hottub.patents
US 12,679,959 B2#3193498 Most CitedActiveUnited States (USPTO)Utility

Method for producing rubber composition, rubber composition and tire produced by employing the same

0Forward Citations (#3193498 Global)
0.0/yrCitation Velocity (#3193498 Global)
0.00Citation PageRank (#3193498 Global)
8Prior Art Cited
4Claims (1 Indep. · 3 Dep.)
0Drawings / Sheets

Abstract

A method for preparing a rubber composition capable of improving the physical properties of a final product is disclosed. A rubber composition is prepared by dispersing polybutene in rubber in a solution phase (PIB extended rubber). The method comprises dispersing hydrophobic extender oil and polybutene in water to prepare an extender oil/polybutene emulsion; adding the extender emulsion to a latex-shaped rubber composition and uniformly dispersing the same in a solution to prepare a rubber/extension oil/polybutene composition; and solidifying, drying and molding the composition in a latex shape through salting-out and acid precipitation. When the rubber composition is applied to a tire tread composite material, the durability, grip property and low rotational resistance are improved, thereby attaining improved braking characteristic, low fuel consumption characteristic, and wear performance.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (4 — 1 Independent, 3 Dependent)

  1. Claim 1Independent Claim

    A method for preparing a rubber composition in which polybutene is dispersed in rubber in a solution phase (PIB extended rubber), the method comprising: dispersing hydrophobic extender oil and polybutene in water to prepare an extender oil/polybutene emulsion; adding the extender oil/polybutene emulsion to a latex-shaped rubber composition and uniformly dispersing the same in a solution to prepare a rubber/extension oil/polybutene composition; and solidifying, drying and molding the rubber/extender oil/polybutene composition on the latex shape through salting-out and acid precipitation, wherein the rubber is an emulsion styrene butadiene rubber (ESBR), and the polybutene is added in an amount of 1 wt % to 3 wt % on the basis of the rubber content.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the latex-shaped rubber composition is prepared by performing an emulsion-polymerization reaction of a composition including a monomer, water, an emulsifier, and an additive, and then recovering residual monomers.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the polybutene has a number average molecular weight of 300 to 3,000 g/mol.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the rubber composition is used as a rubber composition for a tire tread, a rubber composition for a shoe sole, a rubber composition for a belt, or a rubber composition for an asphalt additive.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATION This application claims priority under 35 U.S.C. § 119 or 365 to Korean Patent Application No. 10-2020-0175537, filed on Dec. 15, 2020. The entire teachings of the above application is incorporated herein by reference. BACKGROUND 1. Field The present disclosure relates to a method for producing a rubber composition, a rubber composition and a tire produced by employing the same. 2. Description of the Related Art In general, products using ESBR and natural rubber include tires, shoe soles, belts, hoses, sheets, or sealants, which must have excellent durability, and adhesives which must have excellent adhesion. In order to finally complete these products, it is common to directly input rubber as a raw material together with processing aids including reinforcing materials, additives, etc. into a blender and mix the input materials in a bulk state, or mix the input materials together after manufacturing a master batch, and thus a final rubber composite product can be produced. Korean Patent Publication No. 10-2020-0031529 introduces the results of improving the performance of rubber composites by dispersing a hydrocarbon traction resin in ESBR. However, types of extended resins include coumaron-indene-resin, petroleum resin, terpene polymer, alphamethyl styrene resin, and mixtures thereof, which have a glass transition temperature (Tg) exceeding 30 ° C. Since these materials are generally well soluble in organic solvents, rubbers such as solution styrene-butadiene rubber (SSBR), styrene-butadiene-styrene rubber (SBS), styrene-ethylene-butadiene-styrene rubber (SEBS), butadiene rubber (BR), butyl rubber (IR), isoprene-isobutylene rubber (IIR) or ethylene propylene rubber (EPM), ethylene propylene diene rubber (EPDM), and polyolefin elastomer (POE), which are prepared by solution polymerization, may be extended into a liquid phase by dissolving the resin in an organic solvent, followed by removing the solvent, thereby easily manufact

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (8)

Non-Patent Literature (2)

  • JP2007297416 machine translation (Year: 2024).
  • JP2008255168 machine translation (Year: 2024).