hottub.patents
US 12,723,124 B2#3150701 Most CitedActiveUnited States (USPTO)Utility

Storage-stable polyisocyanate composition and preparation method therefor

0Forward Citations (#3150701 Global)
0.0/yrCitation Velocity (#3150701 Global)
0.00Citation PageRank (#3150701 Global)
21Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

The present invention belongs to the technical field of preparing isocyanate derivatives, and particularly relates to a storage-stable polyisocyanate composition and a preparation method therefor. The method comprises: in the presence of a catalyst system, subjecting an isocyanate monomer to a polymerization reaction; terminating the reaction after a suitable conversion rate is reached, so as to obtain a polyisocyanate reaction solution; and then performing heat treatment on the obtained polyisocyanate reaction solution to obtain a heat-treated polyisocyanate mixture, wherein the heat treatment temperature is 10-30 ° C. higher than the heat-sensitive temperature of the obtained polyisocyanate product, and the heat treatment time is 5-30 min; and then performing separation treatment on the heat-treated polyisocyanate mixture. When the polyisocyanate composition of the present invention is stored at 50 ° C. for 30 days, the viscosity increase is small, thus the stability of the viscosity is ensured, and at the same time, the stability of the free monomer content and the color stability are also significantly improved.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a storage-stable polyisocyanate composition, comprising: carrying out a polymerization reaction on an isocyanate monomer in the presence of a catalyst system; after an appropriate conversion rate is reached, terminating the reaction to obtain a polyisocyanate reaction solution; carrying out heat treatment on the obtained polyisocyanate reaction solution to obtain a heat-treated polyisocyanate mixture, and a time of the heat treatment is 5-30 min; and then carrying out separation treatment on the heat-treated polyisocyanate mixture to remove unreacted isocyanate monomers in the system to prepare the polyisocyanate composition; wherein a temperature of the heat treatment is 10-30 ° C. higher than a heat-sensitive temperature of the obtained polyisocyanate composition; wherein the appropriate conversion rate is defined as: a preset conversion rate for the polyisocyanate composition to be prepared, which is calculated and reflected by controlling NCO % value of the system; wherein the heat-sensitive temperature is defined as: the polyisocyanate composition is heated within a temperature range of 100-200 ° C., the temperature range of 100-200 ° C. is evenly divided into multiple temperature intervals, a viscosity of the heated polyisocyanate composition is measured within these temperature intervals, the measured viscosities and their corresponding temperatures are drawn as a viscosity-temperature curve, and in the drawn curve, a temperature at which a viscosity of the polyisocyanate composition doubles is defined as the heat-sensitive temperature; wherein the obtained polyisocyanate composition satisfies the following conditions (1) and (2) after being stored at 50 ° C. for 30 days: (1) in the stored polyisocyanate composition, the increase of a content of an isocyanate monomer is less than or equal to 0.1 wt %; and (2) in the stored polyisocyanate composition, the increase of a viscosity of the polyisocyanate composition is less than or equal to 15% of an initial viscosity of the polyisocyanate composition.

  2. Claim 2Depends on #1

    The preparation method according to claim 1, wherein the polyisocyanate composition comprises one or more of trimer polyisocyanate, biuret polyisocyanate, and uretdione polyisocyanate; a heat-sensitive temperature of the trimer polyisocyanate is 160-165 ° C.; a heat-sensitive temperature of the biuret polyisocyanate is 140-145 ° C.; a heat-sensitive temperature of the uretdione polyisocyanate is 130-135 ° C.

  3. Claim 3Depends on #1

    The preparation method according to claim 1, wherein the preparation method comprises: (11) under an inert atmosphere, adding the isocyanate monomer to a reaction vessel, heating the isocyanate monomer, adding a catalyst I after the system is heated to a reaction temperature, carrying out a polymerization reaction, and monitoring NCO % of the reaction solution; and when the NCO % drops to an appropriate value, adding a terminating agent I to terminate the reaction to obtain a trimer polyisocyanate reaction solution; (12) carrying out heat treatment on the obtained trimer polyisocyanate reaction solution to obtain a heat-treated trimer polyisocyanate mixture; and (13) then carrying out separation treatment on the heat-treated trimer polyisocyanate mixture through a separation device to remove unreacted isocyanate monomers to prepare trimer polyisocyanate; wherein the heat-sensitive temperature of the trimer polyisocyanate is 160-165 ° C., and the appropriate value is 35% to 45%; wherein a temperature of the heat treatment is 10-30 ° C. higher than a heat-sensitive temperature of the obtained trimer polyisocyanate, and a time of the heat treatment is 5-30 min.

