Braze repair using metal coupon with porous region
Abstract
A component includes a body having a coupon opening defined therein, and an additively manufactured (AM) metal coupon including a dense region, a porous region adjacent the dense region, and a coupon outer surface. The porous region has a first cross-sectional area at a first location at or near the coupon outer surface and a second cross-sectional area less than the first cross-sectional area at a second location distal from the coupon outer surface. A braze material couples the metal coupon in the coupon opening and infiltrates into the porous region, e.g., based at least on a characteristic of the porosity thereof. The dense region may have a third cross-sectional area at the first location and a fourth cross-sectional area greater than the third cross-sectional area at the second location so it can direct the braze material in the porous region toward an inner surface of the coupon opening.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A component, comprising: a body having a coupon opening defined therein; an additively manufactured (AM) metal coupon including a dense region that has a porosity of less than 1% open space volume to total volume of the dense region such that a braze material cannot infiltrate the dense region, a porous region adjacent the dense region, and a coupon outer surface, wherein the porous region has a first cross-sectional area at a first location at or near the coupon outer surface and a second cross-sectional area less than the first cross-sectional area at a second location distal from the coupon outer surface; and wherein braze material couples the AM metal coupon in the coupon opening defined in the body, the braze material infiltrated into the porous region.
- Claim 2Depends on #1
The component of claim 1, wherein the dense region has a third cross-sectional area at the first location and a fourth cross-sectional area greater than the third cross-sectional area at the second location.
- Claim 3Depends on #1
The component of claim 1, wherein the porous region has a porosity between 2% to 50% open space volume to total volume of the porous region.
- Claim 4Depends on #1
The component of claim 1, wherein the porous region has a variable porosity having a higher porosity at the first location and a lower porosity towards a bottom of the coupon opening, and wherein the porous region includes more braze material at the first location than at the second location.
- Claim 5Depends on #1
The component of claim 1, wherein the body is solid material.
- Claim 6Depends on #1
The component of claim 1, wherein the AM metal coupon has a near net shape of the coupon opening in the body of the component.
- Claim 7Depends on #1
The component of claim 1, further comprising a defect coupon opening in the body adjacent the coupon opening, wherein the braze material infiltrates at least part of the defect coupon opening.
- Claim 8Independent Claim
A method of repairing a component having a defect and a component surface, the method comprising: removing at least part of the defect at the component surface by forming a coupon opening in the component; additively manufacturing a metal coupon; positioning the additively manufactured (AM) metal coupon in the coupon opening, the AM metal coupon including a dense region that has a porosity of less than 1% open space volume to total volume of the dense region such that a braze material cannot infiltrate the dense region, a porous region adjacent the dense region, and a coupon outer surface, wherein the porous region has a first cross-sectional area at a first location at or near the coupon outer surface and a second cross-sectional area less than the first cross-sectional area at a second location distal from the coupon outer surface; positioning the braze material at a junction of the coupon outer surface of the AM metal coupon and the component surface of the component; and infiltrati
Technical Overview & Description
TECHNICAL FIELD The disclosure relates generally to component repair, and more specifically, to component repair using a metal coupon with a porous region. BACKGROUND Industrial components occasionally require repair. For example, hot gas path components that are used in turbomachines to direct a working fluid to create energy may require repair. Hot gas path components can take a variety of forms, such as turbine rotating blades or stationary vanes, that include airfoils that direct a working fluid to create energy. Rotating blades are coupled to and act to turn a turbine rotor, and stationary vanes are coupled to a casing of the turbomachine to direct the working fluid towards the rotating blades. Additive manufacturing, such as direct metal laser melting (DMLM) or selective laser melting (SLM), has emerged as a reliable manufacturing method for making industrial components. The advent of additive manufacturing techniques has also provided the ability to replace sections of components such as part of a leading or trailing edge of a turbomachine nozzle. For example, a portion of a leading edge of a turbomachine nozzle may be removed, leaving a cutout in the nozzle, and a new section (referred to herein as a “ coupon ” ) may be coupled in the cutout. The coupon is additively manufactured to have a shape that at least generally matches that of the cutout. The coupon can replace a section of a used turbomachine nozzle or be added as part of a new turbomachine nozzle. However, replacement coupons are made with the same materials and exterior structure as the removed portion of the component. Consequently, the replacement coupons suffer from some of the same drawbacks as the original component and/or cutout with no improvement to general performance characteristics such as coupon strength, oxidation resistance, cycle fatigue, stress/strain resistance, ductility, wear resistance, thermal or electrical conductivity, and/or decreased mass. A single braze material is used t
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (80)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Translation of EP-2450471A1 (no date available).
- Non-Final Office Action dated May 9, 2025 for related U.S. Appl. No. 18/495,808, 16 pages.
- Office Action (Non-Final Rejection) dated Jul. 28, 2025 for related U.S. Appl. No. 18/417,625, 16 pages.
- Office Action (Final Rejection) dated Aug. 8, 2025 for related U.S. Appl. No. 18/495,816, 15 pages.
- Notice of Allowance and Fees Due dated Aug. 5, 2025 for related U.S. Appl. No. 18/495,817, 9 pages.
- Office Action (Non-Final Rejection) dated Aug. 11, 2025 for related U.S. Appl. No. 18/495,809, 13 pages.
- Office Action (Non-Final Rejection) dated Aug. 12, 2025 for related U.S. Appl. No. 18/495,810, 14 pages.
- EP Search Report for EP Application No. 24223562.0, dated Jul. 8, 2025, 7 pages.
- EP Search Report for EP Application No. 24204162.2, dated Mar. 14, 2025, 11 pages.
- Final Office Action for related U.S. Appl. No. 18/495,803, dated Mar. 19, 2025, 26 pages.