Patents
US 12,540,366 B2#156018163 Most CitedActiveUnited States (USPTO)Utility

Heat treatment of high strength cold rolled steel strip

0Forward Citations (#156018163 Global)
0.0/yrCitation Velocity (#156018163 Global)
0.00Citation PageRank (#156018163 Global)
79Prior Art Cited
15Claims (3 Indep. · 12 Dep.)
2Drawings / Sheets

Abstract

A heat treatment of a high strength cold rolled steel strip includes the steps of a) soaking a cold rolled steel strip, b) cooling the soaked steel strip c) heat treating the cooled strip; d) cooling the heat treated steel strip to ambient temperature range; such that the steel strip has a microstructure including various ferrites, retained austenite and martensite. The main components in the steel composition include carbon, manganese, silicon and aluminium in addition to iron.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 79 · Forward citations: 0.

Claims (15 — 3 Independent, 12 Dependent)

  1. Claim 1Independent Claim

    A method of heat treating a cold rolled steel strip, which method comprises the steps of: prior to step a), heating an uncoated cold rolled steel strip from a first temperature, wherein first temperature is room temperature, to a temperature T 1 in the range of 680-740 ° C. at a single constant heating rate V 1 of 15.0-25.0 ° C./s; and further heating the uncoated cold rolled steel strip from the temperature T 1 to a soaking temperature T 2 within a soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) at a heating rate V 2 of 0.5-4.0 ° C./s; a) soaking the uncoated cold rolled steel strip at the soaking temperature T 2 within the soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) for a soaking time t 2 of 1-100 seconds, thereby obtaining a cold rolled steel strip having an at least partially austenitic microstructure; b) cooling the uncoated soaked steel strip resulting from step a) to a temperature T 4 in the range of Bn-Ms, wherein acicular ferrite is formed during the cooling in a temperature range between Bs and Ms, wherein step b) comprises a substep of cooling the soaked steel strip from step a) to a temperature T 3 in the range of 750-550 ° C. at a cooling rate V 3 of 2.0 ° C./s to 15 ° C./s; and wherein step b) comprises a substep of cooling the soaked steel strip from a temperature T 3, to T 4 at a cooling rate V 4 of 20.0-60.0 ° C./s; c) heat treating the uncoated cooled strip obtained in step b) in a range between the temperature Bn-(Ms+50) for a period of time t 5 of 40-120 seconds, by heating to increase temperature from T 4 to a temperature T 5 between T 4 and Bs; c1) optionally a coating step of coating the heat treated steel strip with a protective coating following the heat treating of step c), d) cooling the heat treated, optionally coated, steel strip to a temperature T 7 in the range of ((Ms − 50) to Mf) at a cooling rate of V 7 of 5.0-10.0 ° C./s and further cooling the heat treated, optionally coated, steel strip to ambient temperature at a cooling rate of V 8 of 5.0-20.0 ° C./s; such that the heat treated, optionally coated, steel strip has a microstructure (in vol. %) comprising: polygonal ferrite (PF)+acicular ferrite (AF)+carbide-free higher bainitic ferrite (HBF): 25-55; polygonal ferrite (PF): 0-45; carbide-free lower bainitic ferrite (LBF): 30-65; retained austenite (RA): 5-20; fresh martensite (M): 0-20; wherein the steel strip has a composition (in mass %) comprising: C: 0.15-0.35; Mn: 1.50-3.00; Si: 0.50-2.00; Al: 0.01-1.50; P: less than 0.050; S: less than 0.020; N: less than 0.0080; wherein the sum (Si+Al) is ≥ 0.60; and optionally one or more elements selected from 0 < Cr ≤ 0.35; 0 < Cu ≤ 0.20; 0 < Ni ≤ 0.50; 0 < Mo ≤ 0.30; 0 < Nb ≤ 0.10; 0 < V ≤ 0.10; 0 < Ti ≤ 0.10; 0 < B ≤ 0.0030; 0 < Ca ≤ 0.0050; 0 < REM ≤ 0.0100, wherein REM is one or more rare earth metals; and the remainder being iron and inevitable impurities, wherein the steel strip resulting from step d) has Tensile strength (TS) ≥ 850 MPa; and wherein the steel strip resulting from step d) has: Yield strength (YS) ≥ 500 MPa; and Total elongation (TE) ≥ 14%.

