Method of producing a solid metal carbonate hydrate
Abstract
The present invention relates to a method of producing a solid metal carbonate hydrate by contacting carbon dioxide, water and a metal carbonate to form an aqueous mixture, and applying a vacuum to the aqueous mixture thereby precipitating a metal carbonate hydrate. The invention also relates to solid metal carbonate hydrates obtainable by the aforementioned method. Metal carbonate hydrates are able to increase the alkalinity of aqueous solutions. Accordingly, uses of solid metal carbonate hydrates to increase the alkalinity of a body of water are also included in the invention, as are methods to increase the alkalinity of at least part of a body of water.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.
Claims (13 — 1 Independent, 12 Dependent)
- Claim 1Independent Claim
A method to produce a solid calcium carbonate hydrate comprising: (i) contacting carbon dioxide, water and a metal carbonate to form an aqueous mixture wherein the metal carbonate consists of a calcium carbonate; and (ii) applying a vacuum to the aqueous mixture at temperatures of about 2 to about 15 ° C. thereby precipitating the solid calcium carbonate hydrate.
- Claim 2Depends on #1
The method of claim 1, wherein the vacuum is applied at temperatures of about 5 to about 13 ° C.
- Claim 3Depends on #1
The method of claim 1 wherein the aqueous mixture is a solution.
- Claim 4Depends on #1
The method of claim 1, wherein the carbon dioxide is pressurised to a pressure of greater than about 1 bar, about 1 bar to about 20 bar, about 10 bar to about 18 bar, or about 15 bar.
- Claim 5Depends on #1
The method of claim 1, wherein contacting carbon dioxide, water and a metal carbonate comprises first contacting carbon dioxide and water to form an acidic solution and then contacting the acidic solution with the metal carbonate to form the aqueous mixture.
- Claim 6Depends on #1
The method of claim 1, wherein the calcium carbonate is sourced from limestone.
- Claim 7Depends on #1
The method of claim 1, wherein the solid calcium carbonate hydrate is ikaite.
- Claim 8Depends on #1
The method of claim 1, further comprising venting the aqueous mixture of carbon dioxide prior to applying the vacuum.
- Claim 9Depends on #8
The method of claim 8, wherein the method further comprises recycling the vented carbon dioxide for use in the contacting of step (i).
- Claim 10Depends on #9
The method of claim 9, further comprising recycling the aqueous mixture isolated from the precipitate for use in the contacting of step (i).
- Claim 11Depends on #1
The method of claim 1, wherein applying the vacuum removes carbon dioxide from the aqueous mixture, and the method further comprises recycling the vacuumed carbon dioxide for use in the contacting of step (i).
- Claim 12Depends on #1
The method of claim 1, wherein the method further comprises isolating the precipitate from the aqueous mixture.
- Claim 13Depends on #1
The method of claim 1, wherein the vacuum is applied at pressures of less than about 0.5 bar, about 0.005 to about 0.5 bar or about 0.1 bar.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of United Kingdom Patent Application No. GB 2206475.2 filed on May 4, 2022, the entire disclosures of which are incorporated herein by way of reference. FIELD OF THE INVENTION The present invention relates to a method of producing a solid metal carbonate hydrate. The invention also relates to solid metal carbonate hydrates obtainable by the aforementioned method. BACKGROUND OF THE INVENTION The Paris Agreement [United Nations Framework Convention on Climate Change, 2015], which entered into force in November 2016, aims to hold global temperature changes below 2 ° C. through nationally declared contributions to greenhouse gas emission reductions. Many future scenarios that keep climate change below 2 ° C. do so not only by limiting the use of carbon but also by using technology to limit the impact of carbon use on atmospheric concentrations of CO 2 . These technologies either prevent CO 2 emission into the atmosphere or remove CO 2 from the atmosphere once there. Options for carbon storage include CO 2 injection underground in depleted hydrocarbon reservoirs or saline aquifers, biomass growth, mineralization of natural and waste materials, enhanced ocean productivity and inorganic storage in the ocean. Oceanic uptake has already consumed close to 40% of anthropogenic carbon emissions (Sabine, C. L., and T. Tanhua (2010), An. Rev. Mar. Sci., 2, 175-198). On long timescales the ocean and weathering will reduce atmospheric carbon to values close to preindustrial (Lord, N. S. et al. (2016), Global Biogeochem. Cycles, 30, 2-17). Thus, the issue is not capacity, but rather a question of how to accelerate oceanic carbon uptake and storage in a safe and cost-effective way. The increase in atmospheric CO 2 concentration from preindustrial levels is responsible for a 0.1 decrease in surface water pH. Over the coming 100 years, this is predicted to decrease further by up to 0.4 units (Hoegh-Guldberg O.
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (13)
Non-Patent Literature (2)
- Intellectual Property Office (United Kingdom), Search Report for International Patent Application GB 2206475.2, Nov. 4, 2022.
- European Patent Office, European Search Report for International Patent Application No. EP 23 17 0489, Oct. 17, 2023.