Dielectric material, device including the same, and method of preparing the dielectric material
Abstract
A dielectric material, a device including the same, and a method of preparing the dielectric material are provided. The dielectric material may include a compound represented by the following Formula 1: K 1+x NaSr 4-2x La x Nb 10 O 30 , Formula 1 wherein, in Formula 1, 0 < x < 2.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.
Claims (25 — 2 Independent, 23 Dependent)
- Claim 1Independent Claim
A dielectric material comprising: a compound represented by Formula 1: K 1+x NaSr 4-2x La x Nb 10 O 30, Formula 1 wherein 0 < x < 2.
- Claim 2Depends on #1
The dielectric material of claim 1, wherein 0 < x ≤ 1.
- Claim 3Depends on #1
The dielectric material of claim 1, wherein 0 < x ≤ 0.5.
- Claim 4Depends on #1
The dielectric material of claim 1, wherein the compound includes a tungsten-bronze crystal structure.
- Claim 5Depends on #1
The dielectric material of claim 1, wherein the compound includes a tungsten-bronze crystal structure of KNaSr 4 Nb 10 O 30, and a structure in which a Sr cation located in an A site in a unit lattice of the KNaSr 4 Nb 10 O 30 is substituted with La 3+ as a donor and K +1 as an acceptor.
- Claim 6Depends on #1
The dielectric material of claim 1, wherein the compound has a tetragonal crystal structure.
- Claim 7Depends on #1
The dielectric material of claim 1, wherein a size of a unit lattice of the compound is increased compared to a size of a unit lattice of KNaSr 4 Nb 10 O 30.
- Claim 8Depends on #1
The dielectric material of claim 1, wherein the compound includes at least one of K 1.01 NaSr 3.98 La 0.01 Nb 10 O 30, K 1.05 NaSr 3.9 La 0.05 Nb 10 O 30, K 1.1 NaSr 3.8 La 0.1 Nb 10 O 30, K 1.15 NaSr 3.7 La 0.15 Nb 10 O 30, K 1.2 NaSr 3.6 La 0.2 Nb 10 O 30, K 1.25 NaSr 3.5 La 0.25 Nb 10 O 30, K 1.3 NaSr 3.4 La 0.3 Nb 10 O 30, K 1.35 NaSr 3.3 La 0.35 Nb 10 O 30, K 1.4 NaSr 3.2 La 0.4 Nb 10 O 30, K 1.45 NaSr 3.1 La 0.45 Nb 10 O 30, K 1.5 NaSr 3 La 0.5 Nb 10 O 30, K 1.55 NaSr 2.9 La 0.55 Nb 10 O 30, K 1.6 NaSr 2.8 La 0.6 Nb 10 O 30, K 1.65 NaSr 2.7 La 0.65 Nb 10 O 30, K 1.7 NaSr 2.6 La 0.7 Nb 10 O 30, K 1.75 NaSr 2.5 La 0.75 Nb 10 O 30, K 1.8 NaSr 2.4 La 0.8 Nb 10 O 30, K 1.85 NaSr 2.3 La 0.85 Nb 10 O 30, K 1.9 NaSr 2.2 La 0.9 Nb 10 O 30, K 1.95 NaSr 2.1 La 0.95 Nb 10 O 30, K 2 NaSr 2 LaNb 10 O 30, K 2.05 NaSr 1.9 La 1.05 Nb 10 O 30, K 2.1 NaSr 1.8 La 1.1 Nb 10 O 30, K 2.15 NaSr 1.7 La 1.15 Nb 10 O 30, K 2.2 NaSr 1.6 La 1.2 Nb 10 O 30, or K 2.25 NaSr 1.8 La 1.25 Nb 10 O 30.
- Claim 9Depends on #1
The dielectric material of claim 1, wherein an electric field-polarization graph of the dielectric material has a linear curve shape in which, as an amount of La is increased, residual polarization (Pr) is reduced and in which the polarization is proportional to an applied electric field.
- Claim 10Depends on #1
The dielectric material of claim 1, wherein a maximum permittivity of the dielectric material, at 1 kHz, is within a range of 1,000 to 2,600.
- Claim 11Depends on #1
The dielectric material of claim 1, wherein in a graph showing changes in permittivity according to temperature of the dielectric material, as an amount of La is increased, a temperature (T max) at which the dielectric material has maximum permittivity is decreased.
- Claim 12Depends on #1
The dielectric material of claim 1, wherein the dielectric material is a solid solution including polar nano regions (PNR).
