hottub.patents
US 12,772,403 B2#3101814 Most CitedActiveUnited States (USPTO)Utility

Cover articles with high hardness and anti-reflective properties for infrared sensors

0Forward Citations (#3101814 Global)
0.0/yrCitation Velocity (#3101814 Global)
0.00Citation PageRank (#3101814 Global)
34Prior Art Cited
28Claims (5 Indep. · 23 Dep.)
33Drawings / Sheets

Abstract

A cover article for a sensor is described herein that includes: a substrate comprising a thickness from 50 μ m to 5000 μ m, an outer primary surface, and an inner primary surface; and an outer layered film disposed on the outer primary surface. The substrate is a chemically-strengthened glass or glass-ceramic substrate. The cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 ° .

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 0.

Claims (28 — 5 Independent, 23 Dependent)

  1. Claim 1Independent Claim

    A cover article for a sensor, comprising: a substrate comprising a thickness from 50 μ m to 5000 μ m, an outer primary surface and an inner primary surface, wherein the outer and inner primary surfaces are opposite of one another and the substrate is a chemically-strengthened glass substrate or a glass-ceramic substrate; and an outer layered film disposed on the outer primary surface of the substrate, and wherein the cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 °, wherein the outer layered film comprises a scratch resistant layer comprising a nitride or an oxynitride and having a thickness from about 80 nm to 10,000 nm, wherein the outer layered film comprises a plurality of alternating high refractive index and low refractive index layers, and wherein each of the high refractive index layers comprises a nitride or an oxynitride and has a refractive index greater than a refractive index of each of the low refractive index layers, and wherein one of the low refractive index layers is a capping layer defining an outermost surface of the outer layered film and the capping layer has a thickness of at least 110 nm, and further wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the low refractive index layers of the antireflective region comprise a total thickness of less than 275 nm.

  2. Claim 2Depends on #1

    The cover article of claim 1, wherein the outer layered film comprises a refractive index gradient.

  3. Claim 3Depends on #1

    The cover article of claim 1, wherein the antireflective region comprises a thickness from about 100 nm to about 525 nm.

  4. Claim 4Depends on #1

    The cover article of claim 1, wherein the cover article further exhibits a two-surface average transmittance of greater than 85% for infrared wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 40 °.

  5. Claim 5Depends on #1

    The cover article of claim 1, wherein the cover article exhibits a first-surface average reflectance of less than 5% for infrared wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 40 °.

  6. Claim 6Depends on #1

    The cover article of claim 1, wherein the cover article further exhibits a first-surface average reflectance from 2% to 5% for wavelengths from 800 nm to 1000 nm at an angle of incidence of 8 °.

  7. Claim 7Depends on #1

    The cover article of claim 1, wherein the cover article further exhibits a first-surface reflected CIE color for all angles of incidence from 0 ° to 90 ° with a* from − 10 to +10 and b* from − 12 to +5 (CIE coordinate b*), as measured under illumination from a D65 illuminant.

  8. Claim 8Depends on #1

    The cover article of claim 1, wherein the cover article exhibits a first-surface average photopic reflectance of less than 2% for an angle of incidence of about 8 °.

  9. Claim 9Depends on #1

    The cover article of claim 1, wherein the scratch resistant layer and each of the high refractive index layers comprises SiN x or SiO x N y.

  10. Claim 10Depends on #1

    The cover article of claim 1, wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the antireflective region comprises at least five alternating high refractive index and low refractive index layers.

  11. Claim 11Depends on #1

    The cover article of claim 1, wherein the outer layered film comprises an optical interference layer between the scratch resistant layer and the substrate, the optical interference layer comprising alternating high refractive index and low refractive index layers.

  12. Claim 12Depends on #1

    The cover article of claim 1, wherein the thickness of the capping layer is from 110 nm to about 200 nm.

  13. Claim 13Depends on #1

    The cover article of claim 1, wherein a high refractive index layer adjacent to the capping layer has a thickness from about 10 nm to less than 150 nm.

  14. Claim 14Depends on #1

    The cover article of claim 1, wherein the outer layered film exhibits a residual compressive stress of greater than or equal to 700 Mpa and an elastic modulus of greater than or equal to 140 Gpa.

  15. Claim 15Depends on #1

    The cover article of claim 1, wherein the substrate is a glass-ceramic that comprises an elastic modulus of greater than 85 Gpa and a fracture toughness of greater than 0.8 Mpa · √ m.

  16. Claim 16Depends on #1

    The cover article of claim 1, wherein the outer layered film exhibits a residual compressive stress of from 700 Mpa to 1100 Mpa and an elastic modulus of from 140 Gpa to 200 Gpa.

