hottub.patents
US 12,677,648 B2#3195787 Most CitedActiveUnited States (USPTO)Utility

Treatment of tungsten surface for tungsten gap-fill

0Forward Citations (#3195787 Global)
0.0/yrCitation Velocity (#3195787 Global)
0.00Citation PageRank (#3195787 Global)
42Prior Art Cited
20Claims (3 Indep. · 17 Dep.)
5Drawings / Sheets

Abstract

A method and apparatus for tungsten gap-fill in semiconductor devices are provided. The method includes performing a gradient oxidation process to oxidize exposed portions of a liner layer, wherein the gradient oxidation process preferentially oxidizes an overhang portion of the liner layer, which obstructs or blocks top openings of one or more features formed within a field region of a substrate. The method further includes performing an etchback process to remove or reduce the oxidized overhang portion of the liner layer, exposing the liner layer to a chemical vapor transport (CVT) process to remove metal oxide remaining from the gradient oxidation process and the etchback process, and performing a tungsten gap-fill process to fill or partially fill the one or more features.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 42 · Forward citations: 0.

Claims (20 — 3 Independent, 17 Dependent)

  1. Claim 1Independent Claim

    A method of filling a feature on a substrate, comprising: performing a gradient oxidation process to oxidize exposed portions of a tungsten-containing liner layer, thereby forming tungsten oxide on the tungsten-containing liner layer, wherein the gradient oxidation process preferentially oxidizes an overhang portion of the tungsten-containing liner layer, which obstructs or blocks top openings of one or more features formed within a field region of a substrate; performing an etchback process to reduce the oxidized overhang portion of the tungsten-containing liner layer; exposing the tungsten-containing liner layer to a chemical vapor transport (CVT) process to remove the tungsten oxide remaining on the tungsten-containing liner layer, wherein the CVT process comprises exposing the tungsten-containing liner layer to an inductively coupled plasma (ICP) comprising hydrogen and oxygen; and performing a tungsten gap-fill process to fill or partially fill the one or more features.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the CVT process reduces the tungsten oxide to tungsten.

  3. Claim 3Depends on #1

    The method of claim 1, wherein exposing the tungsten-containing liner layer to the ICP is performed at a temperature of 400 degrees Celsius or less and comprises supplying a processing gas comprising greater than or equal to 90% of hydrogen gas of a total flow of hydrogen gas and oxygen gas.

  4. Claim 4Depends on #3

    The method of claim 3, wherein performing the gradient oxidation process, performing the etchback process, and exposing the tungsten-containing liner layer to the CVT process are performed in a processing chamber without breaking vacuum.

  5. Claim 5Depends on #4

    The method of claim 4, wherein the one or more features comprise a bottom surface and at least one sidewall and the tungsten-containing liner layer is formed over the at least one sidewall and the bottom surface.

  6. Claim 6Independent Claim

    A method of filling a feature formed on a substrate, comprising: depositing one or more tungsten-containing layers over a surface of a substrate, wherein the substrate comprises one or more features formed within a field region of the surface of the substrate, each of the one or more features comprises a sidewall surface and a bottom surface, and the one or more tungsten-containing layers are formed over the field region, the sidewall surface, and the bottom surface of the one or more features; exposing the surface of the substrate to a gradient oxidizing process, wherein the gradient oxidizing process forms preferentially oxidized regions of the tungsten-containing layers that are disposed over the field region of the one or more features; preferentially etching the preferentially oxidized regions of the one or more tungsten-containing layers formed on the surface of the substrate, wherein, after performing the process of preferentially etching the preferentially oxidized regions, a first portion of the one or more tungsten-containing layers remains on the bottom surface of each of the one or more features and a second portion of the one or more tungsten-containing layers remains on the sidewall surface of each of the one or more features; exposing at least the second portion of the one or more tungsten-containing layers to a post-etch treatment process to reduce oxidized tungsten to tungsten and remove contaminants from surfaces of the one or more tungsten-containing layers, wherein the post-etch treatment process comprises exposing the tungsten-containing layers to a hydrogen and oxygen inductively coupled plasma treatment; and filling the one or more features with a second tungsten layer, wherein the process of filling the one or more features with the second tungsten layer comprises preferentially growing the second tungsten layer from the second portion of the one or more tungsten-containing layers on the sidewall surface and the first portion of the one or more tungsten-containing layers that remain on the bottom surface of each of the one or more features.