- Claim 13Depends on #12
The dielectric material of claim 12, wherein the PNR include defect clusters in which a Sr cation located in an A site in a unit lattice of KNaSr 4 Nb 10 O 30 is substituted with La 3+ as a donor, and K +1 as an acceptor.
- Claim 14Depends on #1
A device comprising: a plurality of electrodes; and at least one dielectric layer between the plurality of electrodes, the at least one dielectric layer including the dielectric material of claim 1.
- Claim 15Depends on #14
The device of claim 14, wherein the device is a multi-layered capacitor, the plurality of electrodes includes a plurality of internal electrodes, the at least one dielectric layer includes dielectric layers alternately arranged between the plurality of internal electrodes.
- Claim 16Depends on #15
The device of claim 15, wherein a main component of the plurality of internal electrodes is nickel.
- Claim 17Depends on #14
The device of claim 14, wherein a maximum permittivity of the at least one dielectric layer, at 1 kHz, is within a range of 1,000 to 2,600.
- Claim 18Depends on #14
The device of claim 14, wherein a resistivity of the at least one dielectric layer is within a range of 1.0 E+11 Ω cm to 1.0 E+14 Ω cm.
- Claim 19Depends on #14
The device of claim 14, wherein an effective permittivity of the at least one dielectric layer at room temperature and 125 ° C. when 8.7 V/ μ m of DC bias is applied is within a range of 1,000 to 1,150.
- Claim 20Depends on #14
An electronic device comprising: a capacitor; and a transistor, wherein at least one of the capacitor or the transistor includes the device of claim 14.
- Claim 21Independent Claim
A method of manufacturing a dielectric material, the method comprising: mechanically milling a mixture of potassium salts, sodium salts, strontium salts, niobium compounds, and lanthanum compounds; and heat-treating the mixture under an oxidizing atmosphere, wherein the dielectric material includes a compound represented by the following Formula 1 K 1+x NaSr 4-2x La x Nb 10 O 30, Formula 1 wherein 0 < x < 2.
- Claim 22Depends on #21
The method of claim 21, wherein the heat-treating is performed within a range of 900 ° C. to 1,200 ° C.
- Claim 23Depends on #21
The method of claim 21, further comprising: obtaining a molded article by molding a product of the heat-treating; and performing a second heat-treatment on the molded article.
- Claim 24Depends on #23
The method of claim 23, wherein the second heat-treatment is performed within a range of 1,200 ° C. to 1,500 ° C.
- Claim 25Depends on #21
The method of claim 21, wherein the heat-treating the mixture oxidizes the mixture.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATION This application is based on and claims priority under 35 U.S.C. § 119 to Korean Patent Application No. 10-2021-0164870, filed on Nov. 25, 2021, in the Korean Intellectual Property Office, the disclosure of which is incorporated by reference herein in its entirety. BACKGROUND 1. Field The present disclosure relates to a dielectric material, a device including the same, and a method of preparing the dielectric material. 2. Description of the Related Art As electronic products continue to become smaller and more powerful, more miniaturized capacitors having higher capacitance are needed. In order to provide a miniaturized, high-capacity capacitor, there is a need for a dielectric material with improved dielectric properties. In order to produce a multi-layered ceramic capacitor (MLCC), which is a type of a miniaturized and high-capacity capacitor, a dielectric layer needs to be made thinner. However, an inevitable surge of the electric field may lead to a decrease in dielectric spontaneous polarization, and as a result, permittivity drops significantly. In addition, the need for a high-temperature dielectric material, e.g., for use in MLCC for vehicles and/or special purposes, is gradually increasing. Therefore, there is a demand for the development of a novel dielectric material that has improved permittivity under a high electric field and has a stability in high temperatures. SUMMARY An aspect is to provide a dielectric material having improved permittivity and stable temperature properties of permittivity under a high electric field at room temperature and a high temperature, and retaining an equivalent level of dielectric and temperature characteristics even when used under a redox atmosphere in a device. Another aspect is to provide a device including the dielectric material. Still another aspect is to provide a method of producing the dielectric material. Additional aspects will be set forth in part in the description whic
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (8)
| Patent | Title | Year | Citations |
|---|---|---|---|
| EP 0,774,227 A2 | Vacuum cleaner | — | 0 |
Non-Patent Literature (10)
- Huan-Chu Chen et al,
- “
- Growth and some properties of undoped and Doped (K1
- —
- xNax)0.4(Sr1
- —
- yBay)0.8Nb2O6(KNSBN)Single Crystals With Tungsten-Bronze Structure,
- ”
- Journal of Crystal Growth, 96(2), pp. 357-362, Jan. 23, 1989.
- M. Zriouil et al,