Provided are a cathode material and a preparation method therefor, a cathode sheet and a sodium-ion battery. The cathode material includes a composite particle, a molecular formula of the composite particle is Na 4 M x Mn 1-x/2 V(PO 4 ) 3-x/3 N x , wherein 0.001 ≤ x ≤ 0.05, M is Li and/or K, and N is selected from one or more of F, Cl, Br, and I. According to the present disclosure, by synchronously introducing specific types and contents of anions and cations into a polyanionic phosphate active cathode material to achieve a good synergistic effect between the anions and cations, the particle morphology and size of the material are regulated while the intrinsic conductivity and structural stability of the cathode material are greatly improved, and significant improvement of the comprehensive performance, such as specific capacity, rate capability, cycle stability and compaction density, of the material is promoted.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (20 — 2 Independent, 18 Dependent)
- Claim 1Independent Claim
A cathode material, wherein the cathode material comprises a composite particle, a molecular formula of the composite particle is Na 4 M x Mn 1-x/2 V(PO 4) 3-x/3 N x, wherein 0.001 ≤ x ≤ 0.05, M is Li and/or K, and N is selected from one or more of F, Cl, Br, and I.
- Claim 2Depends on #1
The cathode material according to claim 1, wherein in the molecular formula of the composite particle, 0.001 ≤ x ≤ 0.01, M is Li and/or K, and N is selected from one or more of F, Br, and I.
- Claim 3Depends on #2
The cathode material according to claim 2, wherein, the molecular formula of the composite particle is Na 4 M 0.01 Mn 0.995 V(PO 4) 2.997 N 0.01, wherein M is Li and/or K, and N is selected from one or more of F, Br, and I.
- Claim 4Depends on #3
The cathode material according to claim 3, wherein the molecular formula of the composite particle is Na 4 K 0.01 Mn 0.995 V(PO 4) 2.997 F 0.01, Na 4 Li 0.01 Mn 0.995 V(PO 4) 2.997 F 0.01, Na 4 K 0.01 Mn 0.995 V(PO 4) 2.997 Br 0.01, Na 4 K 0.01 Mn 0.995 V(PO 4) 2.997 I 0.01, Na 4 K 0.001 Mn 0.9995 V(PO 4) 2.9997 F 0.001, or Na 4 K 0.05 Mn 0.975 V(PO 4) 2.983 F 0.05.
- Claim 5Depends on #2
The cathode material according to claim 2, wherein, the molecular formula of the composite particle is Na 4 M 0.001 Mn 0.9995 V(PO 4) 2.9997 N 0.001, wherein M is Li and/or K, and N is F.
- Claim 6Depends on #1
The cathode material according to claim 1, wherein the cathode material further includes a carbon coating layer coated on outer surface of the composite particle, and calculated with a total weight of the cathode material as 100%, a mass fraction of the carbon coating layer is 1%-5%.
- Claim 7Depends on #6
The cathode material according to claim 6, wherein calculated with the total weight of the cathode material as 100%, the mass fraction of the carbon coating layer is 2.0%-2.5%.
- Claim 8Depends on #1
A cathode sheet, wherein the cathode sheet comprises the cathode material according to claim 1.
- Claim 9Depends on #8
A sodium-ion battery, wherein the sodium-ion battery comprises the cathode sheet according to claim 8.
- Claim 10Independent Claim
A method for preparing a cathode material, comprising: preparing a sodium source, a doping element source, a manganese source, a vanadium source and a phosphorus source into a mixed slurry; and sequentially subjecting the mixed slurry to drying and calcination to obtain a cathode material; wherein the cathode material comprises a composite particle, a molecular formula of the composite particle is Na 4 M x Mn 1-x/2 V(PO 4) 3-x/3 N x, wherein 0.001 ≤ x ≤ 0.05, M is Li and/or K, and N is selected from one or more of F, Cl, Br, and I.
- Claim 11Depends on #10
The method for preparing a cathode material according to claim 10, wherein the calcination sequentially comprises: first-stage calcination with a temperature being 320 ° C.-370 ° C. and a temperature-holding time for the first-stage calcination being 3 h-5 h; and second-stage calcination with a temperature being 700 ° C.-750 ° C. and a temperature-holding time for the second-stage calcination being 7 h-9 h.
- Claim 12Depends on #11
The method for preparing a cathode material according to claim 11, wherein the drying is spray drying, and the spray drying is carried out at an air inlet temperature of 200 ° C.-250 ° C. and an air outlet temperature of 100 ° C.-140 ° C.
