Patents
US 12,693,264 B2#155868881 Most CitedActiveUnited States (USPTO)Utility

Detection of magnetization inhomogeneities in ultra-scaled magnetic nanowires

0Forward Citations (#155868881 Global)
0.0/yrCitation Velocity (#155868881 Global)
0.00Citation PageRank (#155868881 Global)
7Prior Art Cited
19Claims (1 Indep. · 18 Dep.)
5Drawings / Sheets

Abstract

The invention concerns a method for nonperturbative detection of one or more magnetic inhomogeneities resulting from nano-defects in a single longitudinal anisotropic magnetic sample structure having a nanometric cross-sectional dimension. A solid-state lattice with a single spin defect is used for magnetometry assessment of the anisotropic magnetic sample structure to determine quantitative information concerning minor defects and inconsistencies in the sample structure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (19 — 1 Independent, 18 Dependent)

  1. Claim 1Independent Claim

    Method for nonperturbative detection of one or more magnetic inhomogeneities resulting from nano-defects in a longitudinal magnetic sample structure possessing a shape-induced anisotropy and having a widest nanometric cross-sectional dimension from 1 nm to 500 nm, or from 1 nm to 50 nm comprising: a) movably positioning a sensing surface of a solid-state lattice sensor of diamond material, comprising one single spin defect (NV) in the apex of the solid-state lattice sensor, at a first scanning position in proximity of the magnetic sample structure, b) irradiating the one spin defect (NV) by applying optical radiation (L) and a microwave field continuously or in one or more pulses to the one spin defect (NV) such as to detect a Zeeman shift upon exposure of the irradiated one spin defect to the magnetic field of the magnetic sample structure, c) detecting a photoluminescence (PL) output signal from the solid-state lattice sensor comprising the one spin defect (NV), d) scanning the surface of the magnetic sample structure in performing steps a) to c) at a series of scanning positions over at least a portion of the length of the magnetic sample structure such as to obtain quantitative information on the magnetic field spatial distribution, wherein an optically detected magnetic resonance (ODMR) spectrum is recorded at each of said scanning positions.

  2. Claim 2Depends on #1

    The method according to claim 1, wherein the spin defect (NV) is a nitrogen-vacancy (NV) point defect in the diamond lattice.

  3. Claim 3Depends on #2

    The method according to claim 2, comprising the step of mapping detected inhomogeneities in a magnetization distribution along a scanned portion of the magnetic sample structure.

  4. Claim 4Depends on #2

    The method according to claim 2, wherein the spin defect is located 100 nm or less, 50 nm or less, 20 nm or less, or 10 nm or less, from the sensing surface of the solid-state lattice sensor.

  5. Claim 5Depends on #1

    The method according to claim 1, wherein the diamond sensor is a monocrystalline diamond sensor.

  6. Claim 6Depends on #1

    The method according to claim 1, comprising the step of mapping detected inhomogeneities in a magnetization distribution along a scanned portion of the magnetic sample structure.

  7. Claim 7Depends on #1

    The method according to claim 1, wherein the magnetic field strength at a scanning position is related to an intensity of PL output signal at that scanning position.

  8. Claim 8Depends on #1

    The method according to claim 1, wherein the magnetic field strength is determined on the basis of the separation of resonance peaks in the recorded ODMR spectrum.

  9. Claim 9Depends on #1

    The method according to claim 1, wherein a detected inhomogeneity in a magnetic field distribution is used to identify and/or to quantify a local inconsistency or defect, such as an inconsistency in geometry, in stoichiometry or in chemical composition, and/or defects in crystallinity or in amorphous characteristics, optionally on the basis of a set of predetermined data.

  10. Claim 10Depends on #9

    The method according to claim 9, wherein the detected inhomogeneity in the magnetic field distribution is based on a set of predetermined data, and wherein said predetermined data are empirical data, for example data obtained from previous measurements of comparable or substantially the same magnetic sample structures.

  11. Claim 11Depends on #1

    The method according to claim 1, wherein the sensing surface of the solid-state lattice sensor is positioned no more than 100 nm, or no more than 50 nm, or no more than 20 nm, or no more than 10 nm, or no more than 1 nm, from the sample surface.

  12. Claim 12Depends on #1

    The method according to claim 1, wherein the spin defect is located 100 nm or less, 50 nm or less, 20 nm or less, or 10 nm or less, from the sensing surface of the solid-state lattice sensor.

