hottub.patents
US 12,525,640 B2#3343611 Most CitedActiveUnited States (USPTO)Utility

Method for producing sulfide solid electrolyte including Sn

0Forward Citations (#3343611 Global)
0.0/yrCitation Velocity (#3343611 Global)
0.00Citation PageRank (#3343611 Global)
12Prior Art Cited
8Structured Claims
0Drawings / Sheets

Abstract

A method for producing a sulfide solid electrolyte includes: preparing a uniform solution that includes at least elemental lithium (Li), elemental tin (Sn), elemental phosphorus (P), and elemental sulfur (S) in an organic solvent; removing the organic solvent from the uniform solution to obtain a precursor; and heat-treating the precursor to obtain a sulfide solid electrolyte.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (8)

  1. Claim 1Independent Claim

    A method for producing a sulfide-based solid electrolyte which comprises: preparing a homogeneous solution that includes at least elemental lithium (Li), elemental tin (Sn), elemental phosphorus (P) and elemental sulfur (S) in an organic solvent; removing the organic solvent from the homogeneous solution to obtain a precursor; and heat-treating the precursor to obtain the sulfide-based solid electrolyte; wherein the preparing of the homogenous solution comprises: mixing Li 2 S and P 2 S 5 with each other in the organic solvent to prepare an Li — P — S homogeneous solution; preparing an Li — Sn — S homogeneous solution that includes at least elemental lithium (Li), elemental tin (Sn) and elemental sulfur (S) in the organic solvent; wherein the preparing of the Li — Sn — S homogeneous solution comprises mixing Li 2 S, SnS, and S with each other in the organic solvent to prepare the Li — Sn — S homogeneous solution; and mixing the Li — P — S homogeneous solution and the Li — Sn — S homoge

  2. Claim 2Depends on #1

    The method according to claim 1, wherein the organic solvent is at least one selected from the group consisting of an ether-based solvent, a nitrile-based solvent and an ester-based solvent.

  3. Claim 3Depends on #1

    The method according to claim 1, wherein the organic solvent is at least one selected from the group consisting of tetrahydrofuran, acetonitrile, ethyl acetate and methyl acetate.

  4. Claim 4Depends on #1

    The method according to claim 1, wherein during the removing of the organic solvent the temperature is 60 to 280 ° C.

  5. Claim 5Depends on #1

    The method according to claim 1, wherein during the heat-treating of the precursor the temperature is 200 ° C. to 700 ° C.

  6. Claim 6Depends on #1

    The method according to claim 1, wherein the sulfide-based solid electrolyte contains an LGPS-based solid electrolyte and has peaks at least 2 θ =19.90 ° ± 0.50 °, 20.20 ° ± 0.50 °, 26.70 ° ± 0.50 ° and 29.20 ° ± 0.50 ° in X-ray diffraction (CuK α: λ =1.5405 Å).

  7. Claim 7Independent Claim

    A method for producing a sulfide-based solid electrolyte which comprises: preparing a homogeneous solution that includes at least elemental lithium (Li), elemental tin (Sn), elemental phosphorus (P) and elemental sulfur (S) in an organic solvent; removing the organic solvent from the homogeneous solution to obtain a precursor; and heat-treating the precursor to obtain the sulfide-based solid electrolyte, wherein the preparing of the homogenous solution comprises: mixing Li 2 S and P 2 S 5 with each other in the organic solvent to prepare an Li — P — S homogeneous solution; preparing an Li — Sn — S homogeneous solution that includes at least elemental lithium (Li), elemental tin (Sn) and elemental sulfur (S) in the organic solvent; mixing Li 2 S and S with each other in the organic solvent to prepare an Li — S homogeneous solution; preparing an Li — Si — S homogeneous solution that includes at least elemental lithium (Li), elemental silicon (Si) and elemental sulfur(S) in the organic so

  8. Claim 8Depends on #7

    The method according to claim 7, wherein the preparing of the Li — Si — S homogeneous solution comprises mixing Li 2 S, SiS 2 and S with each other in the organic solvent to prepare the Li — Si — S homogeneous solution.

Technical Overview & Description

TECHNICAL FIELD The present invention relates to a method for producing a sulfide-based solid electrolyte including Sn. BACKGROUND ART Recently, a demand for lithium ion secondary batteries has been increased in applications including portable information terminals, portable electronic equipments, electric vehicles, hybrid electric vehicles and stationary power storage systems. However, currently, a flammable organic solvent is used as an electrolytic solution in lithium ion secondary batteries, and a strong exterior is required so that an organic solvent does not leak out. Further, for example, in the case of portable personal computers, it is necessary to employ a structure against a risk at the time when an electrolytic solution leaks out. Thus, there is a limitation on structures of devices. Moreover, the range of applications thereof has been widened to movable bodies such as vehicles and aircrafts, and a high capacity is desired for stationary lithium ion secondary batteries. Under such circumstances, importance tends to be placed on safety more than before, and efforts are concentrated on the development of an all-solid-state lithium ion secondary battery in which none of toxic substances such as organic solvents is used. For example, use of an oxide, phosphate compound, organic polymer, sulfide or the like as a solid electrolyte in an all-solid-state lithium ion secondary battery has been examined. Among these solid electrolytes, the sulfide has characteristics that it has high ion conductivity and is relatively soft, and that it is easy to form the interface between solids. The sulfide is stable with respect to active materials and has been developed as a practical solid electrolyte. It has been found that, among sulfide-based solid electrolytes, an Sn-containing sulfide-based solid electrolyte provides satisfactory ion conductivity and high water resistance, and practical use thereof is highly expected (Non-Patent Document 1). As a method for producing a s

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (12)

PatentTitleYearCitations

Non-Patent Literature (10)

  • Extended European Search Report dated Nov. 8, 2023 issued corresponding European family member patent application No. 21741412.7.
  • International Search Report and Written Opinion of the International Searching Authority issued in International Application No. PCT/JP2021/000182, dated Mar. 30, 2021, along with an English translation thereof.
  • Bron, P. et al.,
  • “
  • Li
  • SnP
  • S
  • : an Affordable Lithium Superionic Conductor
  • ”
  • , J. Am. Chem. Soc., Sep. 30, 2013, pp. 15694-15697.