Patents
US 12,725,762 B2#155836654 Most CitedActiveUnited States (USPTO)Utility

Method for etching atomic layer

0Forward Citations (#155836654 Global)
0.0/yrCitation Velocity (#155836654 Global)
0.00Citation PageRank (#155836654 Global)
15Prior Art Cited
16Claims (3 Indep. · 13 Dep.)
23Drawings / Sheets

Abstract

Provided is a method for etching an atomic layer. The method for etching the atomic layer includes providing a substrate to a process chamber, wherein the process chamber comprises a first chamber part and a second chamber part, and the substrate is provided in the second chamber part, generating adsorption gas plasma in the first chamber part, adsorbing radicals of the adsorption gas plasma to the substrate so as to form a treatment layer, generating etching gas plasma in the first chamber part, and allowing electrons and ions of the etching gas plasma to be alternately incident into the treatment layer so as to perform desorption of the treatment layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.

Claims (16 — 3 Independent, 13 Dependent)

  1. Claim 1Independent Claim

    A method for etching an atomic layer, the method comprising: providing a substrate to a process chamber, wherein the process chamber comprises a first chamber part and a second chamber part, and the substrate is provided in the second chamber part; generating adsorption gas plasma in the first chamber part; adsorbing radicals of the adsorption gas plasma to the substrate so as to form a treatment layer; generating etching gas plasma in the first chamber part; adjusting plasma discharge of the second chamber part by increasing a density of the etching gas plasma of the first chamber part to perform an isotropic desorption on the treatment layer or by decreasing the density of the etching gas plasma of the first chamber part to perform an anisotropic desorption on the treatment layer; and allowing electrons and ions of the etching gas plasma to be alternately incident into the treatment layer so as to perform desorption of the treatment layer, wherein the adsorbing the radicals of the adsorption gas plasma to the substrate comprises allowing the radicals of the adsorption gas plasma to pass from the first chamber part to the second chamber part, and the allowing the electrons and the ions of the etching gas plasma to be alternately incident into the treatment layer comprises adjusting a voltage applied to a plurality of grids between the first chamber part and the second chamber part or the substrate to allow the electrons and the ions of the etching gas plasma to be incident into the treatment layer.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the allowing the electrons and the ions of the etching gas plasma to be alternately incident into the treatment layer comprises: grounding or floating the plurality of grids and applying a positive voltage to the substrate to allow the electrons of the etching gas plasma to be incident into the treatment layer; and grounding or floating the plurality of grids and the substrate to allow the ions of the etching gas plasma to be incident into the treatment layer into which the electrons are incident.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the plurality of grids comprise a first grid, a second grid, and a third grid, and the allowing the electrons and the ions of the etching gas plasma to be alternately incident into the treatment layer comprises applying a positive voltage to the second grid and grounding and floating the first grid and the third grid to allow the electrons of the etching gas plasma to be incident into the treatment layer.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the plurality of grids comprise a first grid, a second grid, and a third grid, and the allowing the electrons and the ions of the etching gas plasma to be alternately incident into the treatment layer comprises applying a negative voltage to the second grid and grounding and floating the first grid and the third grid to allow the ions of the etching gas plasma to be incident into the treatment layer.

  5. Claim 5Depends on #1

    The method of claim 1, wherein the adjusting the voltage applied to the plurality of grids or the substrate comprises applying a positive voltage to the substrate and adjusting energy of the electrons of the etching gas plasma incident into the treatment layer to about 1 keV or less.

  6. Claim 6Depends on #1

    The method of claim 1, wherein the adjusting the voltage applied to the plurality of grids or the substrate comprises applying a pulse voltage.

  7. Claim 7Independent Claim

    A method for etching an atomic layer, the method comprising: providing a substrate to a process chamber, wherein the process chamber comprises a first chamber part and a second chamber part, and the substrate is provided in the second chamber part; generating adsorption gas plasma in the first chamber part; adsorbing radicals of the adsorption gas plasma to the substrate so as to form a treatment layer; generating etching gas plasma in the first chamber part; adjusting plasma discharge of the second chamber part by increasing a density of the etching gas plasma of the first chamber part to perform an isotropic desorption on the treatment layer or by decreasing the density of the etching gas plasma of the first chamber part to perform an anisotropic desorption on the treatment layer; and allowing electrons and ions of the etching gas plasma to be alternately incident into the treatment layer so as to perform desorption of the treatment layer, wherein a plurality of grids are provided between the first chamber part and the second chamber part.

