Patents
US 12,534,780 B2#156023455 Most CitedActiveUnited States (USPTO)Utility

Macro-chip reinforced alloy

0Forward Citations (#156023455 Global)
0.0/yrCitation Velocity (#156023455 Global)
0.00Citation PageRank (#156023455 Global)
12Prior Art Cited
20Claims (2 Indep. · 18 Dep.)
1Drawings / Sheets

Abstract

Described herein are methods of forming a neutron shielding material. Such material may comprise a powder blend comprising a first component comprising a blend of a first metal particle and a first ceramic particle; and a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (20 — 2 Independent, 18 Dependent)

  1. Claim 1Independent Claim

    A powder blend comprising: a first component comprising a blend of a first metal particle and a first ceramic particle; and a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix; wherein the first ceramic particle and the first metal particle are present in a weight ratio ranging from about 1:15 to about 1:7.

  2. Claim 2Depends on #1

    The powder blend according to claim 1, wherein the first component and the second component are present in a weight ratio ranging from about 100:1 to about 2:1.

  3. Claim 3Depends on #1

    The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are formed from the same material.

  4. Claim 4Depends on #1

    The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are formed from different materials.

  5. Claim 5Depends on #1

    The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle are each independently selected from the group consisting of alumina, titanium carbide, silicon carbide, tungsten carbide, boron carbide, and mixtures thereof.

  6. Claim 6Depends on #1

    The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are formed from the same material.

  7. Claim 7Depends on #1

    The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are formed from different materials.

  8. Claim 8Depends on #1

    The powder blend according to claim 1, wherein the first metal particle and the chip metal matrix are each independently selected from the group consisting of pure aluminum, an aluminum alloy, steel, a nickel alloy, a titanium alloy, and combinations thereof.

  9. Claim 9Depends on #1

    The powder blend according to claim 1, wherein the reinforcing chip has a height to width aspect ratio ranging from about 1:3 to about 1:1.25.

  10. Claim 10Depends on #1

    The powder blend according to claim 1, wherein the reinforcing chip has a height to thickness aspect ratio ranging from about 2:1 to about 10:1.

  11. Claim 11Depends on #1

    The powder blend according to claim 1, wherein the alloy chips have a width ranging from about 2.0 mm to about 10.0 mm.

  12. Claim 12Depends on #1

    The powder blend according to claim 1, wherein the alloy chips have a thickness ranging from about 0.1 mm to about 1.0 mm.

  13. Claim 13Depends on #1

    The powder blend according to claim 1, wherein the first ceramic particle and the second ceramic particle each have a particle distribution of 100% less than about 250 μ m.

  14. Claim 14Depends on #1

    The powder blend according to claim 1, wherein the first metal particle has a d50 ranging from about 1 μ m to about 20 μ m.

  15. Claim 15Depends on #1

    The powder blend according to claim 1, wherein the first metal particle is an aluminum particle and has a natural oxide formation layer having a thickness ranging from about 3 nm to about 7 nm.

  16. Claim 16Independent Claim

    A powder blend comprising: a first component comprising a blend of a first metal particle and a first ceramic particle; and a second component comprising a reinforcing chip, the reinforcing chip comprising a second ceramic particle dispersed within a chip metal matrix; wherein the first metal particle is an aluminum particle and has a natural oxide formation layer having a thickness ranging from about 3 nm to about 7 nm.

  17. Claim 17Depends on #16

    The powder blend according to claim 16, wherein the chip metal matrix is selected from the group consisting of pure aluminum, an aluminum alloy, steel, a nickel alloy, a titanium alloy, and combinations thereof.

  18. Claim 18Depends on #16

    The powder blend according to claim 16, wherein the first component and the second component are present in a weight ratio ranging from about 100:1 to about 2:1.

  19. Claim 19Depends on #16

    The powder blend according to claim 16, wherein the first ceramic particle and the second ceramic particle are each independently selected from the group consisting of alumina, titanium carbide, silicon carbide, tungsten carbide, boron carbide, and mixtures thereof.

  20. Claim 20Depends on #16

    The powder blend according to claim 16, wherein the first metal particle has a d50 ranging from about 1 μ m to about 20 μ m.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a continuation application of U.S. patent application Ser. No. 17/084,573, filed on Oct. 29, 2020 (now U.S. Pat. No. 11,590,573), which is a divisional of U.S. patent application Ser. No. 15/061,542, filed on Mar. 4, 2016 (now U.S. Pat. No. 10,843,272), which claims the benefit of U.S. Provisional Application No. 62/128,455, filed on Mar. 4, 2015. The disclosures of the above applications are incorporated herein by reference in their entireties. BACKGROUND Composite materials comprising a metal matrix and alloying elements, such as ceramic particles, have long been used for a variety of applications, such as shielding neutron radiation in connection with nuclear reactors. However, adding a greater diversity of metal matrix materials with different types and amounts of alloying elements have creates difficulties with respect to forming grain structures that are suitable for extreme applications (i.e., high temperature, high load-bearing, etc.). Thus, while certain materials may be known to individually provide added performance benefits, there still remains a need for composites materials (and methods of their production) that can successfully incorporate such alloying and matrix materials without undermining the overall structural integrity required for the final application of the composite. BRIEF SUMMARY The present invention is directed to a method of forming a neutron shielding material comprising a) mixing together a first metal particle having a first grain growth temperature; a first ceramic particle; and a reinforcing chip to form a powder blend; and b) processing the powder blend at a hot-work temperature; wherein the reinforcing chip comprises a second ceramic particle dispersed within a chip metal matrix having a second grain growth temperature; and wherein the hot-work temperature is lower than both of the first and second grain growth temperatures. In certain embodiments, the hot-work temperatu

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (10)

  • Corresponding International Search Report and Written Opinion for PCT/US16/20976 dated Jun. 2, 2016.
  • Buyuk et al.
  • “
  • Gamma and Neutron attenuation behaviors of boron carbide-silicon-carbide composites
  • ”
  • Annals of Nuclear Energy, vol. 71 (Sep. 2014): pp. 46-51.
  • Buyuk et al.
  • “
  • Investigation on the Effects of Boron Carbide Particle Size on Radiation Shielding Properties of Boron-Carbide Titanium Diboride Composites
  • ”