Polyolefin formulation containing combination of voltage stabilizer compounds
Abstract
A polyolefin formulation comprising (A) a polyolefin polymer: x weight percent (wt %) of (B) an alkoxyphenol compound of formula (I); and y wt % of (C) a benzophenone compound of formula (II) as described in the specification: wherein y is from 1 to 8 wt %; wherein x is from 0.1 to 3.0 wt %, with the proviso that x is less than 0.5y; and wherein wt % are based on total weight of the polyolefin formulation. Also crosslinked products made therefrom; methods of making and using same; and articles containing same.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 0.
Claims (12 — 1 Independent, 11 Dependent)
- Claim 1Independent Claim
A polyolefin formulation comprising (A) a polyolefin polymer; x weight percent (wt %) of (B) an alkoxyphenol compound of formula (I): wherein R1 is a (C1-C20) alkyl; and y wt % of (C) a benzophenone compound of formula (II): wherein Ar1 is phenyl or an alkylphenyl; wherein y is from 1 to 8 wt %; wherein x is from 0.1 to 3.0 wt %, with the proviso that x is less than 0.5y; and wherein wt % are based on total weight of the polyolefin formulation.
- Claim 2Depends on #1
The polyolefin formulation of claim 1 wherein the Ar1 is phenyl; and R1 is selected from the group consisting of: (i) (C1-C5)alkyl; (ii) (C6-C10alkyl; (iii) methyl; and (iv) heptyl; or wherein the Ar1 is an alkylphenyl; and R1 is selected from the group consisting of: (i) (C1-C5)alkyl; (ii) (C6-C10)alkyl; (iii) methyl; and (iv) heptyl.
- Claim 3Depends on #2
The polyolefin formulation of claim 2 wherein the R1 is methyl or heptyl and the Ar1 is phenyl.
- Claim 4Depends on #1
The polyolefin formulation of claim 1 wherein the (A) polyolefin polymer is selected from the group consisting of: a low-density polyethylene polymer, an ethylene/(C4-C20)alpha-olefin copolymer, an ethylene/(unsaturated carboxylic ester) copolymer, an ethylene/(monocyclic organosiloxane) copolymer, an ethylene/propylene copolymer, an ethylene/propylene/(diene monomer) terpolymer, and a propylene homopolymer.
- Claim 5Depends on #1
The polyolefin formulation of claim 1 comprising from 50.0 to 99.7 weight percent (wt %) of the (A) polyolefin polymer; from x=0.2 wt % to x=0.9 wt % of the (B) alkoxyphenol compound; from 1.6 to 7.4 wt % of the (C) benzophenone compound; and a total of from 0.1 to 43 wt % of at least one additive, wherein each of the at least one additive is different than constituents (A), (B), and (C) and is independently selected from the group consisting of: (D) an organic peroxide; (E) an anti-scorch agent; (F) an antioxidant; (G) a filler; (H) a flame retardant; (I) a hindered amine stabilizer; (J) a tree retardant; (K) a methyl radical scavenger; (L) a crosslinking coagent; (M) a processing aid; (N) a colorant; and a combination of any two or more of additives (D) to (N).
- Claim 6Depends on #5
The polyolefin formulation of claim 5 comprising from 85 to 99.5 weight percent (wt %) of the (A) polyolefin polymer, which is a low-density polyethylene polymer; from 0.30 to 0.50 wt % of the (B) alkoxyphenol compound that is a compound of formula (I) wherein R1 is methyl or heptyl; from 1.5 to 2.4 wt % of the (C) benzophenone compound of formula (II) wherein Ar1 is phenyl; and from 0.1 to 1.5 wt % of at least one (F) antioxidant.
- Claim 7Depends on #1
A method of making the polyolefin formulation of claim 1, the method comprising mixing the (A) polyolefin polymer with the (B) alkoxyphenol compound and the (C) benzophenone compound, and, optionally, at least one additive, in such a way so as to make the formulation.
- Claim 8Depends on #1
A method of making a crosslinked polyolefin product, the method comprising subjecting the polyolefin formulation of claim 1 to a curing condition in such a way so as to crosslink the (A) polyolefin polymer, thereby making the crosslinked polyolefin product.
- Claim 9Depends on #8
A crosslinked polyolefin product made by the method of claim 8.
- Claim 10Depends on #9
An article comprising the polyolefin formulation of, the crosslinked polyolefin product of claim 9.
- Claim 11Depends on #10
A method of transmitting electricity, the method comprising applying a voltage across the conductive core of the coated conductor of claim 10 so as to generate a flow of electricity through the conductive core.
- Claim 12Depends on #9
A coated conductor comprising a conductive core and an insulation layer at least partially covering the conductive core, wherein the insulation layer comprises the crosslinked polyolefin product of claim 9.
Technical Overview & Description
The technical field includes polyolefin formulations for wires and cables. INTRODUCTION Patents in the field include U.S. Pat. Nos. 3,413,263, 6,696,154B2, 8,680,399B2, 9,133,320B2, and U.S. Pat. No. 9,343,198B2. Patent application publications in the field include EP0111043A1, EP2886595, GB1461331A, US20160304699A1, US20160312007A1, WO2010028721A1, WO2012044521, WO2014209661A1, and WO2014172107A1. Publications include About The Significance Of Peroxide Decomposition Products In XLPE Cable Insulations, by H. Wagner and J. Wartusch, IEEE Trans. Electr. Insul, vol. El-12, no. 6, December 1977. Insulated electrical conductors typically comprise a conductive core covered by an insulation layer. The conductive core may be solid or stranded (e.g., a bundle of wires). Some insulated electrical conductors may also contain one or more additional elements such as semiconducting layer(s) and/or a protective jacket (e.g., wound wire, tape, or sheath). Examples are coated metal wires and electrical power cables, including those for use in low voltage ( “ LV ” , > 0 to < 5 kilovolts (kV)), medium voltage ( “ MV ” , 5 to < 69 kV), high voltage ( “ HV ” , 69 to 230 kV) and extra-high voltage ( “ EHV ” , > 230 kV) power cables and their electricity-transmitting/distributing applications. Evaluations of power cables may use AEIC/ICEA specifications and standards and/or IEC test methods. A majority of high and extra-high voltage power cables contain an insulation layer composed of an insulation material that comprises a host polymer and one or more additives. The additive(s) may include antioxidants, a colorant, and/or a hindered amine stabilizer. Electrical breakdown strength (also known as dielectric strength) of the insulation material determines how thick the insulation layer needs to be to satisfy industry specifications for performance of power cables at a particular voltage. All other things being equal, an insulation material having a higher electrical breakdown strength allow
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (30)
Non-Patent Literature (7)
- Wagner,
- “
- About the Significance of Peroxide Decomposition Products in XLPE Cable Insulations
- ”
- , IEEE Trans. Electr. Insul, 1977, p. 395-401, vol. E1-12, No. 6.
- International Search Report and Written Opinion from corresponding International Application No. PCT/US2022/039004 dated Nov. 22, 2022.
- Office Action from corresponding Taiwan application No. 111128742 dated Dec. 15, 2025.