hottub.patents
US 12,757,698 B2#3116433 Most CitedActiveUnited States (USPTO)Utility

Method for gapfill

0Forward Citations (#3116433 Global)
0.0/yrCitation Velocity (#3116433 Global)
0.00Citation PageRank (#3116433 Global)
6Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

A method of gap fill may include depositing a sacrificial Si layer in an opening of a feature and on a field of a substrate. In addition, the method may include depositing a metal layer in the opening and on the field, where at least a portion of the sacrificial Si layer is replaced with the metal layer. The method may also include depositing a metal gapfill material in the opening and on the field directly over the metal layer, where the metal gapfill material completely fills the opening.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for metal gapfill, comprising: depositing a conformal sacrificial Si layer having a thickness of less than or equal to about 4 nm in an opening of a feature and on a field of a substrate; depositing a conformal metal layer in the opening and on the field, wherein at least 95 wt % of the sacrificial Si layer is replaced with the conformal metal layer; and depositing a metal gapfill material in the opening and on the field directly over the conformal metal layer, wherein the metal gapfill material completely fills the opening; wherein the depositing the conformal metal layer comprises atomic layer deposition, comprising contacting the sacrificial Si layer with a metal precursor according to formula I; MXa; (I) wherein M is cobalt, wherein X is fluorine or chlorine; and a is from 2 to 6; and wherein the conformal sacrificial Si layer is deposited over a base metal layer comprising the same metal as the conformal metal layer.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the conformal metal layer is deposited using thermal atomic layer deposition or plasma enhanced atomic layer deposition, at a temperature of greater than or equal to about 200 ° C.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the conformal metal layer has a thickness of less than or equal to about 15 nm.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the conformal metal layer has a thickness from about 5 nm to about 10 nm.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the base metal layer is deposited anisotropically via physical vapor deposition or chemical vapor deposition, followed by the depositing the conformal sacrificial Si layer, in an integrated process without a vacuum break therebetween.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the conformal sacrificial Si layer is deposited using plasma enhanced atomic layer deposition.

  7. Claim 7Depends on #1

    The method of claim 1, wherein the metal gapfill material comprises the same metal as the conformal metal layer.

  8. Claim 8Depends on #1

    The method of claim 1, wherein the metal gapfill material is deposited via physical vapor deposition or chemical vapor deposition.

Technical Overview & Description

RELATED APPLICATION This application is a continuation-in-part of and claims the benefit of priority to U.S. patent application Ser. No. 18/070,185 filed Nov. 28, 2022, the entire disclosure of which is incorporated by reference herein. FIELD Embodiments of the present principles generally relate to methods for gapfill of semiconductor substrates. BACKGROUND When semiconductor devices are manufactured, the devices are formed with contacts to allow electrical connectivity to the device by other devices or for electrical connections external to a chip or circuit. The contacts are made with metal materials that promote electrical conductivity. The higher the conductivity, the less the resistivity. The inventors have observed that current manufacturing techniques produce contacts with high resistivity which reduces electrical conductivity and may cause thermal issues due to resistive heating in the contact, resulting in poor performance and reduced reliability. Thus, the inventors have provided improved methods for gapfill when forming contacts having low resistivity and increased reliability. SUMMARY Embodiments of the present disclosure relate to methods for gapfill of features in a substrate. In embodiments, a method for gapfill may include depositing a sacrificial Si layer in an opening of a feature and on a field of a substrate; depositing a metal layer in the opening and on the field, where at least a portion of the sacrificial Si layer is replaced with the metal layer; and depositing a metal gapfill material in the opening and on the field directly over the metal layer, where the metal gapfill material completely fills the opening. In embodiments, a method for gapfill may include depositing a sacrificial Si layer atop a base metal layer in an opening of a feature and on a field of a substrate; performing an atomic layer deposition process atop the sacrificial Si layer to replace Si atoms with metal atoms and create a metal layer atop the base metal layer in the o

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (6)

PatentTitleYearCitations

Non-Patent Literature (1)

  • PCT International Search Report and Written Opinion for PCT/US2023/035658 dated Feb. 16, 2024.