  17. Claim 17Depends on #1

    The cover article of claim 1, wherein the outer layered film exhibits an elastic modulus of from 140 Gpa to 180 Gpa.

  18. Claim 18Depends on #1

    The cover article of claim 1, wherein the substrate has a residual surface compressive stress of from 200 Mpa to 1200 Mpa and a depth of compression (DOC) of from 5 μ m to 150 μ m.

  19. Claim 19Depends on #1

    The cover article of claim 1, wherein the substrate further exhibits a maximum central tension (CT) value from 80 Mpa to 200 Mpa, and further wherein the substrate has a thickness of about 1.5 mm or less.

  20. Claim 20Depends on #1

    The cover article of claim 1, wherein the substrate has a residual surface compressive stress of from 200 Mpa to 400 Mpa.

  21. Claim 21Depends on #1

    The cover article of claim 1, wherein the cover article exhibits an average failure stress of 800 Mpa or greater in a ring-on-ring test with the outer surface of the outer layered film placed in tension.

  22. Claim 22Depends on #1

    A glass screen protector for a smart phone, comprising: a cover glass; and an adhesive backing disposed on the cover glass, wherein the adhesive backing is for attachment to the smart phone, and further wherein at least one portion of the cover glass comprises a cover article of claim 1.

  23. Claim 23Depends on #1

    A consumer electronic product, comprising: a housing comprising a front surface, a back surface and side surfaces; electronic components at least partially within the housing, the electronic components comprising at least one of a display and a sensor, the display at or adjacent to the front surface of the housing and the sensor at or adjacent to the front surface or the back surface of the housing; and a cover disposed over at least one of the display and the sensor, wherein at least one portion of the cover comprises the cover article of claim 1.

  24. Claim 24Independent Claim

    A cover article for a sensor, comprising: a substrate comprising a thickness from 50 μ m to 5000 μ m, an outer primary surface and an inner primary surface, wherein the outer and inner primary surfaces are opposite of one another and the substrate is a chemically-strengthened glass substrate or a glass-ceramic substrate; and an outer layered film disposed on the outer primary surface of the substrate, wherein the outer layered film comprises a plurality of alternating high refractive index and low refractive index layers, wherein each of the high refractive index layers comprises a nitride or an oxynitride and has a refractive index greater than a refractive index of each of the low refractive index layers, wherein the outer layered film comprises a scratch resistant layer having a thickness from about 80 nm to 10,000 nm, wherein one of the low refractive index layers is a capping layer defining an outermost surface of the outer layered film and the capping layer has a thickness of at least 110 nm, wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the antireflective region comprises a thickness from about 100 nm to about 525 nm, wherein the low refractive index layers of the antireflective region comprise a total thickness of less than 275 nm, wherein the outer layered film exhibits a hardness of at least 8 Gpa, as measured with a Berkovich Indenter Hardness Test from the outermost surface of the outer layered film to a depth from about 100 nm to about 500 nm, and further wherein the cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 °.

  25. Claim 25Independent Claim

    A cover article for a sensor, comprising: a substrate comprising a thickness from 50 μ m to 5000 μ m, an outer primary surface and an inner primary surface, wherein the outer and inner primary surfaces are opposite of one another and the substrate is a chemically-strengthened glass substrate or a glass-ceramic substrate; and an outer layered film disposed on the outer primary surface of the substrate, wherein the cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 °, and further wherein the outer layered film exhibits a residual compressive stress of greater than or equal to 700 Mpa and an elastic modulus of greater than or equal to 140 Gpa, wherein the outer layered film comprises a scratch resistant layer comprising a nitride or an oxynitride and having a thickness from about 80 nm to 10,000 nm, wherein the outer layered film comprises a plurality of alternating high refractive index and low refractive index layers, and wherein each of the high refractive index layers comprises a nitride or an oxynitride and has a refractive index greater than a refractive index of each of the low refractive index layers, and wherein one of the low refractive index layers is a capping layer defining an outermost surface of the outer layered film and the capping layer has a thickness of at least 110 nm, and further wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the low refractive index layers of the antireflective region comprise a total thickness of less than 275 nm.

