Silicidation process for semiconductor devices
Abstract
A method of forming a device includes providing a substrate containing an exposed semiconductor region, forming a metal oxide film over the exposed semiconductor region, and forming an oxygen-scavenging metal film over the metal oxide film. The method includes chemically reducing the metal oxide film to an elemental metal film by scavenging oxygen from the metal oxide film into the oxygen-scavenging metal film; and reacting the elemental metal film with the semiconductor region to form a metal-semiconductor layer, the metal-semiconductor layer forming a source/drain contact region of a transistor.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 0.
Claims (19 — 3 Independent, 16 Dependent)
- Claim 1Independent Claim
A method of forming a device, the method comprising: providing a substrate containing an exposed semiconductor region; forming a nickel oxide film over the exposed semiconductor region; forming an oxygen-scavenging metal film over the nickel oxide film; chemically reducing the nickel oxide film to an elemental nickel film by scavenging oxygen from the nickel oxide film into the oxygen-scavenging metal film; reacting, at a first temperature, the elemental nickel film with the exposed semiconductor region to form an intermediate layer containing atoms from the elemental nickel film and atoms from the exposed semiconductor region, the intermediate layer having a first resistivity of 24 micro-ohm*cm; removing remaining portions of the elemental nickel film and the oxygen-scavenging metal film after forming the intermediate layer; and after the removing, annealing at a second temperature above the first temperature to convert the intermediate layer to a nickel silicide layer, the nickel silicide layer having a second resistivity of 10.5 micro-ohm*cm, the nickel silicide layer forming a source/drain contact region of a transistor.
- Claim 2Depends on #1
The method of claim 1, wherein the oxygen-scavenging metal film is a titanium metal film further including forming the titanium metal film by reacting TiCl 4 with hydrogen and removing unreacted titanium film by etching in a TiCl 4 ambient.
- Claim 3Depends on #1
The method of claim 1, wherein the exposed semiconductor region comprises silicon, germanium, carbon, tin, gallium, indium, or arsenic, or mixtures thereof.
- Claim 4Depends on #1
The method of claim 1, wherein the chemically reducing step and the reacting step are performed simultaneously using a heat-treating step.
- Claim 5Depends on #4
The method of claim 4, wherein the heat-treating step is performed at a substrate temperature between about 400 ° C. and about 750 ° C.
- Claim 6Depends on #1
The method of claim 1, wherein a thickness of the oxygen-scavenging metal film is two times or more of a thickness of the nickel oxide film.
- Claim 7Depends on #1
The method of claim 1, wherein the oxygen-scavenging metal film is a metal selected from a group consisting of Ti, Sc, Y, La and lanthanides, Zr, Hf, V, Nb, and Ta.
- Claim 8Independent Claim
A method of forming source/drain regions, comprising: providing a substrate containing first and second semiconductor regions; selectively forming a metal oxide film over the first semiconductor region; forming an oxygen-scavenging metal film over the first and second semiconductor regions, wherein a thickness of the oxygen-scavenging metal film is two times or more of a thickness of the metal oxide film; chemically reducing the metal oxide film to an elemental metal film by scavenging oxygen from the metal oxide film into the oxygen-scavenging metal film; reacting the elemental metal film with the first semiconductor region to form a metal semiconductor film; reacting the oxygen-scavenging metal film with the second semiconductor region to form an oxygen-scavenging metal semiconductor film; and annealing to reduce resistivities of the metal semiconductor film and the oxygen-scavenging metal semiconductor film.
- Claim 9Depends on #8
The method of claim 8, wherein the oxygen-scavenging metal film is a titanium-containing film further including forming the titanium-containing film by reacting TiCl 4 with H 2 and removing a portion of the titanium-containing film by etching in a TiCl 4 ambient.
- Claim 10Depends on #8
The method of claim 8, wherein the chemically reducing step and the reacting the elemental metal film and the oxygen-scavenging metal film steps are performed simultaneously by heating the substrate.
- Claim 11Depends on #8
The method of claim 8, wherein a metal in the elemental metal film, in the metal oxide film, and in the metal semiconductor film is selected from a group consisting of Ni, Os, Co, Ru, Ir, Pd, Pt, and Rh.
- Claim 12Depends on #8
The method of claim 8, wherein the oxygen-scavenging metal is a metal selected from a group consisting of Ti, Sc, Y, La and lanthanides, Zr, Hf, V, Nb, and Ta.
- Claim 13Depends on #8
The method of claim 8, wherein the metal oxide film includes a nickel oxide film, the elemental metal film includes elemental nickel metal, and the metal semiconductor film includes nickel silicide.