  13. Claim 13Depends on #1

    The method according to claim 1, wherein the solid-state lattice sensor has a detection sensitivity of no more than 10 μ T/ √ Hz, or no more than 5 μ T/ √ Hz, or no more than 2.5 μ T/ √ Hz.

  14. Claim 14Depends on #1

    The method according to claim 1, wherein the magnetic sample structure is a uniaxial sample structure with a single easy axis and the magnetization is aligned along the single easy axis of the magnetic sample structure.

  15. Claim 15Depends on #1

    The method according to claim 1, wherein the magnetic sample structure has at least one maximal transversal dimension perpendicular to its main axis of less than 50 nm, or of less than 30 nm, or of less than 10 nm.

  16. Claim 16Depends on #1

    The method according to claim 1, the magnetic sample structure being a ferromagnet, an anti-ferromagnet, a semi-conductor or a paramagnetic sample structure.

  17. Claim 17Depends on #1

    The method according to claim 1, wherein the magnetic sample structure is a nanowire or nanotube.

  18. Claim 18Depends on #1

    The method according to claim 1, configured to scan a plurality of nanowires arranged on or embedded in a carrier substrate.

  19. Claim 19Depends on #1

    The method according to claim 1, wherein the magnetic sample structure is a nanowire, a nanotube, or a plurality of nanowires embedded in a carrier substrate.

Technical Overview & Description

TECHNICAL DOMAIN The present invention concerns a method to quantify structural integrity in switching elements, as used in spintronic devices. RELATED ART The successful development of spintronics devices is built on the availability of magnetic switching elements to perform logic and memory operations. Magnetic nanowires (NWs) are essential building-blocks as they are considered reliable and offer design flexibility, multiple options for large-area fabrication, and alternative strategies for tuning the magnetic properties of the wire through geometry and anisotropy. For their application in spintronic devices NWs are usually patterned on a carrier material, for example silicon or silicon dioxide (SiO 2 ). Such NW assemblies permit to densely arrange a large number of nanowires, for example between 3 ′ 000 to 20 ′ 000 NW per millimetre (mm) width of the substrate. The NWs are usually distributed uniformly over the area of the carrier material. Switching assemblies for spintronic devices can for example be fabricated through subtractive patterning in analogy to gate spacers from complementary metal-oxide-semiconductor (CMOS) manufacturing processes. Patterned magnetic nanowires represent an optimal media for fast propagation of domain walls (DWs) and high storage density in the ever-growing field spintronic devices. Valid for both logic and memory application, NW-based devices offer fast switching speed, good scalability, and low-power operation. Most importantly, NWs are a convenient architecture to obtain bistable magnetic configuration, single magnetic easy axis, and tuneable properties by changing wire geometry and anisotropy. Importantly, the large uniaxial magnetic anisotropy along their entire length of the wire, namely shape anisotropy, suggest that nanowires have a single magnetic domain that should not generate stray magnetic fields along the entire length of the wire, unless DWs are deliberately injected. DWs can for example be artificially introduced by

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Nanoscale imaging and control of domain-wall hopping with a nitro-gen-vacancy center microscope (Year: 2014).
  • Rondin, et al., Nanoscale magnetic field mapping with a single spin scanning probe magnetometer; Applied Physics Letters, 2012, No. 100, 153118, XP-002718854.
  • Lee, et al., Magnetic imaging of a single ferromagnetic nanowire using diamond atomic sensors; Nanotechnology, 2018, No. 29, IOP Publishing, XP20331090A.
  • Tetienne,et.al., Nanoscale imaging and control of domain-wall hopping with a nitrogen-vacancy center microscope; Science-sciencemag.org, Jun. 20, 2014, vol. 344, Issue 6190, XP55867936A.
  • Berganza, et. al., Multisegmented Nanowires: a Step towards the Control of the Domain Wall Configuration; Scientific Reports, 2017, 7:11576, XP55969269A.
  • Maletinsky, et. al., A robust, scanning quantum system for nanoscale sensing and imaging; arxiv.org; 2011, XP80522275A.
  • Dutta, et. al., Sub-100 nm^2 Cobalt Interconnections; IEEE Electron Device Letters, May 2018, vol. 39, No. 5, pp. 731-734,.
  • International Search Report issued in corresponding International PCT Application No. PCT/IB2022/056427; Dated: Oct. 18, 2022.
  • Written Opinion of the International Searching Authority issued in corresponding International PCT Application No. PCT/IB2022/056427; Dated: Oct. 18, 2022.
  • Celano et al.,