hottub.patents
US 12,550,643 B2#3319757 Most CitedActiveUnited States (USPTO)Utility

Oxidants and strained-ring precursors

0Forward Citations (#3319757 Global)
0.0/yrCitation Velocity (#3319757 Global)
0.00Citation PageRank (#3319757 Global)
60Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

Novel cyclic silicon precursors and oxidants are described. Methods for depositing silicon-containing films on a substrate are described. The substrate is exposed to a silicon precursor and a reactant to form the silicon-containing film (e.g., elemental silicon, silicon oxide, silicon nitride). The exposures can be sequential or simultaneous.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 60 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method of depositing a silicon-containing material on a semiconductor substrate, the method comprising exposing the semiconductor substrate to a cyclic silicon precursor and a reactant, the cyclic silicon precursor includes a 3- or 4-membered ring containing silicon, wherein the cyclic silicon precursor has a general formula of: where X and Y are independently selected from SiH2, NH, S, or Se, wherein at least one of X or Y is S, and R1, R2, R3, and R4 are independently selected from an alkyl group.

  2. Claim 2Depends on #1

    The method of claim 1, wherein the silicon-containing material comprises silicon nitride and the reactant is selected from the group consisting of hydrazine, alkyl hydrazine, allyl hydrazine, hydrogen (H2), ammonia (NH 3), R ′ NH 2, R ′ 2 NH, R ′ 3 N, R ′ 2 SINH 2, (R ′ sSi) 2 NH, and (R ′ 3 Si) 3 N, where each R ′ is independently H or an alkyl group having 1-12 carbon atoms.

  3. Claim 3Depends on #1

    The method of claim 1, wherein the silicon-containing material comprises silicon nitride comprising a nitrogen containing content in a range of from 1% to 40% on an atomic basis.

  4. Claim 4Depends on #1

    The method of claim 1, wherein the cyclic silicon precursor comprises

  5. Claim 5Depends on #1

    The method of claim 1, wherein the silicon-containing material comprises silicon oxide, and the reactant is selected from the group consisting of an oxaziridine and a P/S/N oxide.

  6. Claim 6Depends on #5

    The method of claim 5, wherein the reactant is an oxaziridine.

  7. Claim 7Depends on #6

    The method of claim 6, wherein the silicon oxide film comprises greater than 98 atomic % of silicon and oxygen atoms.

  8. Claim 8Depends on #6

    The method of claim 6, wherein the oxaziridine comprises a compound with a general formula of: where R 1, R 2 and R 3 are independently selected from H, SO 2 NO 2, CN, C1-C8 alkyl, C1-C8 perfluoroalkyl, pyridine, aryl, substituted aryl, perfluoroaryl, SO 2 -NO 2 substituted aryl, or R 2 and R 3 are combined to form a carbonyl.

Technical Overview & Description

TECHNICAL FIELD Embodiments of the disclosure relate to silicon precursors, oxidants and methods for depositing silicon-containing films. More particularly, embodiments of the disclosure are directed to strained-ring silicon precursors, oxaziridine oxidants, P/S/N oxides, and methods of use thereof. BACKGROUND The semiconductor processing industry continues to strive for larger production yields while increasing the uniformity of layers deposited on substrates having larger surface areas. These same factors in combination with new materials also provide higher integration of circuits per unit area of the substrate. As circuit integration increases, the need for greater uniformity and process control regarding layer thickness rises. As a result, various technologies have been developed to deposit layers on substrates in a cost-effective manner, while maintaining control over the characteristics of the layer. Chemical vapor deposition (CVD) is one of the most common deposition processes employed for depositing layers on a substrate. CVD is a flux-dependent deposition technique that requires precise control of the substrate temperature and the precursors introduced into the processing chamber in order to produce a desired layer of uniform thickness. These requirements become more critical as substrate size increases, creating a need for more complexity in chamber design and gas flow technique to maintain adequate uniformity. A variant of CVD that demonstrates excellent step coverage is cyclical deposition or atomic layer deposition (ALD). Cyclical deposition is based upon atomic layer epitaxy (ALE) and employs chemisorption techniques to deliver precursor molecules on a substrate surface in sequential cycles. The cycle exposes the substrate surface to a first precursor, a purge gas, a second precursor and the purge gas. The first and second precursors react to form a product compound as a film on the substrate surface. The cycle is repeated to form the layer to a desir

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • PCT International Search Report and Written Opinion in PCT/US2022/034513 dated Dec. 2, 2022, 13 pages.
  • Wrobel, A. M., et al.,
  • “
  • Mechanism of the Activation of 1,1,3,3-Tetramethyl-1,3-disilacyclobutane in Plasma Chemical Vapor Deposition
  • ”
  • , Chem. Mater., 1994, vol. 6, No. 10, pp. 1766-1770 abstract; pp. 1766-1767, experimental section; table 1; figure 1.
  • Ustynyuk, et al.,
  • “
  • Heteroorganic betaines. 6. Structure and reactivity of silicon-containing organophosphorus betaines with the -S
  • —