- Claim 13Depends on #12
The method for preparing a cathode material according to claim 12, wherein the doping element source is selected from one or more of potassium fluoride, lithium fluoride, potassium bromide, and potassium iodide.
- Claim 14Depends on #11
The method for preparing a cathode material according to claim 11, wherein the first-stage calcination and the second-stage calcination are both carried out under the protection of an inert gas.
- Claim 15Depends on #10
The method for preparing a cathode material according to claim 10, wherein the sodium source is selected from one or more of sodium acetate, sodium carbonate, sodium hydroxide, and sodium nitrate.
- Claim 16Depends on #10
The method for preparing a cathode material according to claim 10, wherein the manganese source is selected from one or more of manganese acetate tetrahydrate, manganese nitrate, manganese phosphate, and manganese oxalate.
- Claim 17Depends on #10
The method for preparing a cathode material according to claim 10, wherein the vanadium source is selected from one or more of ammonium metavanadate, ammonium vanadate, and ammonium sulfate.
- Claim 18Depends on #10
The method for preparing a cathode material according to claim 10, wherein the phosphorus source is selected from one or more of ammonium dihydrogen phosphate, ammonium monohydrogen phosphate, ammonium phosphate, and phosphoric acid.
- Claim 19Depends on #10
The method for preparing a cathode material according to claim 10, wherein the step of preparing the mixed slurry includes: preparing a carbon source into a carbon source solution with a concentration of 0.18 mol/L-0.20 mol/L, adding the sodium source, the doping element source, the manganese source, the vanadium source and the phosphorus source into the carbon source solution, and carrying out stirring to obtain the mixed slurry.
- Claim 20Depends on #19
The method for preparing a cathode material according to claim 19, wherein the carbon source is selected from one or more of glucose, citric acid monohydrate, and soluble starch.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application is a National Stage Entry under 35 U.S.C. § 371 of PCT International Application No PCT/CN2025/071356 filed on Jan. 8, 2025, which claims priority to Chinese Patent Application No. 202510019534.7 filed to the China National Intellectual Property Administration on Jan. 6, 2025 and entitled “ CATHODE MATERIAL AND PREPARATION METHOD THEREFOR, CATHODE SHEET AND SODIUM-ION BATTERY ” , the entire disclosures of each of which are hereby incorporated by reference. TECHNICAL FIELD The present disclosure relates to the technical field of sodium-ion batteries, and specifically relates to a cathode material and a preparation method therefor, a cathode sheet and a sodium-ion battery. BACKGROUND Sodium-ion batteries are expected to become good substitutes for lithium-ion batteries because of abundant sodium resources, low prices and similar electrochemical behaviors to lithium. Due to cost effectiveness, environmental friendliness, safety, temperature adaptability, a fast charging capability and a relatively long cycle life, the sodium-ion batteries have been considered as a promising alternative solution in battery technologies of new energy vehicles. With advances in technology, the sodium-ion batteries are expected to become one of the mainstream battery technologies of the new energy vehicles in the next few years to provide more lasting and safer power for electric vehicles. Cathodes are used as important parts of the sodium-ion batteries, and the performance of which has an important impact on various indicators of the entire batteries. Common sodium-ion cathode materials, such as layered transition metal oxides, Prussian blue compounds and polyanionic compounds, etc., all have the disadvantages of low specific energy and poor cycle stability, which will hinder commercial development and practical application. Therefore, it is urgent to develop cathode materials with excellent electrochemical performance for the sodiu
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
Non-Patent Literature (10)
- The granted search report of counterpart CN application No. 202510019534.7 was issued on Sep. 17, 2025.
- Gao, X. et al:
- “
- phase transformation, charge transfer, and ionic diffusion of NA4MNV(PO4)3 in sodium-ion batteries:a combined first-principles and experimental study
- ”
- ;J.Mater.Chem.A;Jul. 27, 2020;DOI: 10.1039/d0ta05929c; pp. 17477-17486.
- The office action of counterpart KR application No. 10-2025-7007063 was issued on Dec. 18, 2025.
- Zhang et al., Boosting rate and cycling performance of K-doped Na3V2(PO4)2F3 cathode for high-energy-density sodium-ion batteries, Green Energy
- &
- Environment Jul. 2022, pp. 1253-1262, Feb. 1, 2021.