Immobilization of insoluble particles in polymer
Abstract
A method of immobilization of an insoluble dopant. In some embodiments, the insoluble dopant comprises a coordination polymer. In some embodiments, the insoluble dopant comprises a vapochromic coordination polymer. The method may comprise dissolving a polymer carrier in a solvent. The polymer carrier may comprise a thermoplastic such as, but not limited to, polylactic acid, polyethylene glycol or polycarbonate. The insoluble dopant (e.g. a coordination polymer such as a vapochromic coordination polymer) may then be mixed into the dissolved polymer. Phase separation of the mixture of the dopant and dissolved polymer may be induced to form a hydrogel. The hydrogel may be employed as is (e.g. as a raw material for hydrogel 3D printing, as a sensing material, etc.) or may undergo further processing (e.g. solidification, grinding, extrusion, etc.) before being employed, for example, as a raw material for 3D printing, as a sensing material, etc.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (8 — 3 Independent, 5 Dependent)
- Claim 1Independent Claim
A method for immobilizing insoluble dopants in polymer, the method comprising: dissolving a polymer carrier in a solvent; mixing an insoluble dopant in the dissolved polymer carrier to form a doped mixture; inducing phase separation of the doped mixture to obtain a doped hydrogel; allowing the doped hydrogel to solidify to form a doped solid; and activating the doped solid by exposing the doped solid to a target analyte.
- Claim 2Depends on #1
The method according to claim 1 comprising allowing the doped hydrogel to solidify through solvent exchange.
- Claim 3Depends on #1
The method according to claim 1 comprising allowing the doped hydrogel to solidify through solvent exchange by adding methanol to the doped hydrogel.
- Claim 4Independent Claim
A method for immobilizing insoluble dopants in polymer, the method comprising: dissolving a polymer carrier in a solvent; mixing an insoluble dopant in the dissolved polymer carrier to form a doped mixture; and inducing phase separation of the doped mixture to obtain a doped hydrogel; allowing the doped hydrogel to solidify to form a doped solid; and forming pellets from the doped solid.
- Claim 5Depends on #4
The method according to claim 4 comprising activating the doped solid by exposing the doped solid to a target analyte in at least one of: a gaseous form; a liquid form; and a solution form.
- Claim 6Independent Claim
A method for immobilizing insoluble dopants in polymer, the method comprising: dissolving a polymer carrier in a solvent; mixing an insoluble dopant in the dissolved polymer carrier to form a doped mixture; and inducing phase separation of the doped mixture to obtain a doped hydrogel; allowing the doped hydrogel to solidify to form a doped solid; and extruding the doped solid into 3D-printable filament.
- Claim 7Depends on #1
The method according to claim 1 wherein the solvent comprises a halogenated solvent.
- Claim 8Depends on #1
The method according to claim 1 wherein the solvent comprises dichloromethane.
Technical Overview & Description
REFERENCE TO RELATED APPLICATIONS This application is a continuation of Patent Cooperation Treaty (PCT) application No. PCT/CA2021/000007 having an international filing date of 22 Jan. 2021, which in turn claims priority from, and for the purposes of the United States the benefit of 35 USC § 119 in respect of, U.S. application No. 62/964,568 filed 22 Jan. 2020. All of the applications in this paragraph are hereby incorporated herein by reference. TECHNICAL FIELD This invention relates to immobilization of insoluble particles. Particular embodiments provide methods for immobilization of vapochromic coordination polymers to provide vapochromic sensing materials. BACKGROUND Vapochromic coordination polymers are metal-ligand based supramolecular materials constructed primarily from coordination bonding. Vapochromic coordination polymers exhibit changes in their spectroscopic signature in response to exposure to target analytes. For example, the Zn[Au(CN) 2 ] 2 vapochromic coordination polymer is highly sensitive to ammonia where, depending on the polymorph, its spectroscopic emission signature changes from 400-450 nm to 480-580 nm upon exposure to ammonia under excitation with a 405 nm radiation source. Vapochromic coordination polymers can be used in sensors for detection of target analytes, such as ammonia, for example, in environments not suitable for other types of chemical sensors (e.g. high moisture environments, environments comprising volatile/reactive analytes, etc). The accurate detection of ammonia, in particular, is important as it is toxic to humans at levels above 25 parts per million ( “ ppm ” ). For many ammonia detection applications, there is a desirability for accurate detection at levels of 5 ppm and less. For example, ammonia is a chemical that is commonly found in many areas such as: agriculture, refrigeration systems, and power transformers, where detection levels of 1 ppm may be desired. Vapochromic coordination polymers are typically difficult t
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (5)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (10)
- Thakkar et al.,
- “
- Development of 3D-printed polymer-zeolite composite monoliths for gas separation
- ”
- . Chemical Engineering Journal, Sep. 22, 2018 (Sep. 22, 2018), vol. 348(15), pp. 109-116.
- Stevens,
- “
- Vapochromic Coordination Polymer Immobilization Techniques for Ammonia Sensors with Applications to Power Transformers
- ”
- . MSC Thesis, Simon Fraser University, Apr. 16, 2019 (Apr. 16, 2019). Retrieved on Mar. 28, 2021 (Mar. 28, 2021) from http://summit.sfu.ea/system/files/iritems1/19228/etd20197.pdf p. 24, 1. 24-28; p. 25, 26; p. 27-31.