  4. Claim 4Depends on #3

    The preparation method according to claim 3, wherein the catalyst I in step (11) is a quaternary ammonium base and/or a quaternary ammonium salt catalyst; and/or an addition amount of the catalyst I is 0.001-0.1 wt % of a weight of the isocyanate monomer; and/or the terminating agent I in step (11) is selected from an organic acid and/or an acylating agent; and/or a reaction temperature of step (11) is 30-100 ° C.; and/or the separation treatment in step (13) has the process conditions that a separation temperature is 90-180 ° C. and a separation absolute pressure is 5-200 Pa.

  5. Claim 5Depends on #1

    The preparation method according to claim 1, wherein the preparation method comprises: (21) adding the isocyanate monomer and an acid catalyst to a reaction vessel, introducing water vapor as a biuret reagent after the system is heated to a reaction temperature, carrying out a polymerization reaction, and monitoring NCO % of the reaction solution; and when the NCO % drops to an appropriate value, stopping introducing the water vapor to terminate the reaction to obtain a biuret polyisocyanate reaction solution; (22) carrying out heat treatment on the obtained biuret polyisocyanate reaction solution to obtain a heat-treated biuret polyisocyanate mixture; and (23) then carrying out separation treatment on the biuret polyisocyanate mixture through a separation device to remove unreacted monomers to prepare biuret polyisocyanate; wherein the heat-sensitive temperature of the biuret polyisocyanate is 140-145 ° C., and the appropriate value is 33% to 37%; wherein a temperature of the heat treatment is 10-30 ° C. higher than a heat-sensitive temperature of the obtained biuret polyisocyanate, and a time of the heat treatment is 5-30 min.

  6. Claim 6Depends on #5

    The preparation method according to claim 5, wherein a mass ratio of the isocyanate monomer to the water vapor in step (21) is 40-60:1; and/or the acid catalyst in step (21) is selected from one or more of monoalkyl phosphate, dialkyl phosphate, monoaryl phosphate, diaryl phosphate, propionic acid, and pivalic acid, and an amount of the acid catalyst is 0.1-3.0 wt % of a weight of the isocyanate monomer; and/or a reaction temperature of step (21) is 80-280 ° C., and a reaction time of step (21) is 50-400 min; and/or the separation device in step (23) is a two-stage wiped-film evaporator, and the separation treatment has the process conditions that a separation temperature of the first-stage wiped-film evaporator is 110-180 ° C., and a separation absolute pressure of the first-stage wiped-film evaporator is 5-500 Pa; and a separation temperature of the second-stage wiped-film evaporator is 120-180 ° C., and a separation absolute pressure of the second-stage wiped-film evaporator is 5-200 Pa.

  7. Claim 7Depends on #1

    The preparation method according to claim 1, wherein the preparation method comprises: (31) adding the isocyanate monomer to a reaction vessel, heating the isocyanate monomer, adding a catalyst II and a cocatalyst sequentially with stirring after the system is heated to a reaction temperature, carrying out a polymerization reaction, and monitoring NCO % of the reaction solution; and when the NCO % drops to an appropriate value, adding a terminating agent II to terminate the reaction to obtain a uretdione polyisocyanate reaction solution; (32) carrying out heat treatment on the obtained uretdione polyisocyanate reaction solution to obtain a heat-treated uretdione polyisocyanate mixture; and (33) then carrying out separation treatment on the uretdione polyisocyanate mixture through a separation device to remove unreacted monomers in the reaction system to prepare uretdione polyisocyanate; wherein the heat-sensitive temperature of the uretdione polyisocyanate is 130-135 ° C., and the appropriate value is 38% to 42%; wherein a temperature of the heat treatment is 10-30 ° C. higher than a heat-sensitive temperature of the obtained uretdione polyisocyanate, and a time of the heat treatment is 5-30 min.