  2. Claim 2Depends on #1

    The method according to claim 1, wherein step a) comprises soaking a cold rolled steel strip within a temperature range of (Ac3 − 50 ° C.)-(Ac3+10 ° C.).

  3. Claim 3Depends on #1

    The method according to claim 1, wherein step b) comprises cooling the soaked steel strip from step a) to the temperature T 4 at a cooling rate sufficient to avoid pearlite formation.

  4. Claim 4Depends on #1

    The method according to claim 1, wherein the soaking temperature is (Ac3 − 50 ° C.)-(Ac3+10 ° C.).

  5. Claim 5Depends on #1

    The method according to claim 1, wherein step c) is performed at least partially by latent heat produced by the bainite transformation.

  6. Claim 6Depends on #1

    The method according to claim 1, comprising a further heat treatment step between steps c) and d) or if step c1) is present between steps c) and c1), wherein the uncoated steel strip resulting from step c) undergoes heating to a temperature T 6 in the range of Bs-Bn for a period of time t 6.

  7. Claim 7Depends on #1

    The method according to claim 1, wherein the step c1) is performed and comprises a hot dip galvanizing treatment and comprises a further heat treatment step wherein the steel strip resulting from step c) undergoes heating to a temperature T 6 in the range of Bs-Bn for a period of time t 6.

  8. Claim 8Depends on #1

    The method according to claim 1, wherein the step c1) is performed.

  9. Claim 9Depends on #1

    The method according to claim 1, wherein the microstructure comprises in vol. %: polygonal ferrite (PF)+acicular ferrite (AF)+carbide-free higher bainitic ferrite (HBF): 25-50; polygonal ferrite (PF): 10-40; carbide-free lower bainitic ferrite (LBF): 30-60; retained austenite (RA): 7-15; fresh martensite (M): 0-15; and/or wherein the C content in retained austenite (RA) is 0.90 wt. % or more.

  10. Claim 10Depends on #1

    The method according to claim 1, wherein carbide free bainitic ferrite is formed when the temperature in step b is in a range between Bs and Ms, wherein carbide free high bainitic ferrite is formed when the temperature in step b is in a range between Bs and Bn, wherein carbide free low bainitic ferrite is formed when the temperature in step b is in a range between Bn and Ms.

  11. Claim 11Depends on #1

    The method according to claim 1, wherein the heat treated, optionally coated, steel strip has: at least 11% PF.

  12. Claim 12Depends on #1

    The method according to claim 1, wherein the heat treated, optionally coated, steel strip has: 0.01-0.321% Al; at least 1.17% Si; and AF is present.

  13. Claim 13Depends on #1

    A heat treated cold rolled steel strip made by the method of claim 1 and having a composition (in mass %) comprising C: 0.15-0.35; Mn: 1.50-3.00; Si: 0.50-2.00; Al: 0.01-1.50; P: less than 0.050; S: less than 0.020; N: less than 0.0080; wherein the sum (Si+Al) is ≥ 0.60; and optionally one or more elements selected from 0 < Cr ≤ 0.35; 0 < Cu ≤ 0.20; 0 < Ni ≤ 0.50; 0 < Mo ≤ 0.30; 0 < Nb ≤ 0.10; 0 < V ≤ 0.10; 0 < Ti ≤ 0.10; 0 < B ≤ 0.0030; 0 < Ca ≤ 0.0050; 0 < REM ≤ 0.0100, wherein REM is one or more rare earth metals; and the remainder being iron and inevitable impurities; and a microstructure (in vol. %) comprising polygonal ferrite (PF)+acicular ferrite (AF)+higher bainitic ferrite (HBF): 20-55; polygonal ferrite (PF): 0-45; lower bainitic ferrite (LBF): 20-65; retained austenite (RA): 5-20; fresh martensite (M): 0-20; wherein the steel strip resulting from step d) has Tensile strength (TS) ≥ 850 MPa; and wherein the steel strip resulting from step d) has: Yield strength (YS) ≥ 500 MPa; and Total elongation (TE) ≥ 14%.

