Metal-on-metal deposition methods for filling a gap feature on a substrate surface
Abstract
Molybdenum (Mo) metal-on-metal (MoM) deposition methods for providing true bottom-up fill in vias and/or other gap features in device structures. These device structures contain metal at the bottom surface and have dielectric sidewalls. The deposition process provides molybdenum growth only, in some cases, on the metal film/layer to provide a selective process that can be called a metal-on-metal (MoM) process. The Mo MoM deposition process described herein are not limited to thin films (e.g., films less than 50 Å ) and can be used to deposit thicker films (e.g., greater than 50 Å in some cases and greater than 200 Å in other useful cases) on metal surfaces while no, or substantially no, deposition is found on dielectric surfaces.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.
Claims (19 — 3 Independent, 16 Dependent)
- Claim 1Independent Claim
A method for filling a gap feature on a substrate surface, comprising: providing a substrate with a surface comprising a gap feature in a reaction chamber, wherein the gap feature includes a dielectric sidewall and a metal base; partially filling the gap feature with a molybdenum film with a cyclical chemical vapor deposition (cyclical CVD) process, wherein the molybdenum film is selectively deposited on the metal base and wherein a cycle of the cyclical chemical vapor deposition process comprises: providing a molybdenum precursor comprising one or more of MoCl 5 and MoCl 4 in the reaction chamber; and providing a reactant in the reaction chamber to form a layer of the molybdenum film; and repeating the partially filling the gap step until the molybdenum film has at least a predefined thickness.
- Claim 2Depends on #1
The method of claim 1, wherein the metal base comprises a metal selected from the group consisting of tungsten (W), titanium nitride (TiN), ruthenium (Ru), cobalt (Co), and copper (Cu).
- Claim 3Depends on #1
The method of claim 1, wherein the reactant is a reducing agent.
- Claim 4Depends on #1
The method of claim 1, wherein a thickness of molybdenum grown on the dielectric surface is substantially 0 Å.
- Claim 5Depends on #1
The method of claim 1, wherein the molybdenum precursor comprises MoCl 4.
- Claim 6Depends on #1
The method of claim 1, wherein the molybdenum precursor is MoCl 4.
- Claim 7Depends on #1
The method of claim 1, wherein the reactant is continuously provided during the cycle of the cyclical chemical vapor deposition process.
- Claim 8Depends on #7
The method of claim 7, further comprising heating the substrate to a substrate temperature in the range of 350 to 450 ° C. and maintaining the reaction chamber at a pressure in the range of 10 to 100 Torr during the partially filling the gap step.
- Claim 9Depends on #7
The method of claim 7, wherein the reactant consists of hydrogen (H 2).
- Claim 10Depends on #1
The method of claim 1, wherein the predefined thickness is greater than 50 Å and wherein the molybdenum film selectively grows on the metal film relative to the dielectric sidewall for at least the predefined thickness.
- Claim 11Depends on #1
The method of claim 1, wherein the predefined thickness is in the range of 20 to 600 Å and wherein the molybdenum film selectively grows on the metal film relative to the dielectric sidewall for at least the predefined thickness.
- Claim 12Independent Claim
A method of bottom-up filling a gap feature on a surface of a substrate, comprising surface cleaning a substrate with a gap feature having sidewalls with dielectric surface and a bottom surface with a metal film to remove metal oxides from the metal film; after the surface cleaning, providing the substrate in a reaction chamber; heating the substrate to a substrate temperature greater than 350 ° C.; contacting the substrate with a molybdenum precursor comprising one or more of MoCl 5 and MoCl 4 by periodically pulsing the molybdenum precursor; contacting the substrate with a reducing agent, wherein contacting the substrate with the reducing agent comprises continuously providing the reducing agent during the step of contacting the substrate with the molybdenum precursor; and repeating the contacting steps until a molybdenum film is formed on the metal film on the bottom surface of the gap feature, wherein the molybdenum film is formed with a selectivity of at least 50:1 between the metal film and the dielectric surface.
- Claim 13Depends on #12
The method of claim 12, wherein the molybdenum film has a thickness of at least 200 Å.
