Electrodeposition of metals using an ionically resistive ionically permeable element or a shield spatially tailored to die-level patterns on a substrate
Abstract
An apparatus for electroplating a metal on a semiconductor substrate with high control over plated thickness on a die-level includes an ionically resistive ionically permeable element (e.g., a plate with channels), where the element allows for flow of ionic current through the element towards the substrate during electroplating, where the element includes a plurality of regions, each region having a pattern of varied local resistance, and where the pattern of varied local resistance repeats in at least two regions. An electroplating method includes providing a semiconductor substrate to an electroplating apparatus having an ionically resistive ionically permeable element or a grid-like shield having a pattern correlating with a pattern of features on the substrate, and plating metal, while the pattern on the substrate remains spatially aligned with the pattern of the element or the grid-like shield for at least a portion of the total electroplating time.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 28 · Forward citations: 0.
Claims (38 — 4 Independent, 34 Dependent)
- Claim 1Independent Claim
An electroplating apparatus comprising: (a) a plating chamber configured to contain an electrolyte and an anode while electroplating metal onto a semiconductor substrate; (b) a substrate holder configured to hold the semiconductor substrate such that a plating face of the substrate is separated from the anode during electroplating; and (c) an ionically resistive ionically permeable element comprising a substrate-facing surface and an opposing surface, wherein the element allows for flow of ionic current through the element towards the substrate during electroplating, wherein the element comprises a plurality of regions, each region having a pattern of varied local resistance, and wherein the pattern of varied local resistance repeats in at least two regions.
- Claim 2Depends on #1
The electroplating apparatus of claim 1, wherein each of the at least two regions has a length of at least about 5 mm.
- Claim 3Depends on #1
The electroplating apparatus of claim 1, wherein each of the at least two regions has a length of between about 5-50 mm.
- Claim 4Depends on #1
The electroplating apparatus of claim 1, wherein the ionically resistive ionically permeable element comprises at least five regions with repeating pattern of varied local resistance.
- Claim 5Depends on #1
The electroplating apparatus of claim 1, wherein each region has a pattern with varied local porosity.
- Claim 6Depends on #5
The electroplating apparatus of claim 5, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local porosity comprises a pattern of channels with different diameters.
- Claim 7Depends on #6
The electroplating apparatus of claim 6, wherein at least some of the channels have a varying diameter such that the at least some channels have smaller diameter on a first surface of the ionically resistive ionically permeable element than on a surface opposing the first surface.
- Claim 8Depends on #5
The electroplating apparatus of claim 5, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local porosity comprises a pattern of angled channels having different length.
- Claim 9Depends on #5
The electroplating apparatus of claim 5, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local porosity comprises a pattern of helical channels having different length.
- Claim 10Depends on #1
The electroplating apparatus of claim 1, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local resistance comprises a pattern of channels having different length.
- Claim 11Depends on #1
The electroplating apparatus of claim 1, wherein the ionically resistive ionically permeable element is a plate having a plurality of through-channels, wherein channel diameters at the substrate-facing surface of the ionically resistive ionically permeable element are less than about 2 mm.
- Claim 12Depends on #1
The electroplating apparatus of claim 1, wherein the ionically resistive ionically permeable element is positioned such that a distance from the substrate-facing surface of the ionically resistive ionically permeable element to the plating face of the semiconductor substrate is 10 mm or less.
- Claim 13Independent Claim
An electroplating apparatus comprising: (a) a plating chamber configured to contain an electrolyte and an anode while electroplating metal onto a semiconductor substrate; (b) a substrate holder configured to hold the semiconductor substrate such that a plating face of the substrate is separated from the anode during electroplating; and (c) a shield positioned within about 10 mm of the plating face of the semiconductor substrate, wherein the shield has a grid-like shape with a plurality of regions, each region comprising at least one opening, wherein each region has a pattern of varied local resistance, and wherein the pattern of varied local resistance repeats in at least two regions.
- Claim 14Depends on #13
The apparatus of claim 13, wherein the shield is configured to be moved during electroplating such as to agitate the electrolyte near the plating surface of the semiconductor substrate.
- Claim 15Depends on #14
The apparatus of claim 14, wherein the shield comprises one or more protrusions and/or has variable thickness configured to facilitate agitation of the electrolyte during shield movement.
- Claim 16Depends on #1
The electroplating apparatus of claim 1, wherein the apparatus is further configured to generate a lateral flow of electrolyte in a direction parallel to the plating face of the semiconductor substrate.
- Claim 17Depends on #1
The electroplating apparatus of claim 1, further comprising a uniform ionically resistive ionically permeable element stacked with the ionically resistive ionically permeable element of claim 1.
