Methods for fabricating a layered semiconductor structure for NAND memory devices
Abstract
The present disclosure provides a fabrication method to produce a semiconductor structure with increased reliability for use in NAND memory devices. The method can include forming a layered semiconductor structure that includes a first layer, a second layer disposed on the first layer, and a third layer disposed on the second layer. The method can also include forming a channel structure, which can include etching the first layer, the second layer, and the third layer to form an opening through a surface of the semiconductor structure. A portion of the third layer can be exposed at the opening. The forming of the channel structure also include oxidizing the exposed portion of the third layer to form silicon oxide expand the exposed portion of the third layer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.
Claims (17 — 2 Independent, 15 Dependent)
- Claim 1Independent Claim
A method comprising: forming a semiconductor structure comprising a sacrificial layer, a first layer, a second layer disposed on the first layer, and a third layer disposed on the second layer; forming a channel structure, wherein forming the channel structure further comprises: etching the first layer, the second layer, and the third layer to form an opening through a surface of the semiconductor structure, wherein a portion of the third layer is exposed at the opening; and oxidizing the exposed portion of the third layer to form silicon oxide to expand the exposed portion of the third layer, wherein the exposed portion includes: a wide portion having a width defined perpendicular to a length of the channel structure, wherein the wide portion is disposed intersecting at least the second layer; and a narrow portion having a width defined perpendicular to the length of the channel structure, wherein the narrow portion is disposed intersecting at least the third layer and the width of the narrow portion is smaller than the width of the wide portion; removing the sacrificial layer and a portion of the channel structure to form a channel end structure that comprises a bottleneck cross-section based on the expanded exposed portion of the third layer; and disposing a polysilicon material on the channel end structure to form a contact to the third layer of the channel structure.
- Claim 2Depends on #1
The method of claim 1, wherein the oxidizing comprises using a wet oxidation process.
- Claim 3Depends on #1
The method of claim 1, wherein the expanding of the exposed portion of the third layer narrows a portion of the opening.
- Claim 4Depends on #1
The method of claim 1, further comprising: disposing a first channel layer at the opening; disposing a second channel layer at the opening and on the first channel layer; and disposing a third channel layer at the opening and on the second channel layer.
- Claim 5Depends on #4
The method of claim 4, wherein: the expanding of the exposed portion of the third layer narrows a portion of the opening; and the disposing of the first, second, or third channel layers obstructs the narrowed portion of the opening.
- Claim 6Depends on #4
The method of claim 4, further comprising disposing fourth and fifth channel layers at the opening of the channel structure.
- Claim 7Depends on #1
The method of claim 1, wherein the forming of the semiconductor structure comprises forming a layer of silicon oxide for the first layer.
- Claim 8Depends on #1
The method of claim 1, wherein the forming of the semiconductor structure comprises forming a layer of silicon nitride for the second layer.
- Claim 9Depends on #1
The method of claim 1, wherein the oxidizing comprises performing a wet oxidation process using gasses having a temperature greater than approximately 600 degrees Celsius and less than approximately 800 degrees Celsius.
- Claim 10Depends on #1
The method of claim 1, wherein the oxidizing comprises exposing the exposed portion of the third layer to hydrogen gas and oxygen gas.
- Claim 11Depends on #10
The method of claim 10, wherein a ratio of the hydrogen gas to the oxygen gas is greater than approximately 0.14 and less than approximately 7.00.
- Claim 12Depends on #10
The method of claim 10, wherein the oxidizing comprises exposing the exposed portion of the third layer to nitrogen gas.
- Claim 13Depends on #1
The method of claim 1, wherein the semiconductor structure comprises the sacrificial layer affixed to at least the first layer.
- Claim 14Depends on #13
The method of claim 13, further comprising disposing a first channel layer at the opening wherein a portion of the first channel layer is disposed in an etched portion of the sacrificial layer.
- Claim 15Independent Claim
A method of fabricating a semiconductor structure comprising a sacrificial layer, a first layer, a second layer, a third layer, and a channel structure disposed intersecting at least the first, second, and third layers and comprising a void and a narrowed portion, the method comprising: removing the sacrificial layer, wherein the removing of the sacrificial layer comprises removing a portion of the channel structure disposed intersecting the sacrificial layer to form a channel end structure that comprises a bottleneck cross-section; removing the first layer to expose the third layer and the narrowed portion of the channel structure, wherein the narrowed portion has a width defined perpendicular to a length of the channel structure, the narrowed portion is disposed intersecting at least the third layer, and the width of the narrowed portion is smaller than a width of a wide portion having a width defined perpendicular to the length of the channel structure, wherein the wide portion is disposed intersecting at least the second layer, and wherein material produced by the removing of the sacrificial layer is prevented from entering the void of the channel structure based on the narrowed portion obstructing access to the void; and disposing a polysilicon material on the channel end structure to form a contact to a polysilicon structure of the channel structure.
- Claim 16Depends on #15
The method of claim 15, further comprising etching portions of the first and second layers disposed proximal to the narrowed portion of the channel structure.
- Claim 17Depends on #15
The method of claim 15, wherein the removing of the sacrificial layer further comprises using a chemical mechanical polishing process.
Technical Overview & Description
TECHNICAL FIELD The present disclosure generally relates to the field of semiconductor technology, and more particularly, to a method for debugging double program errors in NAND memory. BACKGROUND As memory devices are shrinking to smaller die size to reduce manufacturing cost and increase storage density, scaling of planar memory cells faces challenges due to process technology limitations and reliability issues. A three-dimensional (3D) memory architecture can address the density and performance limitation in planar memory cells. In a 3D NAND flash memory, many layers of memory cells can be stacked vertically such that storage density per unit area can be greatly increased. The vertically stacked memory cells can form memory strings, where the channels of the memory cells are connected in each memory string. Each memory cell can be addressed through a word line and a bit line. Data (i.e., logic states) of the memory cells in an entire memory page sharing the same word line can be read or programmed simultaneously. However, due to aggressive scaling, reliability can be a concern for a 3D NAND flash memory. BRIEF SUMMARY Embodiments of methods and systems for data protection in a memory device are described in the present disclosure. In some embodiments, a fabrication method can produce a semiconductor structure with increased reliability for use in NAND memory devices. The method can include forming a semiconductor structure that includes a first layer, a second layer disposed on the first layer, and a third layer disposed on the second layer. The method can also include forming a channel structure, which can include etching the first layer, the second layer, and the polysilicon layer to form an opening through a surface of the semiconductor structure. A portion of the third layer can be exposed at the opening. The forming of the channel structure can also include oxidizing the exposed portion of the third layer to form silicon oxide to expand the exposed portion o
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.