Abstract

Described herein is a process for making a particulate (oxy)hydroxide of TM, where TM are metals and TM includes at least 60 mol-% nickel, and where said process includes the steps of: (a) providing an aqueous solution ( α ) including water-soluble salts of Ni and of at least one metal selected from the group consisting of Co and Mn, and, optionally, at least one further metal selected from the group consisting of Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and an aqueous solution ( β ) an alkali metal hydroxide and, optionally, an aqueous solution ( γ ) including ammonia, (b) combining the solution ( α ) and the solution ( β ) and, if applicable, the solution ( γ ) at a pH value in a range of from 11.0 to 13.0 in a stirred tank reactor, thereby creating solid particles of a hydroxide containing nickel, said solid particles being slurried.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.

Claims (16 — 2 Independent, 14 Dependent)

  1. Claim 1Independent Claim

    A process for making a particulate (oxy)hydroxide of TM, wherein TM are metals and TM comprises at least 60 mol-% nickel, and wherein said process comprises the steps of: (a) providing an aqueous solution (α) comprising water-soluble salts of Ni and of at least one metal selected from the group consisting of Co and Mn, and, optionally, at least one further metal selected from the group consisting of Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and in a range of from 0.01 to 0.05 mol-% of α - or β -amino acid of TM or the alkali metal salt of TM, and an aqueous solution (β) comprising an alkali metal hydroxide and, optionally, an aqueous solution (γ) comprising ammonia, (b) combining the solution (α) and the solution (β) and, if applicable, the solution (γ) at a pH value in a range of from 10.0 to 13.0 in a stirred tank reactor, thereby creating solid particles of a hydroxide comprising nickel, said solid particles being slurried.

  2. Claim 2Depends on #1

    The process according to claim 1, wherein TM is a combination of metals according to general formula (I) (Ni a Co b Mn c) 1-d M d (I) wherein a is in a range of from 0.7 to 0.99, b is zero or in a range of from 0.01 to 0.2, c is in a range of from zero to 0.2, and d is in a range of from zero to 0.1, M is at least one of Al, Mg, Ti, Mo, Nb, Ta, W and Zr, and b+c > zero, and a+b+c=1.

  3. Claim 3Depends on #1

    The process according to claim 1, wherein said α -amino acid is selected from the group consisting of glycine, the sodium of glycine, and potassium salts.

  4. Claim 4Depends on #1

    The process according to claim 1, wherein the aqueous solutions (α) and (β) are fed into the stirred tank reactor through a coaxial nozzle.

  5. Claim 5Depends on #1

    The process according to claim 1, wherein step (b) is performed in two sub-steps (b1) and (b2), and wherein sub-step (b1) is performed at a pH value that is 0.2 to 2.0 units higher than sub-step (b2).

  6. Claim 6Depends on #1

    The process according to claim 1, wherein step (b) is performed at a pH value that varies by 0.2 units at most.

  7. Claim 7Independent Claim

    A particulate (oxy)hydroxide of TM, wherein TM comprises at least 70 mol-% nickel, wherein said (oxy)hydroxide has an average secondary particle diameter (D50) in a range of from 2 to 20 μ m, wherein TM includes at least one metal selected from the group consisting of Co and Mn, and, optionally, at least one further metal selected from the group consisting of Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, wherein said (oxy)hydroxide comprises in a range of from 0.05% to 1% by weight C as organic carbon, and wherein at least 60 vol.-% of the secondary particles comprise agglomerated primary particles that are perfectly radially oriented primary articles and primary particles whose deviation to a perfectly radial orientation is at most 5 degrees.

  8. Claim 8Depends on #7

    The particulate (oxy)hydroxide according to claim 7, wherein particles of the particulate (oxy)hydroxide display multiple concentric rings, detectable by scanning electron microscopy of a cross-section of such particles.

  9. Claim 9Depends on #7

    The particulate (oxy)hydroxide according to claim 7, wherein TM is a combination of metals according to general formula (I) (Ni a Co b Mn c) 1-d M d (I) wherein a is in a range of from 0.7 to 0.99, b is zero or in a range of from 0.01 to 0.2, c is in a range of from zero to 0.2, and d is in a range of from zero to 0.1, M is at least one of Al, Mg, Ti, Mo, Nb, Ta, W and Zr, and a+b+c=1.

  10. Claim 10Depends on #7

    The particulate (oxy)hydroxide according to claim 7, wherein the particulate (oxy)hydroxide has a bimodal particle size distribution with a first maximum being in a range from 3 to 7 μ m and a second maximum in a range from 11 to 17 μ m.

  11. Claim 11Depends on #7

    The particulate (oxy)hydroxide according to claim 7, wherein the particulate (oxy)hydroxide has a form factor in a range of from 0.87 to 0.99.

  12. Claim 12Depends on #7

    A method of using the particulate (oxy)hydroxide according to claim 7, the method comprising using the particulate (oxy)hydroxide for manufacture of cathode active materials for lithium ion batteries.

