hottub.patents
US 12,763,402 B2#3110752 Most CitedActiveUnited States (USPTO)Utility

Flame-retardant, thermal-insulating, and fireproof material for batteries

0Forward Citations (#3110752 Global)
0.0/yrCitation Velocity (#3110752 Global)
0.00Citation PageRank (#3110752 Global)
4Prior Art Cited
11Claims (3 Indep. · 8 Dep.)
3Drawings / Sheets

Abstract

The present invention discloses a flame-retardant, thermal-insulating, and fireproof material for batteries, and relates to a silicone rubber flame-retardant and thermal-insulating material, which comprises a flame-retardant and thermal-insulating layer and an impact-resistant layer, wherein the flame-retardant and thermal-insulating layer comprises organic silicone rubber, a ceramic-forming filler, a flame retardant, an auxiliary agent, and glass powders with different initial melting temperatures, and molten-state temperature ranges of the glass powders cover 300 ° C. to 1500 ° C. Various glass powders with different molten-state temperature ranges are added to the material, so that when being burned to form a ceramic layer in the temperature range of 300 ° C. to 1500 ° C., the fireproof material always has glass powders in a molten state. The glass powders in the molten state can timely fill holes and cracks that appear at different temperatures in the ceramic layer, and ensure the continuity, integrity, and compactness of the ceramic layer as far as possible, so that the fireproof material has the characteristics of quick ceramic formation at a low temperature and high temperature resistance of about 1500 ° C. The problems that the existing glass powder has a single molten-state temperature range, holes are produced in the ceramic layer due to gasification of the glass powder at a high temperature, the structural compactness is reduced, and the ceramic layer is easily burned through are solved.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 0.

Claims (11 — 3 Independent, 8 Dependent)

  1. Claim 1Independent Claim

    A flame-retardant, thermal-insulating, and fireproof material for batteries, comprising a flame-retardant and thermal-insulating layer and an impact-resistant layer, wherein the flame-retardant and thermal-insulating layer is applied to the surface of the impact-resistant layer; the flame-retardant and thermal-insulating layer and the impact-resistant layer are in a thickness ratio of (2-10):1; the flame-retardant and thermal-insulating layer comprises organic silicone rubber, a ceramic-forming filler, a flame retardant, and an auxiliary agent, and further comprises several glass powders with different initial melting temperatures; molten-state temperature ranges of the several glass powders cover 300 ° C. to 1500 ° C.; and the impact-resistant layer is glass fiber cloth.

  2. Claim 2Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein the impact-resistant layer is formed by bonding multiple layers of glass fiber cloth.

  3. Claim 3Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein the glass powders comprise glass powder A with a molten-state temperature range encompassing 300 ° C. to 700 ° C. and glass powder B with a molten-state temperature range encompassing 700 ° C. to 1500 ° C.; the glass powder A and the glass powder B are in a ratio of (1-2):(1-3) by mass ratio.

  4. Claim 4Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein the glass powders comprise glass powder C with a molten-state temperature range encompassing 300 ° C. to 550 ° C., glass powder D with a molten-state temperature range encompassing 550 ° C. to 900 ° C., and glass powder E with a molten-state temperature range encompassing 900 ° C. to 1500 ° C.; the glass powder C, the glass powder D, and the glass powder E are in a ratio of (1-2):(1-2):(2-3) by mass ratio.

  5. Claim 5Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein the glass powders comprise glass powder F with a molten-state temperature range encompassing 300 ° C. to 800 ° C., glass powder G with a molten-state temperature range encompassing 600 ° C. to 1000 ° C., glass powder H with a molten-state temperature range encompassing 700 ° C. to 1250 ° C., and glass powder I with a molten-state temperature range encompassing 1000 ° C. to 1500 ° C.; the glass powder F, the glass powder G, the glass powder H, and the glass powder I are in a ratio of (1-3):(1-3):(1-3):(1-3) by mass ratio.

  6. Claim 6Depends on #5

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 5, wherein the metal oxide comprises one or more selected from lead oxide, aluminum oxide, lithium oxide, zinc oxide, titanium oxide, magnesium oxide, vanadium oxide, barium oxide, sodium oxide, calcium oxide, strontium oxide, tin oxide, bismuth oxide, and antimony oxide.

  7. Claim 7Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein raw materials of the glass powder comprise one or more selected from silicon oxide, boron oxide, and a metal oxide.

  8. Claim 8Depends on #1

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 1, wherein the flame-retardant, thermal-insulating, and fireproof material will not be burned through under flame impingement at 1500 ° C. for at least 30 min.

