Recycled polishing pad and preparation method thereof
Abstract
According to embodiments of the present invention, there are provided a recycled polishing pad and a process for preparing a recycled polishing pad. The recycled polishing pad comprises a cushion layer, an adhesive layer, and a reused polishing layer having a plurality of grooves on one side, and the compressibility of the reused polishing layer calculated by a specific equation is controlled within a predetermined range; thus, the polishing layer can be reused while excellent polishing rate and polishing uniformity are maintained.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.
Claims (8 — 1 Independent, 7 Dependent)
- Claim 1Independent Claim
A recycled polishing pad, which comprises a cushion layer; an adhesive layer formed on the cushion layer; and a reused polishing layer attached to the adhesive layer and comprising a groove on one side, wherein the compressibility of the reused polishing layer calculated by Equation 1 is 0.9% or more, Compressibility of the reused polishing layer ( %) = T 1 - T 2 T 1 × 1 0 0 [ Equation 1 ] in Equation 1, T 1 is the thickness (mm) of the reused polishing layer measured when the reused polishing layer is pressed with a load of 85 g for 30 seconds, and T 2 is the thickness (mm) of the reused polishing layer measured when the reused polishing layer is further pressed with a load of 885 g for 3 minutes after T 1 is measured, and wherein the recycled polishing pad has a structure in which the cushion layer, the adhesive layer, and the reused polishing layer are sequentially laminated while in contact with each other, and wherein the ratio of the depth of the groove to
- Claim 2Depends on #1
The recycled polishing pad of claim 1, wherein the ratio of the depth of the groove to the total thickness of the recycled polishing pad is 0.2 or less.
- Claim 3Depends on #1
The recycled polishing pad of claim 1, wherein the depth of the groove is 0.10 mm to 0.75 mm.
- Claim 4Depends on #1
The recycled polishing pad of claim 1, wherein the compressibility of the reused polishing layer is 0.9% to 3.0%.
- Claim 5Depends on #1
The recycled polishing pad of claim 1, wherein the thickness of the reused polishing layer is thinner than the thickness of the cushion layer.
- Claim 6Depends on #1
The recycled polishing pad of claim 1, wherein the compressibility of the recycled polishing pad calculated by Equation 2 is 0.25% or more, Compressibility of the recycled polishing pad ( %) = T 3 - T 4 T 3 × 1 0 0 [ Equation 2 ] in Equation 2, T 3 is the thickness (mm) of the recycled polishing pad measured when the recycled polishing pad is pressed with a load of 85 g for 30 seconds, and T 4 is the thickness (mm) of the recycled polishing pad measured when the recycled polishing pad is further pressed with a load of 885 g for 3 minutes after T 3 is measured.
- Claim 7Depends on #1
The recycled polishing pad of claim 1, wherein the reused polishing layer has a hardness of 40 Shore D to 70 Shore D.
- Claim 8Depends on #1
The recycled polishing pad of claim 1, wherein the recycled polishing pad has a hardness of 35 Shore D to 55 Shore D.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATION The present application claims priority under 35 U.S.C. § 119(a) to Korean patent application number 10-2024-0119211 filed on Sep. 3, 2024 in the Korean Intellectual Property Office, the entire disclosure of which is incorporated by reference herein. TECHNICAL FIELD The present invention relates to a recycled polishing pad and a process for preparing the same. BACKGROUND ART A chemical mechanical planarization (CMP) process may be carried out for various purposes in various technical fields. For example, a CMP process may be used to planarize the surfaces of materials and substrates used in semiconductor devices, electronic components, optical components, and the like, remove aggregated substances, resolve damage to crystal lattices, and remove surface defects and contaminants. In a CMP process, a polishing pad may be used to polish the surface of an object to be polished. Since the polishing pad interacts directly with the surface of the object to be polished, it may have an impact on the processing quality of the object to be polished. For example, the polishing characteristics of a CMP process may significantly vary depending on the components contained in the polishing pad and the physical properties of the polishing pad. As environmental problems such as climate change have arisen in recent years, public opinion is forming that companies should take social responsibility for building a society capable of sustainable development through ESG management such as “ carbon neutrality. ” Polishing pads used in a CMP process are consumables and are discarded after use rather than reused, which may cause environmental pollution. Accordingly, attempts have been made to recycle polishing pads upon completion of their use. Meanwhile, as a CMP process proceeds, the pad layer of the polishing pad may wear out, or the pad layer may become thinner. Conventionally, methods for recycling polishing pads have been studied by adding or supplem
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (24)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (2)
- Office Action for Japanese Patent Application No. 2025-116167 issued by the Japanese Patent Office on Aug. 12, 2025.
- Office Action for Chinese Patent Application No. 202510879442.6 issued by the Chinese Patent Office on May 16, 2026.