  8. Claim 8Depends on #7

    The preparation method according to claim 7, wherein the catalyst II in step (31) is a tertiary phosphine catalyst, and an amount of the catalyst II is 0.01-1 wt % of a weight of the isocyanate monomer; and/or the cocatalyst in step (31) is selected from a low molecular mass monovalent fatty alcohol or a low molecular mass polyvalent fatty alcohol, and an amount of the cocatalyst is 0-5 wt % of a weight of the isocyanate monomer; and/or the terminating agent II in step (31) is selected from one or more of acyl chloride, sulfonate, alkyl phosphate, and sulphate, and an amount of the terminating agent II is 80-120% of a molar amount of the catalyst II; and/or a reaction temperature of step (31) is 40-70 ° C.; and/or the separation treatment in step (33) has the process conditions that a separation temperature is 100-160 ° C., and a separation absolute pressure is 5-200 Pa.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a national stage entry under 35 U.S.C. § 371 (b) of PCT International Application No. PCT/CN2020/117698, filed Sep. 25, 2020, the entire disclosure of which is incorporated herein by reference. TECHNICAL FIELD The present disclosure belongs to the field of the preparation of isocyanate derivatives, and in particular, relates to a storage-stable polyisocyanate composition and a preparation method therefor. BACKGROUND It is well known that polyurethane resin coatings have excellent wear resistance, chemical resistance and contamination resistance, and in particular, the polyurethane resin coatings prepared with polyisocyanates derived from aliphatic (alicyclic) isocyanates such as hexamethylene diisocyanate, isophorone diisocyanate and dicyclohexylmethane diisocyanate even have excellent weather resistance. Therefore, these polyisocyanates are often used in polyurethane coatings which can be cured at normal temperature or by heating for painting and repairing buildings, automobiles, airplanes, ships and cross-sea bridges. At present, methods for preparing polyisocyanates through the polymerization reaction of aromatic, aliphatic or alicyclic diisocyanate monomers in the presence of a catalyst are known, and the advantages and disadvantages of various catalyst systems have been discussed in detail in the existing documents, for example, J. Prakt. Chem. 336 (1994) 185-200, CN201410002995.5, CN95113103.6, CN200310120368.3, CN200310120121.1, CN200910128728.1, and CN201280059016.9. However, the main disadvantage of polyisocyanate products prepared by the existing processes is that the viscosity of the polyisocyanate products increases rapidly in the storage process, which seriously affects long-distance transportation and downstream use. In view of the preceding problems, it is particularly important to explore how to improve the stability (especially the viscosity stability) of polyisocyanates in the storage proc

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
US 11,359,045 B2Method for producing isocyanate mixtures containing isocyanurate groups20220
CN 103,724,234 AMethod for preparing polyisocyanate containing biuret—11
CN 105,601,565 BA kind of preparation method of the polyisocyanates of the biuret-containing structure of stable storage20180
CN 110,305,294 AA kind of preparation method of the polyisocyanates containing uretdion groups of stable storage—15
CN 111,072,917 BPolyisocyanate composition with stable storage and preparation method thereof20210
CN 111,201,257 APolyisocyanate composition, coating composition and coating film—11
CN 111,247,185 APolyisocyanate composition, coating composition and coating film—4
CN 111,465,632 AMethod for producing isocyanurate group-containing isocyanate mixtures—2
CN 111,793,182 BPolyisocyanate composition20220
DE 102004060739 A1Preparation of polyisocyanate containing biuret group comprises mixing di- and/or polyisocyanate; water (vapor) as biuret-forming agent; optionally catalyst, in a mixing device and leading the obtained reaction mixture into a reactor—7
EP 4,056,619 A4Storage-stable polyisocyanate composition and preparation method—0
US 8,225,511 B2Portable direct action brittle pipe/soil pipe cutter20120
JP H1036470 APolyisocyanate composition excellent in low-temperature storage stability and its production—5
JP 2002047333 AManufacturing method of uretdione polyisocyanate having improved monomer stability—6
JP 2016037539 APolyisocyanate composition, paint composition and coating—2
JP 2016053127 APolyisocyanate composition, coating composition and coated film—10
KR 20170047877 AManufacturing method of non-yellowish polyisocyanurate with improved preservability—1
WO 2020/078241 A1Pneumatic laundry apparatus and washing method thereof—1
WO 2020/078250 A1Data processing method and device for virtual scene—2

Non-Patent Literature (3)

  • English language translation of CN 111201257 A. (Year: 2020).
  • PCT Search Report and Written Opinion prepared for PCT Application No. PCT/CN2020/117698, completed Jun. 8, 2021.
  • European Search Report issued for Application No. 20954556.5, mailed Dec. 13, 2023.