Abstract
The present disclosure provides poly(tetrafluoroethylene) (PTFE) microparticles with a Dv50 of about 20 μ m to about 30 μ m and a specific surface area (SSA) of at least about 3.0 m 2 /g when measured by a multipoint BET method of ISO 9277. Such PTFE microparticles can be obtained via a method including thermomechanically degrading scrap PTFE in the presence of air and/or oxygen and reducing the particle size of the resultant degraded PTFE.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 0.
Claims (8)
- Claim 1Independent Claim
Microparticles comprising reprocessed poly(tetrafluoroethylene) (PTFE), wherein the microparticles exhibit a Dv50 of about 20 μ m to about 30 μ m and an improved specific surface area (SSA) for particles of that size range of at least about 3.0 m 2 /g when measured by a multipoint BET method of ISO 9277.
- Claim 2Depends on #1
The microparticles of claim 1, wherein the microparticles are prepared via thermomechanically degrading reprocessed PTFE in the presence of air and/or oxygen to give degraded PTFE and reducing particle size of the degraded PTFE.
- Claim 3Depends on #1
The microparticles of claim 1, wherein the microparticles consist essentially of the reprocessed poly(tetrafluoroethylene) and modified poly(tetrafluoroethylene) species.
- Claim 4Depends on #3
The microparticles of claim 3, wherein the modified poly(tetrafluoroethylene) species comprise poly(tetrafluoroethylene) modified by one or more of oxygen atoms, additional carbon atoms, and/or additional hydrogen atoms.
- Claim 5Depends on #1
The microparticles of claim 1, wherein the microparticles are prepared via a method that does not comprise irradiation.
- Claim 6Depends on #2
The microparticles of claim 2, wherein the thermomechanical degrading comprises passing the reprocessed PTFE multiple times through equipment designed for thermomechanical degradation.
- Claim 7Depends on #2
The microparticles of claim 2, wherein the reducing particle size comprises passing the degraded PTFE multiple times through equipment designed for particle size reduction.
- Claim 8Depends on #2
The microparticles of claim 2, wherein the thermomechanical degrading is conducted in an extruder.
Technical Overview & Description
CROSS-REFERENCE TO RELATED APPLICATION The present application is a continuation of U.S. patent application Ser. No. 17/329,346, filed May 25, 2021; which application claims priority to U.S. Provisional Patent Application No. 63/029,851, filed May 26, 2021 and U.S. Provisional Patent Application No. 63/030,634, filed May 27, 2020, which are incorporated by reference in their entireties. FIELD OF THE INVENTION The present application relates generally to the field of poly(tetrafluoroethylene) (PTFE) particles, and to methods of producing such particles. BACKGROUND Poly(tetrafluoroethylene) (PTFE) resin is used in paste extrusion processes to manufacture such products as sheets, profiles, monofilaments, and tubes. Paste extrusion of PTFE generally involves several steps, including: (1) paste preparation or resin mixing with lubricants; (2) preforming; (3) paste extrusion through one or more die heads; and (4) devolatilization. Paste extrusion processes produce scrap PTFE that is either unsintered or sintered. Unsintered scrap includes the end section of a preform (the “ tail ” ) as well as the conical remnant in the die head (the “ cone ” ). Sintered scrap PTFE has gone through the entire process referenced above and includes trim scrap, changeover scrap, and off-spec material from start-up and shut down. It is desirable to provide ways to utilize such scrap PTFE to manufacture new products and reduce waste. In particular, converting the scrap to PTFE microparticles represents one method by which value-added products can be produced, as such microparticles can be useful, e.g., in the fields of lubrication, polymer processing and printing/coating. Current methods of preparing scrap PTFE for grinding/microparticle production involve irradiation with high energy sources such as gamma, e-beam or X-ray to first embrittle the material. Various methods involve cutting, cleaning, drying, sintering, and ball-milling cryogenically; using ultraviolet radiation in combination wit
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (5)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 2006/063140 A2 | Insulating concrete block | — | 0 |
Non-Patent Literature (5)
- JP-62121093-A machine translation (Year: 1987).
- JP-2001011676-A machine translation (Year: 2001).
- JP-2006063140-A machine translation (Year: 2006).
- WO-2007007422-A1 machine translation (Year: 2007).
- JP2001514285A Machine Translation (Year: 2001).