US 12,640,392 B2#3232514 Most CitedActiveUnited States (USPTO)Utility

Method for preparing amorphous lithium borosilicate

0Forward Citations (#3232514 Global)
0.0/yrCitation Velocity (#3232514 Global)
0.00Citation PageRank (#3232514 Global)
80Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a vapour deposition method for preparing an amorphous lithium borosilicate or doped lithium borosilicate compound, the method comprising: providing a vapour source of each component element of the compound, wherein the vapour sources comprise at least a source of lithium, a source of oxygen, a source of boron, and a source of silicon, and, optionally, a source of at least one dopant element; delivering a flow of said lithium, said oxygen, said boron and said silicon, and, optionally, said dopant element; and co-depositing the component elements from the vapour sources onto a substrate wherein the component elements react on the substrate to form the amorphous compound; wherein the amorphous lithium borosilicate or doped lithium borosilicate compound has a lithium content in the range 40-65 atomic %, based on the combined atomic percentages of lithium, boron and silicon.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A vapour deposition method for preparing an amorphous lithium borosilicate or doped lithium borosilicate compound, the method comprising: providing a vapour source of each component element of the compound, wherein the vapour sources comprise at least a source of lithium, a source of oxygen, a source of boron, and a source of silicon, and, optionally, a source of at least one dopant element; delivering a flow of said lithium, said oxygen, said boron and said silicon, and, optionally, said dopant element; and co-depositing the component elements from the vapour sources onto a substrate wherein the component elements react on the substrate to form the amorphous compound; wherein the amorphous lithium borosilicate or doped lithium borosilicate compound has a lithium content in the range 45-65 atomic %, a boron content in the range 15-35 atomic %, and a silicon content in the range 10-25 atomic %, based on the combined atomic percentages of lithium, boron and silicon.

  2. Claim 2Depends on #1

    The vapour deposition method according to claim 1, wherein the lithium borosilicate or doped lithium borosilicate compound has a lithium content of 63 atomic % or less, based on the combined atomic percentages of lithium, boron and silicon.

  3. Claim 3Depends on #2

    The vapour deposition method according to claim 2, wherein the lithium borosilicate or doped lithium borosilicate compound has a lithium content of 60 atomic % or less, based on the combined atomic percentages of lithium, boron and silicon.

  4. Claim 4Depends on #1

    The vapour deposition method according to claim 1, wherein the lithium borosilicate or doped lithium borosilicate compound has a lithium content of at least 50 atomic %, based on the combined atomic percentages of lithium, boron and silicon.

  5. Claim 5Depends on #1

    The vapour deposition method according to claim 1, wherein the amorphous compound is a lithium borosilicate compound that consists essentially of a system of lithium oxide in combination with silicon oxide and boron oxide.

  6. Claim 6Depends on #1

    The vapour deposition method according to claim 1, wherein the composition of the lithium borosilicate compound or doped lithium borosilicate compound lies in the region bounded by 64 atomic % Li-26 atomic % B-10 atomic % Si; 63 atomic % Li-21 atomic % B-16 atomic % Si; 59 atomic % Li-18 atomic % B-23 atomic % Si; 56 atomic % Li-32 atomic % B-12 atomic % Si; and 51 atomic % Li-32 atomic % B-17 atomic % Si; wherein the atomic percentages of each of lithium, boron and silicon are based on the combined percentages of lithium, boron and silicon.

  7. Claim 7Depends on #1

    The vapour deposition method according to claim 1, wherein the composition of the lithium borosilicate compound or doped lithium borosilicate compound lies in the region bounded by 60 atomic % Li-27 atomic % B-13 atomic % Si; 59 atomic % Li-18 atomic % B-23 atomic % Si; 56 atomic % Li-32 atomic % B-12 atomic % Si; and 51 atomic % Li-32 atomic % B-17 atomic % Si; wherein the atomic percentages of each of lithium, boron and silicon are based on the combined percentages of lithium, boron and silicon.

  8. Claim 8Depends on #1

    The vapour deposition method according to claim 1, wherein the composition of the lithium borosilicate compound or doped lithium borosilicate compound lies in the region bounded by 60 atomic % Li-27 atomic % B-13 atomic % Si; 60 atomic % Li-25 atomic % B-15 atomic % Si; 59 atomic % Li-22 atomic % B-19 atomic % Si; 56 atomic % Li-32 atomic % B-12 atomic % Si; and 53 atomic % Li-32 atomic % B-15 atomic % Si; wherein the atomic percentages of each of lithium, boron and silicon are based on the combined percentages of lithium, boron and silicon.

Technical Overview & Description

This application is a national phase of International Application No. PCT/GB2020/053075 filed Dec. 1, 2020, which claims priority to United Kingdom Application No. 1917824.3 filed Dec. 5, 2019, each of which is hereby incorporated herein by reference in its entirety. FIELD OF THE INVENTION The present invention relates to a method for preparing amorphous lithium borosilicate or doped lithium borosilicate compounds by vapour deposition. BACKGROUND TO THE INVENTION The deposition of materials in thin film form is of great interest owing to the many applications of thin films, and a range of different deposition techniques are known. Various techniques are more or less suitable for particular materials, and the quality, composition and properties of the thin film produced typically depends greatly on the process used for its formation. Consequently, much research is devoted to developing deposition processes that can produce thin films appropriate for specific applications. An important application of thin film materials is in solid state thin film cells or batteries, such as lithium ion cells. Such batteries are composed of at least three components. Two active electrodes (the anode and the cathode) are separated by an electrolyte. Each of these components is formed as a thin film, deposited in sequence on a supporting substrate. Additional components such as current collectors, interface modifiers and encapsulations may also be provided. In manufacture, the components may be deposited in the order of cathode current collector, cathode, electrolyte, anode, anode current collector and encapsulation, for example. In the lithium ion example, the anode and the cathode are capable of reversibly storing lithium. Other requirements of the anode and cathode materials are high gravimetric and volumetric storage capacities which can be achieved from a low mass and volume of material, while the number of lithium ions stored per unit should be as high as possible. The materials s

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (80)

PatentTitleYearCitations

Non-Patent Literature (10)

  • Sun, et al., Phase separation and electrical conductivity of lithium borosilicate glasses for potential thin film solid electrolytes, 162 (2) Journal of Power Sources, 1341-1345, Nov. 22, 2006. (Year: 2006).
  • 1 First Examination Report issued to the corresponding Japanese application No. 2021-502892 on Aug. 15, 2023.
  • Ito, et al.,
  • “
  • Ionic Conductivity Of Li2O
  • —
  • B2O3 Thin Films,
  • ”
  • Journal of Non-Crystalline Solids, 57, 1983, pp. 389-400.
  • Rim, et al.,