Chloramine and chlorine removal material and methods for making the same
Abstract
Sorbent materials are described that have enhanced performance in removing chlorine and chloramine, among other toxic compounds. The sorbent materials are formed by a process which includes steps of oxidation, adding a nitrogen-containing compound, and calcining the sorbent. The processes of forming the sorbent materials are also disclosed. The sorbent materials have excellent performance as measured by a chloramine and/or chlorine destruction number, and the sorbents retain a high nitrogen edge concentration. The sorbent materials may also be incorporated into devices such as filter assemblies.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 0.
Claims (32 — 2 Independent, 30 Dependent)
- Claim 1Independent Claim
A method for making a sorbent, comprising: providing a first sorbent feedstock which has not been exposed to a nitrogen containing precursor and selected from the group consisting of activated carbon, reactivated carbon, and a combination thereof, oxidizing the first sorbent feedstock at a temperature of about 400 ° C. to about 900 ° C. to form an oxidized sorbent feedstock, adding a nitrogen containing precursor to the oxidized sorbent feedstock in an amount of about 1 mole of nitrogen per 10 moles of carbon, wherein the nitrogen containing precursor is a reduced nitrogen compound, and heating the oxidized sorbent feedstock to a temperature of at least about 400 ° C. under an inert atmosphere to form a calcined sorbent feedstock, wherein the first sorbent feedstock, oxidized sorbent feedstock, and calcined sorbent feedstock are not subsequently activated with one or more of H 2 O, CO 2, or O 2, wherein the sorbent has a chloramine destruction number (CDN) of at least about 4.0, wherein the CDN is the absolute value of the first order linear kinetic fit, multiplied by 1000, that is applied to natural log of a concentration of chloramine in water versus time, and wherein the initial concentration of chloramine is decreased over a period of 150 minutes.
- Claim 2Depends on #1
The method of claim 1, wherein the nitrogen containing precursor has an oxidation state of − 3.
- Claim 3Depends on #2
The method of claim 2, wherein the nitrogen containing precursor is selected from the group consisting of ammonia, ammonium salts, ammonium carbonate and bicarbonate, ammonium thiocyanate, azodicarbonamide, diammonium phosphate, dicyandiamide, guanidine hydrochloride, guanidine thiocyanate, guanine, melamine, thiourea, urea, and combinations thereof.
- Claim 4Depends on #1
The method of claim 1, wherein heating the oxidized sorbent feedstock comprises heating the oxidized sorbent feedstock to a temperature of at least about 700 ° C.
- Claim 5Depends on #1
The method of claim 1, wherein the first sorbent feedstock is activated carbon and the activated carbon is formed from bituminous coal, sub-bituminous coal, lignite coal, anthracite coal, peat, nut shells, pits, coconut shell, babassu nut, macadamia nut, dende nut, peach pit, cherry pit, olive pit, walnut shell, wood, lignin, polymers, nitrogen-containing polymers, resins, petroleum pitches, rice hulls, bagasse, corn stalks, wheat hulls, graphenes, carbon nanotubes, or any combination thereof.
- Claim 6Depends on #1
The method of claim 1, wherein the steps of oxidizing, adding a nitrogen containing precursor, and heating are each individually performed from one to six (1-6) times.
- Claim 7Depends on #1
The method of claim 1, wherein the first sorbent feedstock has a mean particle diameter of about 1 μ m to about 4 mm.
- Claim 8Depends on #1
The method of claim 1, wherein the CDN is at least about 10.0.
- Claim 9Depends on #1
The method of claim 1, wherein the CDN is in a range of about 10.0 to about 30.0.
- Claim 10Depends on #1
The method of claim 1, wherein the CDN is based on the destruction of monochloramine.
- Claim 11Depends on #1
The method of claim 1, wherein the sorbent has a chlorine destruction number (Cl-DN) of at least about 80.0, wherein the Cl-DN is the absolute value of the first order linear kinetic fit, multiplied by 1000, that is applied to natural log of a concentration of chlorine in water versus time, wherein the initial concentration of chlorine is decreased over a period of 150 minutes.
- Claim 12Depends on #11
The method of claim 11, wherein the Cl-DN is in a range of about 80.0 to about 100.0.
- Claim 13Depends on #1
The method of claim 1, wherein the sorbent has a nitrogen edge concentration of at least about 0.20 atom %.
- Claim 14Depends on #13
The method of claim 13, wherein the sorbent has a nitrogen edge concentration of about 0.20 atom % to about 1.2 atom %.
- Claim 15Depends on #1
The method of claim 1, wherein oxidizing the first sorbent feedstock comprises oxidizing the first sorbent feedstock in a dry atmosphere.
- Claim 16Depends on #1
The method of claim 1, wherein oxidizing the first sorbent feedstock comprises oxidizing the first sorbent feedstock in a humidified atmosphere.
- Claim 17Depends on #1
The method of claim 1, wherein the steps of providing, oxidizing, adding, and heating are performed in that listed order.
- Claim 18Depends on #1
The method of claim 1, further comprising adding an untreated sorbent feedstock in the amount of about 5 wt. % to about 95 wt. % based on the total amount of the sorbent.
