Methods of manufacturing of molybdenum and molybdenum-based structures by electron beam additive manufacturing, particularly structures for nuclear components
Abstract
Methodologies and manufacturing processes to manufacture components by electron beam melting additive manufacturing, particularly components of molybdenum or a molybdenum-based alloy and particularly of complex nuclear component geometries. Input parameters are provided for controlling electron beam melting additive manufacturing equipment, such as electron beam melting machines. The input parameters relate to various process steps, including build set-up, initial thermal treatment, initial layering of powder, pre-consolidation thermal treatment, consolidation, post-consolidation thermal treatment, indexing of layers, and post-build thermal treatment. The methodologies and manufacturing processes allow manufacture of components of molybdenum having a purity of ≥ 99.0% and a density of ≥ 99.75%. Metallographic cross-sections of the manufactured molybdenum components were porosity-free and crack-free.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
A method to manufacture a component by electron beam melting additive manufacturing, the method comprising: a build set-up step including seating a start plate on a powder bed within a reaction zone of a vacuum chamber of an electron beam melting additive manufacturing machine, wherein the start plate has a composition consisting of molybdenum having a purity of 99.0% or higher and wherein the powder bed includes a first powder having a composition consisting of molybdenum having a purity of 99.0% or higher; an initial thermal treatment step including positioning the start plate at a plate offset distance that is based on thermal expansion of the start plate during the initial thermal treatment step, heating the start plate to a first temperature that is sufficient to sinter the powder bed and is equal to or greater than 1040 ° C. and equal to or less than 1350 ° C., holding the start plate at the first temperature, and sintering a portion of the powder bed on which the start plate is
- Claim 2Depends on #1
The method according to claim 1, further comprising, after the consolidation step and before the post-build step: a post-consolidation step including returning the powder bed to the second preheat temperature.
- Claim 3Depends on #2
The method according to claim 2, further comprising, after the post-consolidation step and before the post-build step: an indexing step including moving a position of the start plate by a distance corresponding to thickness of a subsequent layer; a replenishment step in which the current layer of the component is covered with a layer of the first powder; and performing the pre-consolidation step and the consolidation step.
- Claim 4Depends on #3
The method according to claim 3, wherein the post-consolidation step, the indexing step, the replenishment step, the pre-consolidation step, and the consolidation step are repeated a plurality of times until the component is in a final form.
- Claim 5Depends on #1
The method according to claim 1, wherein the plate offset distance is equal to or greater than 0.1 mm and equal to or less than 0.3 mm.
- Claim 6Depends on #5
The method according to claim 5, wherein an area of the densified portion of the agglomerated first powder has a boundary enclosing an area in which the layer of the component is to be formed, wherein the component has a composition consisting of molybdenum having a purity of equal to or greater than 99.0% and a density of equal to or greater than 99.75%, and wherein the component is crack-free and porosity-free.
- Claim 7Depends on #1
The method according to claim 1, wherein an area of the densified portion of the agglomerated first powder has a boundary enclosing an area in which the layer of the component is to be formed.
- Claim 8Depends on #1
The method according to claim 1, wherein the cool-down step includes: removing heat input to the component; and (a) maintaining a vacuum atmosphere in the vacuum chamber for 20 ± 2 minutes followed by backfilling the vacuum chamber with an inert gas to atmospheric pressure or (b) cooling the component to 100 ° C. under an inert gas.
Technical Overview & Description
RELATED APPLICATION DATA This application is based on and claims priority under 35 U.S.C. § 119 to U.S. Provisional Application No. 63/226,099, filed Jul. 27, 2021, the entire contents of which are incorporated herein by reference. STATEMENT REGARDING FEDERALLY SPONSORED RESEARCH OR DEVELOPMENT The invention was made with government support under DOE Cooperative Agreement Number DE-NE0008744 awarded by the Department of Energy and under CRADA No. NFE-19-07627 between BWXT Nuclear Energy, Inc. and UT-Battelle, LLC, management and operating contractor for the Oak Ridge National Laboratory for the U.S. Department of Energy. The Government has certain rights in this invention. TECHNICAL FIELD AND INDUSTRIAL APPLICABILITY The present disclosure relates generally to methods of manufacturing by electron beam additive manufacturing. In particular, methods of manufacturing pure molybdenum and molybdenum-based structures, including structures for nuclear components, by electron beam additive manufacturing are disclosed. BACKGROUND In the discussion that follows, reference is made to certain structures and/or methods. However, the following references should not be construed as an admission that these structures and/or methods constitute prior art. Applicant expressly reserves the right to demonstrate that such structures and/or methods do not qualify as prior art against the present invention. Advanced reactor concepts, such as the GEN IV Very High Temperature Reactor (VHTR) and the GEN IV Ultra High Temperature Reactor (UHTR), continue to be investigated. Advanced manufacturing processes are being investigated to support such advanced reactor concepts. For example, one advanced manufacturing process of interest is additive manufacturing using electron beam melting technologies. Of particular interest is advanced manufacturing processes for complex nuclear component geometries. Additionally, in nuclear applications, manufacture of nuclear components having compositions that a
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (6)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- “
- Additive Manufacturing of Tungsten via Selective Laser Melting and Electron Beam Melting
- ”
- , Jonathan Wright, Jan. 8, 2020 (Year: 2020).
- Wright, Jonathan, Additive Manufacturing of Tungsten via Selective Laser Melting and Electron Beam Melting, The University of Shelfield, Jan. 8, 2020 (Year: 2020).
- K
- ö
- rner,
- “
- Additive manufacturing of metallic components by selective electron beam melting