Abstract

Particular embodiments may provide a solid sulfide electrolyte. Specifically, disclosed herein are methods and systems that can include feeding polymer precursors and sulfides to an extruder, kneading the polymer precursors and the sulfide in the extruder to form a sulfide-polymer composite that includes polyurethane and sulfide, and extruding the sulfide-polymer composite to form a solid sulfide electrolyte.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (20 — 1 Independent, 19 Dependent)

  1. Claim 1Independent Claim

    A method, comprising: feeding a polyol, an isocyanate, and a sulfide into an extruder, wherein the polyol, the isocyanate, and the sulfide are fed into different zones of the extruder; kneading the polyol, the isocyanate, and the sulfide in the extruder to form a sulfide-polymer composite comprising thermoplastic polyurethane and the sulfide; and extruding the sulfide-polymer composite to form a solid electrolyte layer, wherein the extruder is a heated twin screw extruder and all temperatures along a length of a screw barrel of the heated twin screw extruder are between 80-120 ° C.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the sulfide comprises at least about 75% of a total weight of the polyol, isocyanate, and sulfide fed into the extruder.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the sulfide is a ceramic sulfide.

  4. Claim 4Depends on #1

    The method of claim 1, wherein an amount of solvent fed to the extruder is such that the solvent is less than 5 wt. % the total weight of all components fed into the extruder.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the polyol comprises polybutadiene diol, polyester diol, or combinations thereof.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the polyol has a molecular weight of 500-5000 g/mol.

  7. Claim 7Depends on #1

    The method of claim 1, wherein the isocyanate comprises aliphatic diisocyanate, aromatic diisocyanate, or combinations thereof.

  8. Claim 8Depends on #1

    The method of claim 1, wherein a ratio of polyol to isocyanate fed into the extruder is 0.5-1.5.

  9. Claim 9Depends on #1

    The method of claim 1, wherein all temperatures along the length of the screw barrel of the heated twin screw extruder are between 80-115 ° C.

  10. Claim 10Depends on #1

    The method of claim 1, wherein the solid electrolyte layer has a thickness of 15-100 microns.

  11. Claim 11Depends on #1

    The method of claim 1, further comprising extruding the sulfide-polymer composite on a substrate comprising lithium metal.

  12. Claim 12Depends on #1

    The method of claim 1, further comprising feeding a lubricant into the extruder and/or feeding a solvent compatible with the sulfide into the extruder.

  13. Claim 13Depends on #1

    The method of claim 1, wherein the sulfide has a formula of: Li 7-a-b PS 6-a-b X a Y b wherein X is Cl, Br or I; Y is Cl, Br or I; 0 < a < 2; 0 < b < 2.

  14. Claim 14Depends on #1

    The method of claim 1, wherein the sulfide has a formula of: Li 7-a-b PS 6-a-b-c Z c X a Y b wherein X is F, Cl, Br or I; Y is F, Cl, Br or I; Z is O, or Se; 0 ≤ a < 2; 0 ≤ b < 2; 0 ≤ c ≤ 6.

  15. Claim 15Depends on #1

    The method of claim 1, wherein the sulfide has a formula of: xLi 2 S y P 2 S 5 wherein 0 < x < 100; 0 < y < 100.

  16. Claim 16Depends on #1

    The method of claim 1, wherein the sulfide has a formula of: Li 7-x X 1-y P y S 6-z Y z wherein X is B, N, As, Sb, Al, Si, Ge, Ga, Sn; Y is F, Cl, Br, I; 0 < x < 2; 0 ≤ y < 1; 0 ≤ z ≤ 2.

  17. Claim 17Depends on #1

    The method of claim 1, wherein the sulfide has a formula of: Li 8-x M 1-x M ′ x S 4-y O y wherein M is Si or Ge; M ′ is P, Al, Zn, Ga, Sb or V; 0 < x < 1.6; 0 ≤ y < 4.

  18. Claim 18Depends on #1

    The method of claim 1, wherein the sulfide comprises at least about 85% of a total weight of the polyol, isocyanate, and sulfide fed into the extruder.

  19. Claim 19Depends on #1

    The method of claim 1, wherein the sulfide comprises at least about 95% of a total weight of the polyol, isocyanate, and sulfide fed into the extruder.

  20. Claim 20Depends on #1

    The method of claim 1, wherein the sulfide comprises about 75-99.9 wt. % of a total weight of the polyol, isocyanate, and sulfide fed into the extruder.

Technical Overview & Description

INTRODUCTION The disclosure is generally directed to solid sulfide electrolytes and systems and methods of making such electrolytes, which can be used in lithium-ion batteries. BRIEF SUMMARY Some sulfide electrolytes may not be chemically compatible with polar solvents. Specifically, the poor compatibility with polar solvents can force the selection of polymer binders that are soluble in nonpolar solvents to manufacture various layers for a battery cell. The quality and uniformity of the electrode (crack free), and cohesion and adhesion between binder and particles can depend on the polymer-sulfide interaction, glass transition temperature, and elastic modulus. However, most of these properties can depend on the chemical structure of the polymer backbone. In general, sulfides are polar in nature and currently used binders (such as styrene-isoprene-styrene (SIS), styrene-ethylene/butylene-styrene (SEBS), etc.) are nonpolar. Thus, the microphases of such sulfide electrolytes may separate at the molecular level resulting in brittle films. These films may require high stack pressure to make good contact with Li metal and composite cathodes which can exacerbate embrittlement. The next generation of binders for sulfide electrolytes should be able to balance hydrophobic and hydrophilic groups to have good compatibility with sulfides, conformal coating, good adhesion, and elasticity. The more hydrophilic portion of block copolymers (e.g., polyacrylonitrile-polystyrene (PS-PAN)) with PAN > 30 wt % may not be soluble in the solvents that are compatible with sulfides, limiting the selection of binders with better properties. Thus, today's solutions to these problems focus on finding the right solvent for the known binders even though they may not be the best for adhesion and/or interfacial contact and/or finding the binders that are soluble in sulfide compatible solvents. However, these solutions may not be that advantageous because of polarity mismatch between ideal binders a

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (8)