- Claim 14Depends on #12
The method of claim 12, wherein the metal film comprises a metal selected from the group consisting of W, TiN, Ru, Co, and Cu.
- Claim 15Depends on #12
The method of claim 12, wherein the molybdenum precursor comprises MoCl 5 and wherein the substrate temperature is in the range of 350 to 550 ° C.
- Claim 16Depends on #12
The method of claim 12, wherein the molybdenum precursor comprises MoCl 4.
- Claim 17Independent Claim
A method for selectively depositing a molybdenum film on a semiconductor device structure, comprising: providing a device structure in a reaction chamber, wherein the device structure comprises a substrate including a dielectric surface and a metal surface; partially forming a molybdenum film selectively on the metal surface with a cyclical chemical vapor deposition (cyclical CVD) process, wherein a unit cycle of the cyclical chemical vapor deposition process comprises: providing a molybdenum precursor in the reaction chamber; purging the molybdenum precursor from the reaction chamber; and providing a reactant in the reaction chamber, wherein the reactant comprises a reducing agent; repeating the partially forming the molybdenum film step until the molybdenum film has a thickness greater than 200 Å and wherein a thickness of molybdenum grown on the dielectric surface is substantially 0 Å.
- Claim 18Depends on #17
The method of claim 17, wherein the metal surface comprises a metal selected from the group consisting of W, TiN, Ru, Co, and Cu and wherein the molybdenum precursor is selected from the group consisting of MoCl 5, MoCl 4, MoO 2 Cl 2, and MoOCl 4.
- Claim 19Depends on #18
The method of claim 18, wherein the method further comprises, prior to the partially forming the molybdenum film step, heating the substrate to a substrate temperature in the range of 350 to 550 ° C. when the molybdenum precursor comprises MoCl 5 or MoCl 4 and in the range of 350 to 450 ° C. when the molybdenum precursor comprises MoO 2 Cl 2 or MoOCl 4.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application is a nonprovisional of, and claims priority to and the benefit of, U.S. Provisional Patent Application No. 63/282,217, filed Nov. 23, 2021 and entitled “ METAL-ON-METAL DEPOSITION METHODS FOR FILLING A GAP FEATURE ON A SUBSTRATE SURFACE, ” which is hereby incorporated by reference herein. FIELD OF INVENTION The present disclosure relates generally to methods for filling a gap feature on a substrate surface and particularly to methods for filling one or more gap features with a molybdenum (Mo) metal film utilizing Mo metal-on-metal (MoM) selective bottom-up fill deposition processes. The present disclosure also generally relates to semiconductor device structures including one or more gap features filled with a molybdenum metal film. BACKGROUND OF THE DISCLOSURE Semiconductor fabrication processes for forming semiconductor device structures, for example, transistors, memory elements, and integrated circuits, are wide ranging and may include deposition processes, etch processes, thermal annealing processes, lithography processes, and doping processes, amongst others. A particular semiconductor fabrication process commonly utilized is the deposition of a metal film into a gap feature thereby filling the gap feature (which may include a gap, a trench, a via, and the like) with the metal film, a process commonly referred to as “ gap fill. ” Substrates used during the manufacture of semiconductor devices may comprise a multitude of gap features on a substrate with a non-planar surface. The gap features may comprise substantially vertical gap features being disposed between protruding portions of the substrate surface or indentations formed in a substrate surface. The gap features may also comprise substantially horizontal gap features being disposed between two adjacent materials bounding the horizontal gap feature. As semiconductor device structure geometries have decreased and high aspect ratio features have becom
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (80)
Non-Patent Literature (10)
- Juppo, Marika et al.,
- “
- Deposition of molybdenum thin films by an alternate supply of MoCl 5 and Zn,
- ”
- J. Vac. Sci. Technol. A 16(5), Sep./Oct. 1998; 2845-2850.
- Bhave, Mandar, et al.,
- “
- Developer-soluble Gap fill materials for patterning metal trenches in Via-first Dual Damascene process
- ”
- . Proc. SPIE 5376, Advances in Resist Technology and Processing XXI, (May 14, 2004); pp. 640-647.