Process for making a coated cathode active material
Abstract
Described herein is a process for making an electrode active material according to general formula Li 1+ (TM 1-y M 1 y ) 1-x O 2 , where TM includes a combination of Ni and at least one of Co, Mn and Al, M 1 is selected from the group consisting of Nb, Ta, and at least one of Co, Mn and Al, y is in a range of from 0.001 to less than 0.01, and x is in a range of from zero to 0.2, said process including the following steps: (a) mixing (A) a mixed oxide or (oxy)hydroxide of Mn, Co and Ni, and (B) at least one lithium compound selected from the group consisting of lithium hydroxide, lithium oxide and lithium carbonate, and (C) an amorphous compound of Nb or Ta, and (b) subjecting said mixture to heat treatment, where at least 60 mole-% of a transition metal of TM is Ni.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 0.
Claims (12 — 2 Independent, 10 Dependent)
- Claim 1Independent Claim
Process A process for making an electrode active material according to general formula Li 1+x (TM 1-y M 1 y) 1-x O 2, wherein TM is a combination of metals according to general formula (I), (Ni a Co b Mn c) 1-d M 2 d (I) wherein a is in a range of from 0.6 to 0.99, b is in a range of from 0.005 to 0.2, c is in a range of from 0.005 to 0.2, and d is in a range of from zero to 0.1, M 2 is at least one of Al, Mg, W, Ti, and Zr, a+b+c=1, x is in a range of from zero to 0.2, M 1 is selected from the group consisting of Nb and Ta, and y is in a range of from 0.001 to less than 0.01, said process comprising the following steps: (a) mixing (A) a particulate mixed oxide or (oxy) hydroxide of Mn, Co and Ni, and (B) at least one lithium compound selected from the group consisting of lithium hydroxide, lithium oxide and lithium carbonate, and (C) an amorphous compound of Nb or Ta, and (b) subjecting said mixture to heat treatment at a temperature in a range of from 700 to 1000 ° C., wherein at least 60 mole-% of a transition metal of TM is Ni.
- Claim 2Depends on #1
The process according to claim 1, wherein said mixing in step (a) is performed in a dry state.
- Claim 3Depends on #1
The process according to claim 1, wherein step (b) is performed in a rotary kiln or a roller hearth kiln.
- Claim 4Depends on #1
The process according to claim 1, wherein (C) is amorphous niobic acid Nb 2 O 5 or amorphous Ta 2 O 5.
- Claim 5Depends on #1
The process according to claim 1, wherein (C) has an average particle diameter (D50) in a range of from 1 to 100 μ m.
- Claim 6Depends on #1
The process according to claim 1, wherein a compound (D) is present in step (a) and is selected from the group consisting of oxides or (oxy) hydroxides of Al, Ti and Zr.
- Claim 7Depends on #1
The process according to claim 1, wherein (A) is obtained by co-precipitation of a mixed hydroxide of nickel, cobalt and manganese, followed by drying under air and de-hydration.
- Claim 8Independent Claim
An electrode active material according to the general formula Li 1+x (TM 1-y M 1 y) 1-x O 2, wherein TM is a combination of metals according to general formula (I), x is in a range of from zero to 0.2, M 1 is selected from the group consisting of Nb and Ta, and y is in a range of from 0.001 to less than 0.01, (Ni a Co b Mn c) 1-d M 2 d (I) wherein a is in a range of from 0.6 to 0.99, b is in a range of from 0.005 to 0.2, c is in a range of from 0.005 to 0.2, and d is in a range of from zero to 0.1, M 2 is at least one of Al, Mg, W, and Zr, a+b+c=1, and an average particle diameter (D50) in a range of from 3 to 20 μ m, wherein at least 60 mol-% of TM is Ni, wherein Nb or Ta, respectively, is enriched on a surface of primary particles compared to a bulk, and wherein the electrode active material is comprised of secondary particles that are agglomerates of primary particles.
- Claim 9Depends on #8
The electrode active material according to claim 8, wherein M 1 is Nb.
- Claim 10Depends on #8
A cathode comprising (α) the electrode active material according to claim 8, (β) carbon in electrically conductive form, and (γ) a binder material.
- Claim 11Depends on #10
The cathode according to claim 10 comprising (α) 80 to 98% by weight cathode active material, (β) 1 to 17% by weight of carbon, and (γ) 3 to 10% by weight of the binder material, wherein the percentages refer to a sum of (α), (β) and (γ).
- Claim 12Depends on #10
An electrochemical cell comprising the cathode according to claim 10.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application is a U.S. National Phase Application of PCT/EP2021/078103, filed Oct. 12, 2021, which claims the benefit of priority to European Patent Application No. 20201960.0, filed Oct. 15, 2020, and European Patent Application No. 21200525.0, filed Oct. 1, 2021, the entire contents of which are hereby incorporated by reference herein. The present invention is directed towards a process for making an electrode active material according to general formula L 1+x (TM 1-y M 1 y ) 1-x O 2 , wherein TM includes a combination of Ni and at least one of Co, Mn and Al, and optionally at least one more metal selected from Mg, Al, Ti, Zr, and W, and x is in the range of from zero to 0.2, and M 1 is selected from Nb and Ta, and y is in the range of from 0.001 to less than 0.01, preferably 0.001 to 0.0065, more preferably 0.002 to 0.005: (a) mixing (A) a particulate mixed oxide or (oxy)hydroxide of Mn, Co and Ni, and (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) an amorphous compound of Nb or Ta, (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000 ° C., wherein at least 60 mole-% of the metal of TM is Ni. Lithium ion secondary batteries are modern devices for storing energy. Many application fields have been and are contemplated, from small devices such as mobile phones and laptop computers through car batteries and other batteries for e-mobility. Various components of the batteries have a decisive role with respect to the performance of the battery such as the electrolyte, the electrode materials, and the separator. Particular attention has been paid to the cathode materials. Several materials have been suggested, such as lithium iron phosphates, lithium cobalt oxides, and lithium nickel cobalt manganese oxides. Although extensive research has been performed the solutions found so far still leave room for improvement. Cathode
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (11)
Non-Patent Literature (7)
- European Search Report for EP Patent Application No. 20201960.0 dated Apr. 1, 2021; 3 pages.
- International Search Report and Written Opinion for PCT/EP2021/078103 mailed on Dec. 20, 2021, 11 pages.
- Nakajima et al.,
- “
- Nb2O5-nH2O as a Heterogeneous Catalyst with Water-Tolerant Lewis Acid Sites
- ”
- , J. Am. Chem. Soc., vol. 133, pp. 4224-4227 (2011).