  26. Claim 26Independent Claim

    A cover article for a sensor, comprising: a glass-ceramic substrate comprising a first primary surface and a second primary surface, the primary surfaces opposing one another; and an outer layered film defining an outer surface, the outer layered film disposed on the first primary surface, wherein the cover article exhibits a hardness of greater than 15 Gpa, as measured by a Berkovich Hardness Test at an indentation depth of about 125 nm from the outer surface of the outer layered film, and further wherein the cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 °, wherein the outer layered film comprises a scratch resistant layer comprising a nitride or an oxynitride and having a thickness from about 80 nm to 10,000 nm, wherein the outer layered film comprises a plurality of alternating high refractive index and low refractive index layers, and wherein each of the high refractive index layers comprises a nitride or an oxynitride and has a refractive index greater than a refractive index of each of the low refractive index layers, and wherein one of the low refractive index layers is a capping layer defining an outermost surface of the outer layered film and the capping layer has a thickness of at least 110 nm, and further wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the low refractive index layers of the antireflective region comprise a total thickness of less than 275 nm.

  27. Claim 27Independent Claim

    A cover article for a sensor, comprising: a substrate comprising a thickness from 50 μ m to 5000 μ m, an outer primary surface and an inner primary surface, wherein the outer and inner primary surfaces are opposite of one another and the substrate is a chemically-strengthened glass substrate or a glass-ceramic substrate; and an outer layered film disposed on the outer primary surface of the substrate, wherein the outer layered film exhibits a hardness of at least 8 Gpa, as measured with a Berkovich Indenter Hardness Test from the outermost surface of the outer layered film to a depth from about 100 nm to about 500 nm, and further wherein the cover article exhibits a first-surface average reflectance of less than 10% for wavelengths from 1000 nm to 1700 nm for at least one angle of incidence from 8 ° to 60 °, wherein the outer layered film comprises a scratch resistant layer comprising a nitride or an oxynitride and having a thickness from about 80 nm to 10,000 nm, wherein the outer layered film comprises a plurality of alternating high refractive index and low refractive index layers, and wherein each of the high refractive index layers comprises a nitride or an oxynitride and has a refractive index greater than a refractive index of each of the low refractive index layers, and wherein one of the low refractive index layers is a capping layer defining an outermost surface of the outer layered film and the capping layer has a thickness of at least 110 nm, and further wherein the outer layered film comprises an antireflective region over the scratch resistant layer, and the low refractive index layers of the antireflective region comprise a total thickness of less than 275 nm.

  28. Claim 28Depends on #27

    The cover article of claim 27, wherein the antireflective region comprises a thickness from about 100 nm to about 525 nm.

Technical Overview & Description

CLAIM OF PRIORITY This application claims the benefit of priority under 35 U.S.C. § 119 of U.S. Provisional Application No. 63/321,905 filed Mar. 21, 2022, and claims the benefit of priority under 35 U.S.C. § 119 of U.S. Provisional Application No. 63/450,687 filed Mar. 8, 2023, the content of which is incorporated herein by reference in its entirety. FIELD OF THE DISCLOSURE This disclosure relates to durable and/or scratch resistant cover articles for electronic devices and, more particularly, to durable and/or scratch resistant cover articles for infrared sensors and other sensors. BACKGROUND Cover articles are often used to protect critical devices within electronic products, to provide a user interface for input and/or display, and/or many other functions. Such products include mobile devices, such as smart phones, mp3 players, and computer tablets. Cover articles also include architectural articles, transportation articles (e.g., articles used in automotive applications, trains, aircraft, sea craft, etc.), appliance articles, or any article that requires some transparency, scratch-resistance, abrasion resistance, or a combination thereof. These applications often demand scratch-resistance and strong optical performance characteristics, in terms of maximum light transmittance and minimum reflectance. Furthermore, some cover applications require that the color exhibited or perceived, in reflection and/or transmission, does not change appreciably as the viewing angle is changed. In display applications, this is because, if the color in reflection or transmission changes with viewing angle to an appreciable degree, the user of the product will perceive a change in color or brightness of the display, which can diminish the perceived quality of the display. In other applications, changes in color may negatively impact the aesthetic requirements or other functional requirements. Recently, infrared (IR) sensors are increasingly being deployed in these same applications

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Corning Inc.,
  • “
  • Information Related to Coatings on Commercially Available Tablet Devices
  • —
  • Supplying data related to the Apple iPad Air 2 (released Oct. 2014), Apple iPad Pro 2nd Generation (released Jun. 2017), and Apple iPad Air 4th Generation (released Oct. 2020)
  • ”
  • 28 pages. This document has not been published in a book, magazine, journal, etc.
  • International Search Report and Written Opinion of the International Searching Authority; PCT/US2023/015431; dated Aug. 28, 2023; 19 pages; European Patent Office.
  • Katsuyama, T.,
  • “