  7. Claim 7Depends on #6

    The method of claim 6, wherein the post-etch treatment process further comprises exposing the tungsten-containing layers to argon.

  8. Claim 8Depends on #6

    The method of claim 6, wherein the hydrogen and oxygen inductively coupled plasma treatment is performed at temperatures of 400 degrees Celsius or less and comprises supplying a processing gas comprising greater than or equal to 90% of hydrogen gas of a total flow of hydrogen gas and oxygen gas.

  9. Claim 9Depends on #8

    The method of claim 8, wherein the sidewall surface is defined by a dielectric material selected from silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof.

  10. Claim 10Depends on #9

    The method of claim 9, wherein depositing the one or more tungsten-containing layers over the surface of the substrate, comprises: depositing a tungsten liner layer over the one or more features via a physical vapor deposition process; and depositing a boron-tungsten nucleation layer over the tungsten liner layer via an atomic layer deposition (ALD) process.

  11. Claim 11Depends on #10

    The method of claim 10, wherein filling the one or more features with the second tungsten layer comprises a chemical vapor deposition (CVD) gap-fill process.

  12. Claim 12Depends on #6

    The method of claim 6, wherein exposing the surface of the substrate to the gradient oxidizing process, preferentially etching the preferentially oxidized regions of the one or more tungsten-containing layers formed on the surface of the substrate, and exposing at least the second portion of the one or more tungsten-containing layers to the post-etch treatment process are performed in a first process chamber disposed on a cluster tool.

  13. Claim 13Independent Claim

    A method of filling a feature formed on a substrate, comprising: depositing one or more tungsten-containing layers over a surface of a substrate, wherein the substrate comprises one or more features formed within a field region of the surface of the substrate, each of the one or more features comprises a sidewall surface and a bottom surface, and the one or more tungsten-containing layers are formed over the field region, the sidewall surface, and the bottom surface of the one or more features; exposing the surface of the substrate to a gradient oxidizing process, wherein the gradient oxidizing process forms preferentially oxidized regions of the tungsten-containing layers that are disposed over the field region of the one or more features; preferentially etching the preferentially oxidized regions of the one or more tungsten-containing layers formed on the surface of the substrate, wherein, after performing the process of preferentially etching the preferentially oxidized regions, a first portion of the one or more tungsten-containing layers remains on the bottom surface of each of the one or more features and a second portion of the one or more tungsten-containing layers remains on the sidewall surface of each of the one or more features; exposing at least the second portion of the one or more tungsten-containing layers to a post-etch treatment process to reduce oxidized tungsten to tungsten and remove contaminants from surfaces of the one or more tungsten-containing layers, wherein the post-etch treatment process comprises a chemical vapor transport (CVT) process, the CVT process comprising a volatilization process and a reduction process, and the volatilization process proceeds via the following reaction (I) WO2+2H2O → WO2 (OH) 2+H2 and the reduction process proceeds via the following reaction (II) WO2 (OH) 2+3H2 → W+4H2O; and filling the one or more features with a second tungsten layer, wherein the process of filling the one or more features with the second tungsten layer comprises preferentially growing the second tungsten layer from the second portion of the one or more tungsten-containing layers on the sidewall surface and the first portion of the one or more tungsten-containing layers that remain on the bottom surface of each of the one or more features.

  14. Claim 14Depends on #13

    The method of claim 13, wherein the gradient oxidation process, the etching, and the post-etch treatment process are performed in a processing chamber without breaking vacuum.

  15. Claim 15Depends on #13

    The method of any of claim 13, wherein the sidewall surface is defined by a dielectric material selected from silicon oxide, silicon nitride, silicon oxynitride, or a combination thereof.

  16. Claim 16Depends on #15

    The method of claim 15, wherein depositing the one or more tungsten-containing layers over the surface of the substrate, comprises: depositing a tungsten liner layer over the one or more features via a physical vapor deposition process; and depositing a boron-tungsten nucleation layer over the tungsten liner layer via an atomic layer deposition (ALD) process.

  17. Claim 17Depends on #16

    The method of claim 16, wherein filling the one or more features with the second tungsten layer comprises a chemical vapor deposition (CVD) gap-fill process.

