hottub.patents
US 12,768,075 B2#3106114 Most CitedActiveUnited States (USPTO)Utility

Single crystal diamond component and method for producing

0Forward Citations (#3106114 Global)
0.0/yrCitation Velocity (#3106114 Global)
0.00Citation PageRank (#3106114 Global)
15Prior Art Cited
20Claims (1 Indep. · 19 Dep.)
3Drawings / Sheets

Abstract

A single crystal CVD diamond component and a method of fabricating the single crystal CVD diamond component. The single crystal CVD diamond component comprises a surface, wherein at least a portion of the surface has been processed by chemical mechanical polishing, CMP, and a layer of quantum spin defects, said layer of quantum spin defects being disposed within 500 nm of the surface.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.

Claims (20 — 1 Independent, 19 Dependent)

  1. Claim 1Independent Claim

    A single crystal CVD diamond component comprising: a surface, wherein at least a portion of the surface has been processed by chemical mechanical polishing, CMP; a layer of quantum spin defects, said layer of quantum spin defects being disposed within 500 nm of the surface, wherein the chemical mechanical polishing of the surface reduces subsurface damage, which increases decoherence time, T 2, of the quantum spin defects; and wherein the single crystal CVD diamond component has at least one lateral dimension of at least 0.5 mm.

  2. Claim 2Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein at least a portion of the surface has been processed by inductively coupled plasma, ICP, etching prior to the chemical mechanical polishing.

  3. Claim 3Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein at least a portion of the surface has been processed by mechanical polishing prior to the chemical mechanical polishing.

  4. Claim 4Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the quantum spin defects are selected from the group consisting of: silicon containing defects; nickel containing defects; chromium containing defects; germanium containing defects; tin containing defects; nitrogen containing defects; and negatively charged nitrogen-vacancy defects NV −.

  5. Claim 5Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein a concentration of quantum spin defects is equal to or greater than 1 × 10 13 defects/cm 3, and wherein the concentration of quantum spin defects is equal to or less than 4 × 10 18 defects/cm 3.

  6. Claim 6Depends on #5

    The single crystal CVD diamond component according to claim 5, wherein the concentration of quantum spin defects is equal to or less than 2 × 10 18 defects/cm 3.

  7. Claim 7Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the surface has a surface roughness Ra of no more than 5 nm.

  8. Claim 8Depends on #1

    The single crystal CVD diamond component according to claim 1, comprising a further layer having a single substitutional nitrogen concentration of no more than 300 ppb, said layer being disposed distal to the surface relative to the layer of quantum spin defects.

  9. Claim 9Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the layer of quantum spin defects is disposed within 200 nm of the surface.

  10. Claim 10Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the single crystal CVD diamond component has the at least one lateral dimension of at least 1 mm.

  11. Claim 11Depends on #1

    A device comprising the single crystal CVD diamond component according to claim 1.

  12. Claim 12Depends on #1

    A method of fabricating the single crystal CVD diamond component as claimed in claim 1, the method comprising: providing a single crystal CVD diamond having a surface and at least one lateral dimension of at least 0.5 mm; processing at least a portion of the surface using chemical mechanical polishing, CMP, such that the single crystal CVD diamond comprises a layer of quantum spin defects, said layer of quantum spin defects being disposed within 500 nm of the surface.

  13. Claim 13Depends on #12

    The method according to claim 12, further comprising, prior to processing at least a portion of the surface using chemical mechanical polishing, processing the portion of the surface using inductively coupled plasma, ICP, etching.

  14. Claim 14Depends on #12

    The method according to claim 12, further comprising: implanting nitrogen into the surface of the single crystal CVD diamond; and annealing the single crystal CVD diamond to cause migration of vacancy and/or nitrogen defects within the single crystal CVD diamond and formation of nitrogen-vacancy defects from the implanted nitrogen and the vacancy defects; such that the implanting and annealing form the layer of quantum spin defects disposed within 500 nm of the surface.

  15. Claim 15Depends on #12

    The method according to claim 12, further comprising, prior to processing at least a portion of the surface using chemical mechanical polishing, providing the single crystal CVD diamond having a quantum spin defect concentration equal to or greater than 1 × 10 13 defects/cm 3.

  16. Claim 16Depends on #15

    The method according to claim 15, further comprising, prior to processing at least a portion of the surface using chemical mechanical polishing, providing the single crystal CVD diamond having the quantum spin defect concentration equal to or less than 4 × 10 18 defects/cm 3.

  17. Claim 17Depends on #5

    The single crystal CVD diamond component according to claim 5, wherein the concentration of quantum spin defects is equal to or greater than 1 × 10 14 defects/cm 3.

  18. Claim 18Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the surface has a surface roughness Ra of no more than 2 nm.

  19. Claim 19Depends on #8

    The single crystal CVD diamond component according to claim 8, wherein the further layer has the single substitutional nitrogen concentration of no more than 200 ppb, said layer being disposed distal to the surface relative to the layer of quantum spin defects.

  20. Claim 20Depends on #1

    The single crystal CVD diamond component according to claim 1, wherein the layer of quantum spin defects is disposed within 200 nm of the surface.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a § 371 national stage of International Application No. PCT/EP2022/068565, filed Jul. 5, 2022, which claims priority to Great Britain Application No. 2109750.6, filed Jul. 6, 2021. FIELD OF THE INVENTION This disclosure relates to a single crystal diamond components, in particular those that include quantum spin defects, and methods for producing the same. BACKGROUND Point defects in synthetic diamond material, particularly quantum spin defects and/or optically active defects, have been proposed for use in various imaging, sensing, and processing applications including: luminescent tags; magnetometers; spin resonance devices such as nuclear magnetic resonance (NMR) and electron spin resonance (ESR) devices; spin resonance imaging devices for magnetic resonance imaging (MRI); and quantum information processing devices such as for quantum communication and computing. Many point defects have been studied in synthetic diamond material including: silicon containing defects such as silicon-vacancy defects (Si — V), silicon di-vacancy defects (Si — V 2 ), silicon-vacancy-hydrogen defects (Si — V:H), silicon di-vacancy hydrogen defects (S — V 2 :H); nickel containing defect; chromium containing defects; and nitrogen containing defects such as nitrogen-vacancy defects (N — V), di-nitrogen vacancy defects (N — V — N), and nitrogen-vacancy-hydrogen defects (N — V — H). These defects are typically found in a neutral charge state or in a negative charge state. It will be noted that these point defects extend over more than one crystal lattice point. The term point defect as used herein is intended to encompass such defects but not include larger cluster defects, such as those extending over ten or more lattice points, or extended defects such as dislocations which may extend over many lattice points. It has been found that certain defects are particularly useful for sensing and quantum processing applications when in th

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Mildren, Rich P. et al.,
  • “
  • Refractive and Diffractive Diamond Optics,
  • ”
  • Chapter 4, p. 130, Optical Engineering of Diamond, Wiley-VCH 2013.
  • Sangtawesin, Sorawis et al.,
  • “
  • Origins of Diamond Durface Noise Probed by Correlating Single-Spin Measurements with Surface Spectroscopy,
  • ”
  • Physical Review X 9(3): 031052(17), 2018.