Abstract

Described herein is a method of depositing a conformal, optically transparent coating onto a surface of one or more internal components that are enclosed within an assembled device including an optical encoder using a non-line-of-sight deposition process without altering a structure of the assembled device or impacting functionality of the assembled device. Also described is an assembled device including an optical encoder, where one or more internal components enclosed within the optical encoder and a coating deposited onto a surface of the internal components, where the coating is a conformal, optically transparent coating that is resistant to corrosion by at least one of fluorine-, chlorine-, sulfur-, hydrogen-, bromine-, or nitrogen-based acids and that does not negatively impact functionality of the internal components.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method comprising: loading an assembled device comprising an optical encoder into a deposition chamber, wherein the assembled device comprises one or more internal components that are enclosed within an interior of the optical encoder and an optical window in a wall of the optical encoder, and wherein the one or more internal components capture a position of an object external to the assembled device in accordance with a type associated with the optical encoder; and depositing a conformal, optically transparent coating onto a surface of the internal components using a non-line-of-sight deposition process without altering a structure of the assembled device or impacting functionality of the assembled device, wherein the conformal, optically transparent coating penetrates an exterior of the assembled device through one or more openings of the assembled device that expose the interior of the assembled device to an external environment.

  2. Claim 2Depends on #1

    The method of claim 1, wherein depositing the conformal, optically transparent coating onto the surface of the internal components comprises: injecting a precursor for the conformal, optically transparent coating into the deposition chamber, wherein the precursor penetrates the exterior of the assembled device through the one or more openings of the assembled device.

  3. Claim 3Depends on #1

    The method of claim 1, wherein depositing the conformal, optically transparent coating onto the surface of the internal components comprises performing a chemical vapor deposition process of a poly (p-xylylene) polymer in a vacuum, and wherein the conformal, optically transparent coating comprises a poly (p-xylylene) polymer coating.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the internal components comprise one or more optical components.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the one or more optical components comprise at least one of an optical lens or a laser head.

  6. Claim 6Depends on #4

    The method of claim 4, wherein the one or more optical components are configured to at least one of emit light that exits the assembled device through the optical window or receive light that enters the assembled device through the optical window.

  7. Claim 7Depends on #1

    The method of claim 1, wherein the conformal, optically transparent coating has an approximately uniform thickness of between about 0.1 microns to about 20 microns, and wherein the coating coats an entire interior of the assembled device.

  8. Claim 8Depends on #1

    The method of claim 1, wherein the conformal, optically transparent coating has a thickness of between about 4 microns to about 5 microns.

Technical Overview & Description

RELATED APPLICATIONS This application is a continuation of U.S. application Ser. No. 16/820,338, filed Mar. 16, 2020, which claims the benefit under 35 U.S.C. § 119(e) of U.S. Provisional Patent Application No. 62/823,540, filed Mar. 25, 2019, which are incorporated herein, in their entirety, by this reference. TECHNICAL FIELD Embodiments of the present disclosure relate to methods of coating a surface of one or more internal components enclosed within an interior of an assembled device with a conformal, optically transparent coating, as well as to assembled devices having such a coating. BACKGROUND Various manufacturing processes expose assembled devices to high temperatures, a mixture of corrosive gases, high stress, and combinations thereof. For example, an assembled device may be exposed to an environment containing fluorine-, chlorine-, sulfur-, hydrogen-, bromine-, or nitrogen-based gases. Such gases may penetrate such an assembled device and condense on surfaces of internal components of the assembled device as acids. The acids may erode and/or corrode the internal and external components of assembled devices, increasing the devices' susceptibility to defects. An assembled device may include one or more internal components which are enclosed within an interior of the assembled device. The manufacturing process of the assembled device may make it difficult to individually protect each internal component enclosed within the assembled device from exposure to the corrosive conditions described above. Additionally, given a wide range of use applications for an assembled device, it may be difficult for a manufacturer to predict the type of environment each assembled device may be exposed to and individually protect each internal component in accordance with that environment's conditions prior to assembling the assembled device. Furthermore, disassembly of assembled devices in order to add protection to internal components may be impracticable, as such disassembly m

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (9)

PatentTitleYearCitations

Non-Patent Literature (1)

  • PCT International Search Report and Written Opinion for International Application No. PCT/US2020/023450 mailed Jul. 8, 2020, 12 pages.