- Claim 18Independent Claim
An ionically resistive ionically permeable element, wherein the element is configured to allow for flow of ionic current through the element towards a substrate during electroplating, wherein the element comprises a plurality of regions, each region having a pattern of varied local resistance, and wherein the pattern of varied local resistance repeats in at least two regions.
- Claim 19Depends on #18
The ionically resistive ionically permeable element of claim 18, wherein each of the at least two regions has a length of at least about 5 mm.
- Claim 20Depends on #18
The ionically resistive ionically permeable element of claim 18, wherein each of the at least two regions has a length of between about 5-50 mm.
- Claim 21Depends on #18
The ionically resistive ionically permeable element of claim 18, wherein each region has a pattern with varied local porosity.
- Claim 22Depends on #21
The ionically resistive ionically permeable element of claim 21, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local porosity comprises a pattern of channels with different diameters.
- Claim 23Depends on #22
The ionically resistive ionically permeable element of claim 22, wherein the ionically resistive ionically permeable element comprises channels having a smaller diameter on one side of the ionically resistive element than on an opposing side.
- Claim 24Depends on #21
The ionically resistive ionically permeable element of claim 21, wherein the ionically resistive ionically permeable element comprises non-communicating through-channels, and wherein the pattern of varied local porosity comprises a pattern of angled channels having different length.
- Claim 25Independent Claim
A method of electrodepositing a metal onto a semiconductor substrate, the method comprising: (a) providing a semiconductor substrate having a pattern of features into an electroplating apparatus, wherein the electroplating apparatus comprises an ionically resistive ionically permeable element or a grid-like shield having a plurality of openings, wherein the ionically resistive ionically permeable element or the grid-like shield is positioned within about 10 mm of a plating face of the semiconductor substrate, and wherein the ionically resistive ionically permeable element or the grid like shield comprise a pattern correlating to the pattern of features of the semiconductor substrate; (b) registering orientation of the semiconductor substrate with the ionically resistive element or the grid-like shield such that the pattern of the features on the semiconductor substrate and the matching pattern of the ionically resistive element or the grid-like shield are spatially aligned; and (c) electroplating metal onto the semiconductor substrate, while maintaining the semiconductor substrate stationary or spatially aligned relative to the ionically resistive element or the grid-like shield at least during a portion of a total electroplating time.
- Claim 26Depends on #25
The method of claim 25, wherein the features on the semiconductor substrate are through-mask features, and wherein isolated regions of through-mask features are matched with more resistive portions of the ionically resistive ionically permeable element or are more shielded by the grid-like shield than denser regions of through-mask features.
- Claim 27Depends on #25
The method of claim 25, wherein the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive element or the grid-like shield for at least 10% of the total electroplating time.
- Claim 28Depends on #25
The method of claim 25, wherein the method comprises providing a lateral flow of electrolyte parallel to the semiconductor substrate during electroplating.
- Claim 29Depends on #28
The method of claim 28, wherein (c) comprises electroplating metal onto the semiconductor substrate, wherein the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive element or the grid-like shield during the total electroplating time.
- Claim 30Depends on #28
The method of claim 28, wherein (c) comprises electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive element or the grid-like shield during about 30-90% of the total electroplating time and such that the semiconductor substrate is rotated relative to the ionically resistive element or the grid-like shield during about the remainder of the total electroplating time.
- Claim 31Depends on #28
The method of claim 28, wherein (c) comprises electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains spatially aligned relative to the ionically resistive element or the grid-like shield during about 30-90% of the total electroplating time and such that the semiconductor substrate is rotated relative to the ionically resistive element or the grid-like shield for the remaining time of the total electroplating time, wherein the ionically resistive ionically permeable element or the grid-like shield is moved with respect to the semiconductor substrate in at least one of rotational and lateral translational movement.
- Claim 32Depends on #28
The method of claim 28, wherein the semiconductor substrate has a symmetrical pattern of features and wherein (c) comprises: (i) electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive element or the grid-like shield during a portion of the total electroplating time; (ii) rotating the substrate relative to the ionically resistive element or the grid-like shield by 180 degrees; and (iii) continuing electroplating in a new orientation.
- Claim 33Depends on #32
The method of claim 32, further comprising repeating (i)-(iii) at least once.
- Claim 34Depends on #28
The method of claim 28, wherein the semiconductor substrate has a symmetrical pattern of features and wherein (c) comprises: (i) electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive element or the grid-like shield during a portion of the total electroplating time; (ii) rotating the substrate relative to the ionically resistive element or the grid-like shield by 90 degrees; and (iii) continuing electroplating in a new orientation.