- Claim 19Independent Claim
A sorbent formed by a method comprising the steps of: providing a first sorbent feedstock which has not been exposed to a nitrogen containing precursor and selected from the group consisting of activated carbon, reactivated carbon, and a combination thereof, oxidizing the first sorbent feedstock at a temperature of about 400 ° C. to about 900 ° C. to form an oxidized sorbent feedstock, adding a nitrogen containing precursor to the oxidized sorbent feedstock in an amount of about 1 mole of nitrogen per 10 moles of carbon, wherein the nitrogen containing precursor is a reduced nitrogen compound, and heating the sorbent feedstock to a temperature of at least about 400 ° C. under an inert atmosphere to form a calcined sorbent feedstock, wherein the first sorbent feedstock, oxidized sorbent feedstock, and calcined sorbent feedstock are not subsequently activated with one or more of H 2 O, CO 2, or O 2, wherein the sorbent has a chloramine destruction number (CDN) of at least about 4.0, wherein the CDN is the absolute value of the first order linear kinetic fit, multiplied by 1000, that is applied to natural log of a concentration of chloramine in water versus time, and wherein the initial concentration of chloramine is decreased over a period of 150 minutes.
- Claim 20Depends on #19
The sorbent of claim 19, wherein the nitrogen containing precursor has an oxidation state of − 3.
- Claim 21Depends on #20
The sorbent of claim 20, wherein the nitrogen containing precursor is selected from the group consisting of ammonia, ammonium carbonate and bicarbonate, ammonium thiocyanate, azodicarbonamide, diammonium phosphate, dicyandiamide, guanidine hydrochloride, guanidine thiocyanate, guanine, melamine, thiourea, urea, and combinations thereof.
- Claim 22Depends on #19
The sorbent of claim 19, wherein the first sorbent feedstock has a mean particle diameter of about 1 μ m to about 4 mm.
- Claim 23Depends on #19
The sorbent of claim 19, wherein the CDN is at least about 10.0.
- Claim 24Depends on #19
The sorbent of claim 19, wherein the CDN is in a range of about 10.0 to about 30.0.
- Claim 25Depends on #19
The sorbent of claim 19, wherein the CDN is based on the destruction of monochloramine.
- Claim 26Depends on #19
The sorbent of claim 19, wherein the sorbent has a chlorine destruction number (Cl-DN) of at least about 80.0, wherein the Cl-DN is the absolute value of the first order linear kinetic fit, multiplied by 1000, that is applied to natural log of a concentration of chlorine in water versus time, wherein the initial concentration of chlorine is decreased over a period of 150 minutes.
- Claim 27Depends on #26
The sorbent of claim 26, wherein the Cl-DN is about 80.0 to about 100.0.
- Claim 28Depends on #19
The sorbent of claim 19, wherein the sorbent has a nitrogen edge concentration of at least about 0.20 atom %.
- Claim 29Depends on #28
The sorbent of claim 28, wherein the sorbent has a nitrogen edge concentration of about 0.20 atom % to about 1.2 atom %.
- Claim 30Depends on #19
The sorbent of claim 19, further comprising an untreated sorbent feedstock in the amount of about 5 wt. % to about 95 wt. % based on the total amount of the sorbent.
- Claim 31Depends on #19
A filter assembly comprising the sorbent of claim 19.
- Claim 32Depends on #19
The sorbent of claim 19, wherein the activated carbon or the reactivated carbon is formed from one or more of bituminous coal, lignite coal, anthracite coal, peat, nut shells, pits, coconut shell, babassu nut, macadamia nut, dende nut, peach pit, cherry pit, olive pit, walnut shell, wood, lignin, polymers, resins, petroleum pitches, bagasse, rice hulls, corn husks, wheat hulls and chaff, graphenes, and carbon nanotubes.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATIONS This application is a continuation of U.S. Non-Provisional application Ser. No. 15/895,410 filed on Feb. 13, 2018, now U.S. Pat. No. 10,702,853, which claims priority to U.S. Provisional Application 62/458,371 filed on Feb. 13, 2017, the entire contents of which are incorporated by reference herein. GOVERNMENT INTERESTS Not applicable PARTIES TO A JOINT RESEARCH AGREEMENT Not applicable INCORPORATION BY REFERENCE OF MATERIAL SUBMITTED ON A COMPACT DISC Not applicable BACKGROUND Sorbent materials having high surface areas and which have been chemically modified to have catalytic properties are well known for their oxidative and decomposition properties. These properties find use in a variety of fields, in particular the removal and destruction of chlorine, chloramine, trihalomethanes, haloacetic acids, and hydrogen peroxides which are formed when water is disinfected. The sorbent materials are typically formed from various activated carbons and carbonaceous chars which are thermally treated with a nitrogen containing precursor followed by activation to produce the catalytic activated carbon. Alternately, a nitrogen containing precursor can be charred and activated. Activation is normally carried out at high temperature with an activating gas such as steam (water), carbon dioxide, or oxygen. These methods are described in several U.S. Patents, including U.S. Pat. Nos. 6,342,129, 6,706,194, 5,356,849, 5,338,458, and 9,174,205, all of which are incorporated by reference in their entirety. There are disadvantages to the prior art nitrogen pretreatment and activation techniques. The activation process gasifies the surface portion of the carbonaceous char or other sorbent material, which results in small pores being formed as the carbon or other material on the surface of the sorbent particles vaporizes. These pores are responsible for the high total surface area of the sorbent material, and therefore its high performance. However, t
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (47)
Non-Patent Literature (10)
- Machine Translation for JP-2009056449 (Year: 2009).
- Machine Translation for JP H1029043 (Year: 1998).
- International Search Report and Written Opinion for PCT/US2018/017973 dated May 29, 2018.
- Sharifi et al.,
- “
- Formation of Active Sites for Oxygen Reduction Reactions by Transformation of Nitrogen Functionalities in Nitrogen-Doped Carbon Nanotubes.
- ”
- ACS Nano, vol. 6, No. 10, 2012, pp. 8904-8912, doi:10.1021/nn302906r.
- “
- The Chemistry of Nitrogen and Phosphorous.