- Claim 14Depends on #8
The method of claim 8, further comprising: removing a remaining portion of the oxygen-scavenging metal film, a remaining portion of the elemental metal film, or both, from the substrate.
- Claim 15Depends on #8
The method of claim 8, wherein the first semiconductor region is p-type silicon or p-type silicon germanium and wherein the second semiconductor region is n-type silicon or n-type silicon germanium or n-type carbon doped silicon.
- Claim 16Depends on #8
The method of claim 8, wherein selectively forming the metal oxide film over the first semiconductor region includes forming the metal oxide film over the first and the second semiconductor regions and removing the metal oxide film from the second semiconductor region by masking the first semiconductor region and removing the metal oxide film from the second semiconductor region using an etching process.
- Claim 17Independent Claim
A method of forming a device, the method comprising: providing a substrate containing first and second semiconductor regions; selectively forming a nickel oxide film over the first semiconductor region; forming a titanium metal film over the first and second semiconductor regions; chemically reducing the nickel oxide film to an elemental nickel metal film by oxygen scavenging from the nickel oxide film to the titanium metal film; reacting the elemental nickel metal film with the first semiconductor region to form a nickel semiconductor film; and reacting the titanium metal film with the second semiconductor region to form a titanium semiconductor film, wherein the chemically reducing step and the reacting steps include a heat-treating step; removing unreacted portions of the elemental nickel metal film and unreacted portions of the titanium metal film after forming the nickel semiconductor film and the titanium semiconductor film; and annealing to: convert the titanium semiconductor film to a titanium silicide layer, the titanium silicide layer comprising a lower resistance than a resistance of the titanium semiconductor film; and convert the nickel semiconductor film to a nickel silicide layer, the nickel silicide layer comprising a lower resistance than a resistance of the nickel semiconductor film, the annealing being performed at a higher temperature than the heat-treating step.
- Claim 18Depends on #17
The method of claim 17, further including forming the titanium metal film by reacting TiCl 4 with H 2 and removing the unreacted portions of the titanium metal film comprises etching in a TiCl 4 ambient.
- Claim 19Depends on #17
The method of claim 17, wherein the first semiconductor region comprises p-type silicon, p-type silicon germanium, p-type germanium, or p-type germanium-tin and wherein the second semiconductor region comprises n-type silicon, n-type carbon doped silicon, or n-type germanium.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Application No. 63/329,260 filed on Apr. 8, 2022, which application is hereby incorporated herein by reference. TECHNICAL FIELD The invention relates generally to the field of semiconductor device manufacturing and, more particularly, to silicidation processes. BACKGROUND For most advanced semiconductor devices complementary metal-oxide semiconductor (CMOS) technology is employed. CMOS technology utilizes p-type and n-type metal-oxide semiconductor field effect transistors (MOSFETs) in complementary pairs for logic functions. It is desirable to have MOSFETs with a high drive current when the devices are on in order to achieve a low delay when switching the device. In order to achieve a high drive current, various source and drain (source/drain) structures have been employed in order to maximize the drive current of the MOSFETs by imparting strain to the channel region of the device and/or by minimizing the contact resistivity to the source/drain of the MOSFETs. In many advanced MOSFETs epitaxial semiconductor layers with high doping are employed in the source/drain of the MOSFETs. For instance, highly doped epitaxial silicon, or carbon doped silicon, (Si:C) is frequently employed for the source/drain structures of n-type silicon MOSFETs (nMOSFETs) while highly doped epitaxial germanium doped silicon (SiGe) is frequently employed for the source/drain structures of p-type MOSFETs (pMOSFETs). When forming advanced MOSFETs, part of the semiconductor that is present in the source and drain structures of the MOSFETs can be converted into low-resistivity metal silicides. This is done to provide a conductive path with a low bulk resistivity in the device, and to ensure a good contact resistance. Nickel, cobalt and titanium silicides, for example, have been used for this process in silicon MOSFETs. In some cases it is beneficial to have different silicides in the source/drain of t
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (17)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Machine translation of KR-2012045570-A (Year: 2012).
- Wilson, Rachel L., et al.,
- “
- Chemical vapour deposition (CVD) of nickel oxide using the novel nickel dialkylaminoalkoxide precursor [Ni(dmam
- ′
- )2] (dmamp
- ′
- 2-dimethylamino-2-methyl-1-propanolate),
- ”
- RSC Advances, 2021, 11, Royal Society of Chemistry, Jun. 15, 2021, 7 pages.