A method for manufacturing a coating material formed on an inner surface of a chamber is provided. The method includes: i) providing a substrate including at least one material selected from the group consisting of SiC, SiO 2 , and Al 2 O 3 ; ii) providing a first coating portion including SiO x (0.1 ≤ x ≤ 2 as a molar ratio) or AlO y (0.1 ≤ y ≤ 1.5 as a molar ratio) on the substrate; iii) providing a second coating portion including YO z (0.1 ≤ z ≤ 1.5 as a molar ratio) on the first coating portion; iv) providing a laminate in which the first coating portion and the second coating portion are repeatedly stacked; and v) heating the laminate to provide a coating layer of a single crystalline layer by a solid-state reaction between the first coating portion and the second coating portion.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A method for manufacturing a coating material formed on an inner surface of a chamber, the method comprising: providing a substrate comprising at least one material selected from the group consisting of SiC, SiO2, and Al2O3; providing a first coating portion with a thickness of 0.4 μ m to 1 μ m comprising AlOy (0.1 ≤ y ≤ 1 as a molar ratio) on the substrate by physical vapor deposition; providing a second coating portion with a thickness of 0.5 μ m to 2.5 μ m comprising YOz (0.1 ≤ z ≤ 1 as a molar ratio) on the first coating portion by physical vapor deposition; providing a laminate in which the first coating portion and the second coating portion are repeatedly stacked; and heating the laminate to provide a coating layer of a single crystalline layer by a solid-state reaction between the first coating portion and the second coating portion.
- Claim 2Depends on #1
The method of claim 1, wherein the substrate comprises the Al2O3 in the providing the substrate, the laminate is heated at 1000 ° C. to 1500 ° C., and the coating layer comprises Y α Al β O γ (2.5 ≤ α ≤ 3.5, 4.5 ≤ β ≤ 5.5, 11.5 ≤ γ ≤ 12.5 as a molar ratio) in the providing the coating layer.
- Claim 3Depends on #1
The method of claim 1, wherein the substrate comprises the Al2O3 in the providing the substrate, the laminate is heated at 1000 ° C. to 1500 ° C., and the coating layer comprises at least one compound selected from the group consisting of Y3Al5O12, YAlO4, and Y4Al2O9 in the providing the coating layer.
- Claim 4Depends on #3
The method of claim 3, wherein a ratio of the thickness of the second coating portion to the thickness of the first coating portion is 0.8 to 1.2 when the coating layer comprises Y3Al5O12 in the providing the laminate.
- Claim 5Depends on #3
The method of claim 3, wherein a ratio of the thickness of the second coating portion to the thickness of the first coating portion is 1.3 to 1.8 when the coating layer comprises YAlO4 in the providing the laminate.
- Claim 6Depends on #3
The method of claim 3, wherein the ratio of the thickness of the second coating portion to the thickness of the first coating portion is 1.6 to 2.5 when the coating layer comprises Y4Al2O9 in the providing the laminate.
- Claim 7Depends on #1
The method of claim 1, wherein the laminate is heated to 800 ° C. to 1300 ° C., the thickness of the coating layer is smaller than the thickness of the laminate, and a ratio of the thickness of the laminate to the thickness of the coating layer is 1.25 to 1.6 In the providing the coating layer.
- Claim 8Depends on #1
The method of claim 1, wherein the first coating portion and the second coating portion are repeatedly stacked 2 to 10 times in the providing the laminate.
Technical Overview & Description
TECHNICAL FIELD The present invention relates to a chamber coating material and its manufacturing method. More specifically, the present invention relates to a chamber coating material having corrosion resistance even in plasma or a strong corrosive atmosphere, and a method for manufacturing the same. BACKGROUND ART In recent years, due to the rapid development of the mobile industry, miniaturization and high integration of semiconductors and the like are more urgently required. Therefore, in order to highly integrate semiconductors, new technologies for stacking in 3D form are being developed, and in this case, a different process from the existing semiconductor process is required. That is, since it is necessary to form the device in an erected state, then quickly etch and remove a specific part in a short time, an etching gas or solution having strong corrosiveness is required. By using such an etchant having strong acidity, the window or inner wall in the chamber for manufacturing the device is corroded. That is, as the inner surface of the chamber comes into contact with plasma in which a reactive halogen gas is injected or a strong acid etching atmosphere, resulting aggregates fall and contaminate the device being manufactured. Therefore, it is necessary to prepare a coating material capable of maintaining corrosion resistance even in plasma or a strongly acidic atmosphere in which reactive halogen gas is injected. DISCLOSURE Technical Problem A coating material for a corrosion-resistant chamber for plasma or a strong corrosive atmosphere is provided. In addition, a method for manufacturing the aforementioned coating material is provided. Technical Solution The method of manufacturing a coating material for a chamber according to an embodiment of the present invention includes: i) providing a substrate including at least one material selected from the group consisting of SiC, SiO 2 , and Al 2 O 3 ; ii) providing a first coating portion including SiO x (0.1 ≤ x
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (22)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (4)
- Laura Granados et al. Silicate glass-to-glass hermetic bonding for encapsulation of next-generation optoelectronics: A Review. Elsevier. Material Today. vol. 47. Jul./Aug. 2021 (Year: 2021).
- KIPO, A PCT Search Report
- &
- Written Opinion of Application No. PCT/KR2020/003386, dated Nov. 30, 2020.