld that would indicate a weakness in the weld, and/or wherein the identical microstructure comprises crystal growth regions of similar size; d. wherein the laser beam is blue with a wavelength from about 405 nm to about 500 nm and the laser beam is directed to the work piece as a focused spot having power density of less than 800 kW/cm 2 with a spot size from about 50 μ m to about 250 μ m.
- Claim 2Depends on #1
The method of claim 1, wherein the weld is formed by conduction mode welding.
- Claim 3Depends on #1
The method of claim 1, comprising applying a shielding gas selected from the group consisting of He, Ar, N 2.
- Claim 4Depends on #1
The method of claim 1, comprising applying a shielding gas and adding hydrogen to remove oxide layers and promote wetting of the weld.
- Claim 5Depends on #1
The method of claim 1, comprising directing a second laser beam to a same area as the laser beam to form the weld.
- Claim 6Depends on #4
The method of claim 4, comprising directing a second laser beam to a same area as the laser beam to form the weld.
Technical Overview & Description
This application is a continuation of U.S. application Ser. No. 15/884,672 filed Jan. 31, 2018, which claims under 35 U.S.C. § 119(e)(1) the benefit of the filing date of U.S. provisional application Ser. No. 62/452,598 filed Jan. 31, 2017, the entire disclosure of each of which is incorporated herein by reference. BACKGROUND OF THE INVENTION Field of the Invention The present inventions relate to laser processing of materials, and in particular laser joining of copper materials using laser beams having wavelengths from about 350 nm to about 500 nm, and greater. Laser welding of copper has proven to be very challenging due to high reflectivity, high thermal conductivity and high heat capacity. Numerous methods have been developed to weld copper ranging from ultrasonic welding to IR laser welding. These prior copper welding methods, however, have many shortcomings and limitations. For example, one market where these limitations are seen is in the area of high performance electronics for the growing electronic vehicle market. A better weld quality with higher speed, than can be obtained by these prior techniques, is needed to produce high performance batteries and electronics for the growing automotive markets. When using an IR laser source at 1030 nm, the high reflectivity of the copper at this wavelength makes it difficult to couple power into the material to heat and weld it. One method to overcome the high reflectivity is to use a high-power level ( > 1 kW) IR laser to initiate a keyhole weld which then couples the power into the material. The problems with this method of welding, among other things, is that the vapor in the keyhole can lead to a micro-explosion, spraying molten copper all over the parts being welded or the micro-explosion can cause a hole completely through the parts being welded. Consequently, researchers have had to rely on rapidly modulating the laser power to try to prevent these defects during welding. It has been discovered that the defects
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (80)
Non-Patent Literature (10)
- U.S. Appl. No. 17/562,953, filed Dec. 27, 2021, Zediker.
- 3D Systems Inc.; iPro 8000 and 9000 Brochure, 2010.
- 3D Systems Inc.; Sinterstation HiQ Series, 2012.
- 3D Systems Inc.; sPro 125 and sPro 250
- —
- Direct Metal SLM Production Printer.
- Lee, Benjamin G.; Wavelength beam combining of quantum cascade laser arrays for remote sensing; The International Society for Optical Engineering, SPIE 2009.
- Lisinetskii, V. A.; Raman Gain Coefficient of Barium Nitrate Measured for the Spectral Region of TI: Sapphire Laser, Journal of Nonlinear Optical Physics and Materials, vol. 14, No. 1 (2005), pp. 107-114.
- McKay, Aaron; Diamond-based concept for combining beams at very high average powers, Laser Photonics Rev., 2017.
- Mildren, R. P.; Efficient, all-solid-state, Raman laser in the yellow, orange and red, Optics Express, Mar. 8, 2004, vol. 12, No. 5.