hottub.patents
US 12,709,552 B2#3164168 Most CitedActiveUnited States (USPTO)Utility

Methods for battery-grade aqueous solutions of nickel salts

0Forward Citations (#3164168 Global)
0.0/yrCitation Velocity (#3164168 Global)
0.00Citation PageRank (#3164168 Global)
10Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

Methods are provided for preparing an aqueous nickel salt solution from an aqueous mixed metal salt solution comprising cobalt, manganese, and nickel salts and one or more impurity salts. The method includes precipitating a first group of impurity salts and the manganese salt to form an aqueous pre-extraction solution. The aqueous pre-extraction solution and an organic extractant solution are mixed to form an aqueous raffinate phase and a loaded organic phase, wherein the aqueous raffinate phase is the aqueous nickel salt solution.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for preparing an aqueous nickel salt solution from an aqueous mixed metal salt solution comprising a cobalt salt, a manganese salt, a nickel salt and one or more impurity salts, the method comprising: precipitating a first group of the one or more impurity salts and the manganese salt from the aqueous mixed metal salt solution to form one or more impurity precipitates, a manganese oxide precipitate, and an aqueous pre-extraction solution; and mixing the aqueous pre-extraction solution and an organic extractant to form an aqueous raffinate phase and a loaded organic phase, wherein the aqueous raffinate phase is the aqueous nickel salt solution and the loaded organic phase comprises the cobalt salt and a second group of the one or more impurity salts.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the first group of the one or more impurity salts comprises a copper salt, an aluminum salt, and an iron salt.

  3. Claim 3Depends on #1

    The method of claim 1, wherein precipitating the first group of impurity salts and the manganese salt includes one or more of cementation, base hydrolysis, and oxidation.

  4. Claim 4Depends on #1

    The method of claim 1, wherein precipitating the first group of the one or more impurity salts comprises: mixing the aqueous mixed metal salt solution and iron powder or nickel powder to form a copper precipitate and a copper depleted solution, separating the copper precipitate and the copper depleted solution; mixing the copper depleted solution and a base to form one or more metal hydroxide precipitates and a nickel enriched solution; separating the one or more metal hydroxide precipitates and the nickel enriched solution; and mixing an oxidizing gas and the nickel enriched solution to form the manganese oxide precipitate and the aqueous pre-extraction solution.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the oxidizing gas comprises a mixture of sulfur dioxide and oxygen.

  6. Claim 6Depends on #4

    The method of claim 4, further comprising adjusting a pH of the nickel enriched solution to a manganese oxidation pH in a range of from 2 to 6 while mixing the oxidizing gas.

  7. Claim 7Depends on #1

    The method of claim 1, wherein a concentration of the manganese salt in the aqueous pre-extraction solution is less than or equal to 1 ppm.

  8. Claim 8Depends on #1

    The method of claim 1, wherein the organic extractant is a dialkylphosphinic acid.

Technical Overview & Description

CROSS REFERENCE TO RELATED APPLICATIONS The present application claims priority to U.S. Provisional Application No. 63/678,222 entitled, “ BATTERY-GRADE NICKEL SOLUTION ” , filed on Aug. 1, 2024, and U.S. Provisional Application No. 63/754,453 entitled, “ METHODS FOR BATTERY-GRADE AQUEOUS SOLUTIONS OF NICKEL SALTS ” , and filed on Feb. 5, 2025. The entire contents of each of the above-identified applications are hereby incorporated by reference for all purposes. FIELD The present description relates generally to methods for producing a battery-grade nickel salt solution from an aqueous mixed metal salt solution. BACKGROUND/SUMMARY Many technologies, such as electric vehicles and cellphones to name a few, rely on lithium-ion batteries (LIBs). However, LIBs degrade after a finite number of charging/discharging cycles and thus become spent LIBs and demand replacement. Recycling of spent LIBs to recover metals such as lithium, nickel, cobalt, and/or manganese as battery-grade materials is important to maintaining a critical and circular supply of metals for LIBs. LIB chemistry varies and includes elements in addition to the recovery metals of interest. For example, in addition to lithium, nickel, cobalt, and/or manganese, LIBs may include magnesium, iron, aluminum, copper, and zinc, as well as calcium, chromium, phosphorus, silicon, tin, titanium, and zirconium. Increasingly, LIBs favor high nickel cathode materials. Forming a battery grade nickel solution from a spent LIB recycling stream provides a cost effective and circular source of nickel salts for new LIBs. Conventionally, separating nickel from a mixed metal source, such as mixed metal mining products, demands multiple liquid/liquid extraction steps followed by crystallization of the nickel salts from the resulting solution to form nickel salts at battery-grade purity levels. The inventors have recognized the problems discussed above and find the problems may be at least partially addressed by a method for prepa

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (10)

Non-Patent Literature (3)

  • English translation of WO Publication 2025-048109, Mar. 2025.
  • English translation of CN Publication 114457245, May 2022.
  • ISA Korean Intellectual Property Office, International Search Report and Written Opinion Issued in Application No. PCT/US2025/034292, Oct. 22, 2025, WIPO, 11 pages.