  18. Claim 18Depends on #13

    The method of claim 13, wherein exposing the surface of the substrate to the gradient oxidizing process, preferentially etching the preferentially oxidized regions of the one or more tungsten-containing layers formed on the surface of the substrate, and exposing at least the second portion of the one or more tungsten-containing layers to the post-etch treatment process are performed in a first process chamber disposed on a cluster tool.

  19. Claim 19Depends on #13

    The method of claim 13, wherein the volatilization process and the reduction process of the chemical vapor transport (CVT) process are performed cyclically to recover a conductive tungsten surface by removing surface contaminants comprising one or more of fluorine, boron, and nitrogen prior to filling the one or more features with the second tungsten layer.

  20. Claim 20Depends on #19

    The method of claim 19, wherein, after the etchback process and prior to filling the one or more features with the second tungsten layer, the post-etch treatment reduces impurity levels of the surface contaminants comprising one or more of fluorine, boron, and nitrogen on the tungsten-containing layers.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Patent Application Ser. No. 63/354,354, filed Jun. 22, 2022, which is incorporated by reference herein in its entirety. TECHNICAL FIELD The present disclosure relates to a method and apparatus for forming thin-films. More particularly, the disclosure relates to a method and apparatus for tungsten gap-fill in semiconductor devices. BACKGROUND The fabrication of microelectronic devices typically involves a complicated process sequence requiring hundreds of individual processes performed on semi-conductive, dielectric and conductive substrates. Examples of these processes include oxidation, diffusion, ion implantation, thin film deposition, cleaning, etching, lithography among other operations. Each operation is time consuming and expensive. With ever-decreasing critical dimensions for microelectronic devices, the design and fabrication for these devices on substrates become increasingly complex. Control of the critical dimensions and process uniformity becomes increasingly more significant. Complex multilayer stacks involve precise process monitoring of the critical dimensions for the thickness, roughness, stress, density, and potential defects. Multiple incremental processes in the process recipes for forming the devices ensure critical dimensions are maintained. However, each recipe process may utilize one or more processing chambers that add additional time for forming the devices in the processing systems and also provides additional opportunities for forming defects. Thus, each process adds to the overall fabrication cost for the completed microelectronic devices. Additionally, as critical dimensions on these devices shrink, past fabrication techniques encounter new hurdles. For example, as a liner and/or nucleation layer is prepared to grow a metal gap-fill, the liner and/or nucleation layer may be still be present on the sides of the gap causing the fill material to

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (42)

PatentTitleYearCitations
US 6,271,129 B1Method for forming a gap filling refractory metal layer having reduced stress200120
US 7,592,256 B2Method of forming tungsten film20091
US 7,776,698 B2Selective formation of silicon carbon epitaxial layer20103
US 8,071,478 B2Method of depositing tungsten film with reduced resistivity and improved surface morphology20119
US 9,082,826 B2Methods and apparatuses for void-free tungsten fill in three-dimensional semiconductor features201512
US 9,169,556 B2Tungsten growth modulation by controlling surface composition20159
US 9,748,105 B2Tungsten deposition with tungsten hexafluoride (WF6) etchback20177
US 10,680,008 B2Methods of manufacturing semiconductor devices20200
US 10,879,114 B1Conductive fill20202
US 11,177,387 B2Semiconductor device and manufacturing method thereof20210
US 11,978,666 B2Void free low stress fill20241
KR 20050032364 AHeater type humidifier having automatic switch function of water supply—2
KR 20070117397 ASystem and method for verifying a capability and a load of mobile communication system—2
KR 20130012032 AEnvironment-friendly multipurpose warter treatment apparatus—0
KR 20130109164 AMethod and apparatus for transmitting ack/nack in a wireless communication system based on tdd—6
KR 20130122713 AElectronic cigarette charged by cellphone charger—15
KR 20140106083 AMobile Terminal and Driving Method thereof—0
KR 20140120700 ASystem and method for diriver integration insurance—1
KR 20190122923 ADisplay apparatus and method of manufacturing the same—3
KR 20210066466 AMethod and system for interworking restaurant device and smart farm device—0
KR 20210134952 A개선된 용해도를 갖는 스테비올 글리코사이드 조성물—0

Non-Patent Literature (2)

  • Office Action for Korean Application No. 10-2025-7001743 dated Jul. 22, 2025.
  • International Opinion and Search Report dated Jul. 31, 2023 for International Application No. PCT/US2023/018108.