  13. Claim 13Depends on #7

    A process for manufacture of an electrode active material for lithium ion batteries, wherein said process comprises the steps of mixing the particulate (oxy)hydroxide according to claim 7 with a source of lithium and thermally treating said mixture at a temperature in a range of from 600 to 1000 ° C.

  14. Claim 14Depends on #7

    A cathode comprising (1) at least one electrode active material according to claim 7, (2) carbon in electrically conductive form, and (3) a binder material.

  15. Claim 15Depends on #14

    The cathode according to claim 14, wherein the cathode comprises (1) 80 to 98% by weight cathode active material, (2) 1 to 17% by weight of carbon, and (3) 1 to 15% by weight of binder material, wherein the percentages refer to a sum of (1), (2) and (3).

  16. Claim 16Depends on #7

    A process for manufacture of an electrode active material for lithium ion batteries, wherein said process comprises the steps of mixing a pre-calcined particulate (oxy)hydroxide according to claim 7 with a source of lithium and thermally treating said mixture at a temperature in a range of from 600 to 1000 ° C.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a U.S. National Phase Application of PCT/EP2021/075441, filed Sep. 16, 2021, which claims the benefit of priority to European Patent Application No. 20201539.2, filed Oct. 13, 2020, the entire contents of which are hereby incorporated by reference herein. The present invention is directed towards a process for making a particulate (oxy)hydroxide of TM wherein TM are metals and TM comprises at least 60 mol-% nickel and wherein said process comprises the steps of: (a) Providing an aqueous solution ( α ) containing water-soluble salts of Ni and of at least one metal selected from Co and Mn, and, optionally, at least one further metal selected from Ti, Zr, Mo, W, Al, Mg, Nb, and Ta, and in the range of from 0.01 to 0.05 mol-%, referring to TM, of α - or β -amino acid or its alkali metal salt, and an aqueous solution ( β ) containing an alkali metal hydroxide and, optionally, an aqueous solution ( γ ) containing ammonia, (b) combining a solution ( α ) and a solution ( β ) and, if applicable, a solution ( γ ) at a pH value in the range of from 10.0 to 13.0 in a stirred tank reactor, thereby creating solid particles of a hydroxide containing nickel, said solid particles being slurried. Lithium ion secondary batteries are modern devices for storing energy. Many application fields have been and are contemplated, from small devices such as mobile phones and laptop computers through car batteries and other batteries for e-mobility. Various components of the batteries have a decisive role with respect to the performance of the battery such as the electrolyte, the electrode materials, and the separator. Particular attention has been paid to the cathode materials. Several materials have been suggested, such as lithium iron phosphates, lithium cobalt oxides, and lithium nickel cobalt manganese oxides. Although extensive research has been performed the solutions found so far still leave room for improvement. The electrode

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 5,861,131 AProcess for producing nickel hydroxide19996
US 2010310869 A1POWDER NiaMbOx(OH)y COMPOUNDS, PROCESSES FOR MAKING THE SAME, AND USES THEREOF IN BATTERIES—9
US 2017352884 A1Nickel cobalt manganese composite hydroxide and process for producing same—10
US 2021005877 A1Positive electrode material for rechargeable lithium ion batteries—6
US 2022006084 A1Method of Preparing Positive Electrode Active Material Precursor and Positive Electrode Active Material Precursor—0
US 2022399544 A1Nickel manganese composite hydroxide and method for producing same, positive electrode active material for nonaqueous electrolyte secondary battery and method for producing same, and nonaqueous electrolyte secondary battery—2
US 2023081939 A1Positive Electrode Active Material Precursor for Secondary Battery, Positive Electrode Active Material, and Lithium Secondary Battery Including the Positive Electrode Active Material—0
US 2023253559 A1Nickel-manganese composite hydroxide, method for producing the same, positive electrode active material for nonaqueous electrolyte secondary battery, method for producing the same, and nonaqueous electrolyte secondary battery—0
CN 104,157,872 ALow-cost high-capacity multiple-type nickel-manganese precursor, preparation method thereof and cathode material—2
CN 104,157,873 AMethod for preparing modified lithium iron phosphate by using polymerization reaction—6
CN 112,777,647 AHigh-nickel hydroxide with narrow particle size distribution and preparation method thereof—23
EP 1,189,296 A2Lithiated oxide materials and methods of manufacture—74
EP 3,023,391 A1Nickel-manganese-based composite oxyhydroxide, production method therefor, and use therefor—2
JP 2013180917 ANickel-containing hydroxide and method for producing the same—6
JP 2014510004 A遷移金属水酸化物を製造するための方法—4
GB 201,620,283 D0System for monitoring seeds and methods therof—0
JP 2017178701 AMethod for producing nickel-manganese composite oxyhydroxide—7
WO 2012/095381 A2Method for producing transition metal hydroxides—15
WO 2013/117508 A1Method for producing mixed carbonates which can contain hydroxide(s)—6
WO 2020/094482 A1Process for making a nickel composite hydroxide—5

Non-Patent Literature (1)

  • International Search Report and Written Opinion for corresponding PCT/EP2021/075441 mailed Oct. 12, 2021; 9 pages.