  9. Claim 9Independent Claim

    A flame-retardant, thermal-insulating, and fireproof material for batteries, comprising a flame-retardant and thermal-insulating layer and an impact-resistant layer, wherein the flame-retardant and thermal-insulating layer is applied to the surface of the impact-resistant layer; the flame-retardant and thermal-insulating layer and the impact-resistant layer are in a thickness ratio of (2-10):1; the flame-retardant and thermal-insulating layer comprises organic silicone rubber, a ceramic-forming filler, a flame retardant, and an auxiliary agent, and further comprises several glass powders with different initial melting temperatures; molten-state temperature ranges of the several glass powders cover 300 ° C. to 1500 ° C.; wherein the glass powders comprise glass powder F with a molten-state temperature range encompassing 300 ° C. to 800 ° C., glass powder G with a molten-state temperature range encompassing 600 ° C. to 1000 ° C., glass powder H with a molten-state temperature range encompassing 700 ° C. to 1250 ° C., and glass powder I with a molten-state temperature range encompassing 1000 ° C. to 1500 ° C.; the glass powder F, the glass powder G, the glass powder H, and the glass powder I are in a ratio of (1-3):(1-3):(1-3):(1-3) by mass ratio; wherein the raw materials of the glass powder further comprise stannous fluoride.

  10. Claim 10Independent Claim

    A flame-retardant, thermal-insulating, and fireproof material for batteries, comprising a flame-retardant and thermal-insulating layer and an impact-resistant layer, wherein the flame-retardant and thermal-insulating layer is applied to the surface of the impact-resistant layer; the flame-retardant and thermal-insulating layer and the impact-resistant layer are in a thickness ratio of (2-10):1; the flame-retardant and thermal-insulating layer comprises organic silicone rubber, a ceramic-forming filler, a flame retardant, and an auxiliary agent, and further comprises several glass powders with different initial melting temperatures; molten-state temperature ranges of the several glass powders cover 300 ° C. to 1500 ° C.; wherein the flame-retardant and thermal-insulating layer comprises, in parts by mass, 40-60 parts of the organic silicone rubber, 20-30 parts of the ceramic-forming filler, 15-25 parts of the flame retardant, 2-10 parts of the glass powders, and 2-5 parts of the auxiliary agent.

  11. Claim 11Depends on #10

    The flame-retardant, thermal-insulating, and fireproof material for batteries according to claim 10, wherein the flame-retardant and thermal-insulating layer further comprises 10-17 parts of an extending filler.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS The present application is a 371 of international Application PCT/CN2023/120328, filed Sep. 21, 2023, which claims the priority to Chinese Patent Application No. 202211274999.X, filed in China on Oct. 18, 2022. The contents of the applications are incorporated herein by reference in their entireties. TECHNICAL FIELD The present invention relates to a silicone rubber flame-retardant, thermal-insulating, and fireproof material, in particular to a flame-retardant, thermal-insulating, and fireproof material for new energy vehicle battery packs. BACKGROUND Generally, the thermal runaway probability of a battery is one in ten million. However, in an electric vehicle, after thousands of batteries are integrated to form a battery pack, the thermal runaway probability of the battery pack is increased to one in ten thousand, and one battery thermal runaway may cause the thermal runaway of the whole battery pack. The combustion temperature of the battery pack after the thermal runaway can reach 1500 ° C., and there is also a strong impact, which is a great challenge to the safety of the electric vehicle. Studies have shown that ceramic silicone rubber is currently the most suitable material scheme for use in new energy vehicle battery packs to prevent the continuous thermal runaway of cells and avoid the ignition of adjacent modules. The ceramic silicone rubber is a ceramifiable polymer composite material, which has excellent performance of common polymers at room temperature and can form a compact ceramic structure at a high temperature so as to have ceramic characteristics. Due to the relatively high bond energy of Si — O bond in the silicone rubber, the silicone rubber itself has good thermal stability. In addition, when the silicone rubber is burned under a high-temperature flame, the Si — O bond can be converted into continuous, antioxidative, and insulating network SiO 2 ash to cover the surface of the cell, so that further ablatio

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (4)

Non-Patent Literature (7)

  • Machine translation of CN106280446. Retrieved Feb. 2, 2026.
  • Machine translation of CN107141811. Retrieved Feb. 2, 2026.
  • Lou et al.
  • “
  • Preparation and properties of ceramifiable flame-retarded silicone rubber composites
  • ”
  • , Journal of Thermal Analysis and Calorimetry, (2017); pp. 813-821.