- Claim 35Depends on #28
The method of claim 28, wherein (c) comprises electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive ionically permeable element or the grid-like shield during a portion of the total electroplating time in a first electroplating cell; and electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to a second ionically resistive ionically permeable element or a second grid-like shield during a portion of the total electroplating time in a second electroplating cell, wherein both in the first cell and the second cell matching and registration for the semiconductor substrate feature pattern is retained, but wherein a direction of lateral flow in the second cell is opposite relative to the features of the semiconductor substrate from the first cell.
- Claim 36Depends on #28
The method of claim 28, wherein (c) comprises electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to the ionically resistive ionically permeable element or the grid-like shield during a portion of the total electroplating time in a first electroplating cell; and electroplating metal onto the semiconductor substrate, such that the semiconductor substrate remains stationary or spatially aligned relative to a second ionically resistive ionically permeable element or a second grid-like shield during a portion of the total electroplating time in a second electroplating cell, wherein both in the first cell and the second cell matching and registration for the semiconductor substrate feature pattern is retained, but wherein a direction of lateral flow in the second cell is different relative to the features of the semiconductor substrate from the first cell; and continue transferring the semiconductor substrate consecutively to multiple electroplating cells and electroplating in multiple electroplating cells, wherein a direction of lateral flow in the cells relative to the features of the semiconductor substrate is different.
- Claim 37Depends on #28
The method of claim 28, wherein (c) comprises varying a direction of lateral electrolyte flow during electroplating.
- Claim 38Depends on #25
The method of claim 25, further comprising: applying photoresist to the semiconductor substrate; exposing the photoresist to light; patterning the photoresist and transferring the pattern to the semiconductor substrate; and selectively removing the photoresist from the semiconductor substrate.
Technical Overview & Description
INCORPORATION BY REFERENCE A PCT Request Form is filed concurrently with this specification as part of the present application. Each application that the present application claims benefit of or priority to as identified in the concurrently filed PCT Request Form is incorporated by reference herein in its entirety and for all purposes. FIELD OF THE INVENTION The present disclosure relates generally to a method and apparatus for electroplating a metal layer on a semiconductor wafer. More particularly, the method and apparatus described herein are useful for controlling plating uniformity. BACKGROUND In semiconductor device manufacturing, a conductive material, such as copper, is often deposited by electroplating onto a seed layer of metal to fill one or more recessed features on a semiconductor wafer substrate. Electroplating is a method of choice for depositing metal into the vias and trenches of the wafer during damascene processing, and is also used in wafer level packaging (WLP) applications to form pillars and lines of metal on the wafer substrate. Another application of electroplating is filling of Through-Silicon Vias (TSVs), which are relatively large vertical electrical connections used in 3D integrated circuits and 3D packages. In some electroplating substrates, the seed layer is exposed over the entire surface of the substrate prior to electroplating (typically in damascene and TSV processing), and electrodeposition of metal occurs over the entirety of the substrate. In other electroplating substrates, a portion of the seed layer is covered by a non-conducting mask material, such as by photoresist, while another portion of the seed layer is exposed. In such substrates with partially masked seed layer electroplating occurs only over the exposed portions of the seed layer, while the covered portions of the seed layer are protected from being plated upon. Electroplating on a substrate having a seed layer that is coated with patterned mask material (e.g., phot
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (28)
Non-Patent Literature (10)
- International Preliminary Report on Patentability dated Aug. 10, 2023 in Application No. PCT/US2022/012969.
- International Preliminary Report on Patentability dated Sep. 28, 2023, in PCT Application No. PCT/US2022/020436.
- International Search Report and Written Opinion dated Dec. 6, 2024 in PCT Application No. PCT/US2024/043164.
- International Search Report and Written Opinion dated Jul. 5, 2022, in PCT Application No. PCT/US2022/020436.
- International Search Report and Written Opinion dated May 17, 2022, in PCT Application No. PCT/US2022/012969.
- KR Office Action dated Apr. 27, 2023, in application No. KR10-2016-0057962 with English translation.
- KR Office Action dated Dec. 20, 2023 in KR Application No. 10-2016-0057962 with English Translation.
- KR Office Action dated Mar. 22, 2022, in Application No. KR1020210084236 with English translation.
- KR Office Action dated May 17, 2022, in Application No. KR10-2016-0030112 with English translation.
- KR Office Action dated Sep. 14, 2022, in Application No. KR10-2022-0101229 with English translation.