  14. Claim 14Independent Claim

    A method of heat treating a cold rolled steel strip, which method comprises the steps of: prior to step a) heating an uncoated cold rolled steel strip from room temperature to a temperature T 1 in the range of 680-740 ° C. at a single constant heating rate V 1 of 15.0-25.0 ° C./s; and further heating the uncoated cold rolled steel strip from the temperature T 1 to a soaking temperature T 2 within a soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) at a heating rate V 2 of 0.5-4.0 ° C./s; a) soaking the uncoated cold rolled steel strip at the soaking temperature T 2 within the soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) for a soaking time t 2 of 1-100 seconds, thereby obtaining a cold rolled steel strip having an at least partially austenitic microstructure; b) cooling the uncoated soaked steel strip resulting from step a) to a temperature T 4 in the range of Bn-Ms, wherein acicular ferrite is formed during the cooling in a temperature range between Bs and Ms; wherein step b) comprises a substep of cooling the soaked steel strip from step a) to a temperature T 3 in the range of 750-550 ° C. at a cooling rate V 3 of 2.0 ° C./s to 15 ° C./s; and wherein step b) comprises a substep of cooling the soaked steel strip from a temperature T 3, to T 4 at a cooling rate V 4 of 20.0-60.0 ° C./s; c) heat treating the uncoated cooled strip obtained in step b) in a range between the temperature Bn-(Ms+50) for a period of time t 5 of 40-120 seconds, by heating to increase temperature from T 4 to a temperature T 5 between T 4 and Bs; c1) optionally a coating step of coating the heat treated steel strip with a protective coating following the heat treating of step c), d) cooling the heat treated, optionally coated, steel strip to a temperature T 7 in the range of ((Ms − 50) to Mf) at a cooling rate of V 7 of 5.0-10.0 ° C./s and further cooling the heat treated, optionally coated, steel strip to ambient temperature at a cooling rate of V 8 of 5.0-20.0 ° C./s; such that the heat treated, optionally coated, steel strip has a microstructure (in vol. %) consisting of: polygonal ferrite (PF)+acicular ferrite (AF)+carbide-free higher bainitic ferrite (HBF): 25-55; polygonal ferrite (PF): 0-45; carbide-free lower bainitic ferrite (LBF): 30-65; retained austenite (RA): 5-20; fresh martensite (M): 0-20; cementite+pearlite: less than 5; wherein the steel strip has a composition (in mass %) comprising: C: 0.15-0.35; Mn: 1.50-3.00; Si: 0.50-2.00; Al 0.01-1.50; P: less than 0.050; S: less than 0.020; N: less than 0.0080; wherein the sum (Si+Al) is ≥ 0.60; and optionally one or more elements selected from 0 < Cr ≤ 0.35; 0 < Cu ≤ 0.20; 0 < Ni ≤ 0.50; 0 < Mo ≤ 0.30; 0 < Nb ≤ 0.10; 0 < V ≤ 0.10; 0 < Ti ≤ 0.10; 0 < B ≤ 0.0030; 0 < Ca ≤ 0.0050; 0 < REM ≤ 0.0100, wherein REM is one or more rare earth metals; and the remainder being iron and inevitable impurities, wherein the steel strip resulting from step d) has Tensile strength (TS) ≥ 850 MPa; and wherein the steel strip resulting from step d) has: Yield strength (YS) ≥ 500 MPa; and Total elongation (TE) ≥ 14%.