  8. Claim 8Depends on #7

    The method of claim 7, wherein the allowing the electrons and the ions of the etching gas plasma to be alternately incident into the treatment layer comprises adjusting a voltage applied to the plurality of grids between the first chamber part and the second chamber part or the substrate.

  9. Claim 9Depends on #8

    The method of claim 8, wherein the adjusting the voltage applied to the plurality of grids between the first chamber part and the second chamber part or the substrate comprises applying a positive voltage to one or more grids of the plurality of grids to pass the electrons of the etching gas plasma and to block the ions of the etching gas plasma.

  10. Claim 10Depends on #8

    The method of claim 8, wherein the adjusting the voltage applied to the plurality of grids between the first chamber part and the second chamber part or the substrate comprises applying a negative voltage to one or more grids of the plurality of grids to pass the ions of the etching gas plasma and to block the electrons of the etching gas plasma.

  11. Claim 11Depends on #8

    The method of claim 8, wherein the adjusting the voltage applied to the plurality of grids between the first chamber part and the second chamber part or the substrate comprises applying a pulse voltage.

  12. Claim 12Depends on #7

    The method of claim 7, further comprising: before the generating the etching gas plasma in the first chamber part, purging residue of the adsorption gas plasma.

  13. Claim 13Depends on #7

    The method of claim 7, wherein the etching gas plasma comprises an inert gas.

  14. Claim 14Depends on #7

    The method of claim 7, wherein, in the performing the desorption on the treatment layer, allowing the electrons of the etching gas plasma to be incident into the treatment layer so as to remove a portion of the treatment layer and allowing the ions of the etching gas plasma to be incident into the treatment layer, into which the electrons are incident, to charge-neutralize the treatment layer are repeatedly performed.

  15. Claim 15Depends on #7

    The method of claim 7, wherein the electrons of the etching gas plasma incident into the treatment layer have energy of about 1 keV or less.

  16. Claim 16Independent Claim

    A method for etching an atomic layer, the method comprising: providing a substrate to a process chamber, wherein the process chamber comprises a first chamber part and a second chamber part, and the substrate is provided in the second chamber part; generating adsorption gas plasma in the first chamber part; adsorbing radicals of the adsorption gas plasma to the substrate so as to form a treatment layer; generating etching gas plasma in the first chamber part; adjusting plasma discharge of the second chamber part by increasing a density of the etching gas plasma of the first chamber part to perform an isotropic desorption on the treatment layer or by decreasing the density of the etching gas plasma of the first chamber part to perform an anisotropic desorption on the treatment layer; and allowing electrons of the etching gas plasma to be incident into the treatment layer so as to remove a portion of the treatment layer; and allowing ions of the etching gas plasma to be incident into the treatment layer, into which the electrons are incident, to charge-neutralize the treatment layer, wherein the radicals of the adsorption gas plasma pass from the first chamber part to the second chamber part through a shutter, a removal of the portion of the treatment layer and a charge-neutralization of the treatment layer are repeatedly performed until the treatment layer is completely detached, and a voltage applied to a plurality of grids between the first chamber part and the second chamber part or the substrate is adjusted so that the electrons or the ions of the etching gas plasma are incident into the treatment layer.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This U.S. non-provisional patent application claims priority under 35 U.S.C. § 119 of Korean Patent Application No. 10-2022-0161244, filed on Nov. 28, 2022, the entire contents of which are hereby incorporated by reference. BACKGROUND The present disclosure herein relates to a method for etching an atomic layer, and more particularly, to a method for etching an atomic layer using electrons. Semiconductor devices may be manufactured through various processes. For example, semiconductor devices may be manufactured by performing a photo process, an etching process, a deposition process, and the like on a wafer such as silicon. The etching of the atomic layer may be applied in various manners to the processes of manufacturing the semiconductor device. The etching of the atomic layer may be carried out by chemical, thermal, or physical methods, and may be attracting attention as a next-generation etching technology as a technology of etching materials one by one in atomic units. To implement precise etching of the atomic layer, it is necessary to etch an object to be etched while maintaining structural integrity of the object. SUMMARY The present disclosure provides a method for etching an atomic layer, which is capable of minimizing structural deformation. The present disclosure also provides a method for more accurately etching an atomic layer by adjusting a voltage of a grid and a substrate. The object of the present invention is not limited to the aforesaid, but other objects not described herein will be clearly understood by those skilled in the art from descriptions below. An embodiment of the inventive concept provides a method for etching an atomic layer, the method including: providing a substrate to a process chamber, wherein the process chamber includes a first chamber part and a second chamber part, and the substrate is provided in the second chamber part; generating adsorption gas plasma in the first chamber part; adso

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.