  15. Claim 15Independent Claim

    A method of heat treating a cold rolled steel strip, which method comprises the steps of: prior to step a), heating an uncoated cold rolled steel strip from room temperature to a temperature T 1 in the range of 680-740 ° C. at a single constant heating rate V 1 of 15.0-30.0 ° C./s; and further heating the uncoated cold rolled steel strip from the temperature T 1 to a soaking temperature T 2 within a soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) at a heating rate V 2 of 0.5-4.0 ° C./s; a) soaking the uncoated cold rolled steel strip at the soaking temperature T 2 within the soaking temperature range of (Ac3 − 60 ° C.) to (Ac3+20 ° C.) for a soaking time t 2 of 1-86 seconds, thereby obtaining a cold rolled steel strip having an at least partially austenitic microstructure; b) cooling the uncoated soaked steel strip resulting from step a) to a temperature T 4 in the range of Bn-Ms, wherein acicular ferrite is formed during the cooling at a temperature between Bs and Ms, wherein step b) comprises a substep of cooling the soaked steel strip from step a) to a temperature T 3 in the range of 750-550 ° C. at a cooling rate V 3 of 2.0 ° C./s to 15 ° C./s; and wherein step b) comprises a substep of cooling the soaked steel strip from a temperature T 3 in the range of 750-550 ° C., to T 4 at a cooling rate V 4 of 20.0-60.0 ° C./s; c) heat treating the uncoated cooled strip obtained in step b) at a temperature between Bn-(Ms+50) for a period of time t 5 of 40-120 seconds, by heating to increase temperature from T 4 to a temperature T 5 between T 4 and Bs; c1) optionally a coating step of coating the heat treated steel strip with a protective coating following the heat treating of step c), d) cooling the heat treated, optionally coated, steel strip to a temperature T 7 in the range of ((Ms − 50) to Mf) at a cooling rate of V 7 of 5.0-10.0 ° C./s and further cooling the heat treated, optionally coated, steel strip to ambient temperature at a cooling rate of V 8 of 5.0-20.0 ° C./s; such that the heat treated, optionally coated, steel strip has a microstructure (in vol. %) comprising: polygonal ferrite (PF)+acicular ferrite (AF)+higher bainitic ferrite (HBF): 25-55; polygonal ferrite (PF): 0-45; lower bainitic ferrite (LBF): 30-65; retained austenite (RA): 5-20; fresh martensite (M): 0-20; wherein the steel strip has a composition (in mass %) comprising C: 0.15-0.35; Mn: 1.50-3.00; Si: 0.50-2.00; Al: 0.01-1.50; P: less than 0.050; S: less than 0.020; N: less than 0.0080; wherein the sum (Si+Al) is ≥ 0.60; and optionally one or more elements selected from 0 < Cr ≤ 0.35; 0 < Cu ≤ 0.20; 0 < Ni ≤ 0.50; 0 < Mo ≤ 0.30; 0 < Nb ≤ 0.10; 0 < V ≤ 0.10; 0 < Ti ≤ 0.10; 0 < B ≤ 0.0030; 0 < Ca ≤ 0.0050; 0 < REM ≤ 0.0100, wherein REM is one or more rare earth metals; and the remainder being iron and inevitable impurities, wherein the steel strip resulting from step d) has Tensile strength (TS) ≥ 850 MPa; and wherein the steel strip resulting from step d) has at least one of the properties: Yield strength (YS) ≥ 500 MPa; and Total elongation (TE) ≥ 14%.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This is a § 371 National Stage Application of International Application No. PCT/EP2020/066212 filed on Jun. 11, 2020, claiming the priority of European Patent Application No. 19180701.5 filed on Jun. 17, 2019. FIELD OF THE INVENTION The present invention relates to a method of heat treating a high strength cold rolled steel strip. BACKGROUND OF THE INVENTION In the art various types of cold rolled steels and manufacturing processes have been proposed for meeting the requirements in automotive applications. E.g. extra low carbon steel is used in automotive steel strip in view of its formability. This steel type shows a tensile strength in the range of 280-380 MPa. HSLA (high strength low alloy) steels contain microalloying elements. They are hardened by a combination of precipitation and grain refining. Advanced high strength steels (AHSS), such as dual phase (DP) steels and transformation induced plasticity (TRIP) steels, are currently typical of high-ductility, high-strength steels that are used in the automotive manufacturing industry. In DP steels the presence of martensite within a ferrite matrix enables a tensile strength higher than 450 MPa combined with good cold formability to be obtained. To achieve simultaneously a high yield strength/tensile strength ratio and an even higher tensile strength, i.e., above 800 MPa, steels having complex (CP) microstructures including ferrite, bainite, martensite and/or retained austenite have been developed. However, due to the difference of the deformation capabilities between the ferrite, bainite or martensite structures and the retained austenite structure, these steels are generally inferior in stretch flange formability. Therefore their use is limited to automobile parts which do not require high formability. TRIP type tempered martensitic steel (Q & P steel through quench and partitioning) that consists of tempered martensite as the matrix phase and residual austenite, and TRIP

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (79)

PatentTitleYearCitations
US 9,650,708 B2High-strength flat steel product and method for producing same20177
US 2010108200 A1High yield ratio and high-strength hot-dip galvanized steel sheet excellent in workability and production method thereof—29
US 2011146852 A1High strength steel sheet and method for manufacturing the same—76
US 2011162762 A1High strength steel sheet and method for manufacturing the same—31
US 2011198002 A1High-strength galvanized steel sheet with excellent formability and method for manufacturing the same—54
US 2014242415 A1HIGH-STRENGTH HOT-DIP GALVANIZED STEEL SHEET AND HIGH-STRENGTH ALLOYED HOT-DIP GALVANIZED STEEL SHEET HAVING EXCELLENT FORMABILITY AND SMALL MATERIAL ANISOTROPY WITH ULTIMATE TENSILE STRENGTH OF 980 MPa OR MORE AND MANUFACTURING METHOD THEREFOR—29
US 2014305553 A1High-strength cold-rolled steel sheet having small variations in strength and ductility and manufacturing method for the same—12
US 2014322559 A1High-Strength Flat Steel Product and Method for Producing Same—43
US 2015101712 A1Method for manufacturing high-strength cold-rolled steel sheet with outstanding workability—26
US 2015167133 A1High strength cold rolled steel sheet and method of producing such steel sheet—13
US 2015184274 A1High-strength hot-dip galvanized steel sheet having excellent yield strength and formability, and manufacturing method therefor—12
US 2016208359 A1High-strength steel sheet having excellent ductility and low-temperature toughness, and method for producing same—11
US 2016237520 A1High-strength steel sheet having excellent formability and low-temperature toughness, and method for producing same—13
US 2017130292 A1Method for Producing a High Strength Steel Sheet having Improved Strength, Ductility and Formability—13
US 2017137910 A1Method for Producing an Ultra High Strength Coated or Not Coated Steel Sheet and Obtained Sheet—7
US 2017191150 A1Steel strip having high strength and high formability, the steel strip having a hot dip zinc based coating—19
US 2018010207 A1High-strength plated steel sheet and method for producing same—18
US 2019040482 A1High-strength steel sheet and method for manufacturing the same—5
US 2019040483 A1High-strength steel sheet and method for producing the same—4
US 2019338388 A1Tempered and coated steel sheet having excellent formability and a method of manufacturing the same—5
US 2020040420 A1High-strength steel sheet and method for producing the same—7
US 2020190612 A1High strength cold-rolled steel sheet having excellent yield strength, ductility, and hole expandability, hot-dip galvanized steel sheet, and method for producing same—8
US 2020283869 A1High-strength cold-rolled steel sheet—3
US 2021262069 A1Flat Steel and Method for Producing Same—1
US 2022205058 A1A high strength steel product and a process to produce a high strength steel product—3
US 2022316021 A1Method of heat treating a cold rolled steel strip—1
US 2022316024 A1Heat treatment of cold rolled steel strip—0
US 2022316026 A1Method of heat treating a high strength cold rolled steel strip—0
CN 108,603,271 AHigh-strength steel sheet and its manufacturing method—14
CN 108,699,660 AHigh-strength steel sheet and method for producing same—5

Non-Patent Literature (10)

  • International Search Report and Written Opinion mailed Oct. 21, 2020 for PCT/EP2020/066207 to Tata Steel Ijmuiden B.V. filed Jun. 11, 2020.
  • International Search Report and Written Opinion mailed Oct. 21, 2020 for PCT/EP2020/066208 to Tata Steel Ijmuiden B.V. filed Jun. 11, 2020.
  • International Search Report and Written Opinion mailed Oct. 9, 2020 for PCT/EP2020/066212 to Tata Steel Ijmuiden B.V. filed Jun. 11, 2020.
  • International Search Report and Written Opinion mailed Oct. 21, 2020 for PCT/EP2020/066216 to Tata Steel Ijmuiden B.V. filed Jun. 11, 2020.
  • A.-F. Gourguesh. M. Flowert. C. Lindley, Materials Science and Technology, vol. 16, Jan. 2000 (Jan. 1, 2000), pp. 26-40.
  • Notification of Reason for Rejection mailed Jul. 2, 2024 for Japanese Patent Application No. 2021-575076, filed Jun. 11, 2020.
  • Notification of Reason for Rejection mailed Jul. 2, 2024 in Japanese Patent Application No. 2021-575078 (Translation of Official Action).
  • Guhui Gao et al:
  • “
  • A carbide-free bainite/martensite/austenite triplex steel with enhanced mechanical properties treated by a novel quenching-partitioning-tempering process