High-strength Portland cement slurry for ultra-high temperature cementing, preparation method therefor and application thereof

0Forward Citations (#156058852 Global)
0.0/yrCitation Velocity (#156058852 Global)
0.00Citation PageRank (#156058852 Global)
20Prior Art Cited
14Claims (1 Indep. · 13 Dep.)
0Drawings / Sheets

Abstract

A high-strength Portland cement slurry for ultra-high-temperature cementing, a preparation method therefor and an application thereof. In parts by weight, the composition of the cement slurry comprises: 100 parts of Portland cement, 4-6 parts of a high temperature anti-cracking material, 80-105 parts of a high-temperature reinforcing material, 70-78 parts of water, 0.5-1.5 parts of a dispersant, 1-3 parts of a fluid loss reducer, 0.5-2.5 parts of a retarder and 0.2-0.5 parts of a defoamer; the high-temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin and aluminum sulfate, a combination of acid-washed quartz sand, metakaolin, feldspar and sodium sulfate, or a combination of acid-washed quartz sand, metakaolin, feldspar and calcium nitrite. The cement slurry has good settling stability, rapid strength development in low temperatures, high compressive strength of cement stone at a high temperature of 600 ° C., and stable development of long-term high-temperature compressive strength.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 20 · Forward citations: 0.

Claims (14 — 1 Independent, 13 Dependent)

  1. Claim 1Independent Claim

    A high-strength Portland cement slurry for ultra-high temperature cementing, comprising by weight: 100 parts of Portland cement, 4-6 parts of a high temperature anti-cracking material, 80-105 parts of a high temperature reinforcing material, 70-78 parts of water, 0.5-1.5 parts of a dispersant, 1-3 parts of a fluid loss additive, 0.5-2.5 parts of a retarder, and 0.2-0.5 parts of a defoamer; wherein the high temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin, and aluminum sulfate in a mass ratio of 25-35:5-15:1, or a combination of acid-washed quartz sand, metakaolin, feldspar, and sodium sulfate in a mass ratio of 25-35:5-15:5-15:1, or a combination of acid-washed quartz sand, metakaolin, feldspar, and calcium nitrite in a mass ratio of 25-35:5-15:5-15:1.

  2. Claim 2Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the Portland cement is one or two or more of Grade A, Grade B, Grade C, Grade D, Grade E, Grade F, Grade G, Grade H and Grade J Portland cements for cementing oil and gas wells.

  3. Claim 3Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the high temperature anti-cracking material comprises a combination of two materials from basalt fiber, mullite, and sepiolite, and the mass ratio between the two materials is 1-3:1.

  4. Claim 4Depends on #3

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 3, wherein the mass ratio between the two materials constituting the high temperature anti-cracking material is 1:1.

  5. Claim 5Depends on #2

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 2, wherein the high temperature anti-cracking material comprises a combination of two materials from basalt fiber, mullite, and sepiolite, and the mass ratio between the two materials is 1-3:1.

  6. Claim 6Depends on #5

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 5, wherein the mass ratio between the two materials constituting the high temperature anti-cracking material is 1:1.

  7. Claim 7Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the high temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin, and aluminum sulfate in a mass ratio of 30:10:1.

  8. Claim 8Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the high temperature reinforcing material is a combination of acid-washed quartz sand, metakaolin, feldspar, and sodium sulfate in a mass ratio of 30:10:10:1, or a combination of acid-washed quartz sand, metakaolin, feldspar, and calcium nitrite in a mass ratio of 30:10:10:1.

  9. Claim 9Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the dispersant comprises an aldehyde-ketone condensate or a polycarboxylic acid-based dispersant.

  10. Claim 10Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the fluid loss additive is an AMPS polymer-based fluid loss additive.

  11. Claim 11Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the retarder is one or two or more of hydroxyethylidenediphosphonic acid, etidronic acid and ethylenediamine tetramethylene phosphonic acid.

  12. Claim 12Depends on #1

    The high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, wherein the defoamer is dimethyl silicone and/or tributyl phosphate.

  13. Claim 13Depends on #1

    A method for producing the high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, comprising the steps of: dry-mixing the high temperature anti-cracking material, the high temperature reinforcing material, the fluid loss additive, the dispersant and the Portland cement uniformly; wet-mixing the retarder, the defoamer and water uniformly; and adding the dry mixture to the wet mixture under stirring, and stirring them until uniform to obtain the high-strength Portland cement slurry for ultra-high temperature cementing.

  14. Claim 14Depends on #1

    A method of a cementing operation, wherein the method uses the high-strength Portland cement slurry for ultra-high temperature cementing according to claim 1, the cementing operation is a cementing operation at 600 ° C. or higher; in the cementing operation, the high-strength Portland cement slurry forms cement stone after a curing process.

Technical Overview & Description

CROSS-REFERENCE TO RELATED APPLICATIONS This application is a continuation of International Application No. PCT/CN2021/126618, filed on Oct. 27, 2021, which claims priority to Chinese Patent Application No. 202011313439.1, filed on Nov. 20, 2020, both of which are hereby incorporated by reference in their entireties. TECHNICAL FIELD The present disclosure relates to a high-strength Portland cement slurry for ultra-high temperature cementing and a production method and use thereof, and belongs to the technical field of well cementing. BACKGROUND For thermal recovery of super heavy oil fire flooding and coalbed gasification, the temperature in the wellbore is 600 ° C.-1000 ° C., and ordinary sand-containing cement stone in the well has a loose structure, significantly reduced compressive strength, and increased permeability at high temperature, which seriously affects the annular sealing ability of the cement sheath and greatly shortens the production life of thermal recovery wells for super heavy oil fire flooding and coal gasification wells. Therefore, it is necessary to develop a cement slurry system with high compressive strength of cement stone at high temperature and stable development of long-term compressive strength at high temperature. At present, Portland cement with quartz sand, aluminate cement and phosphoaluminate cement are mainly used as the cement slurry system for cementing. Although the high temperature compressive strength is higher than that of pure cement slurry, there are still some problems as follows. (1) The high temperature compressive strength of Portland cement with quartz sand at 600 ° C. declines very seriously, and the cement sheath tends to lose the interlayer sealing ability. (2) The price of aluminate cement or phosphoaluminate cement is ten or more times that of Portland cement. (3) It is difficult to develop admixtures such as fluid loss additive and retarder suitable for aluminate cement or phosphoaluminate cement, while Portland

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (20)

PatentTitleYearCitations
US 4,676,832 ASet delayed cement compositions and methods of using the same1987240
US 2012014812 A1Compressor Surge Control System and Method—42
US 2018037795 A1Downhole fluids and methods of use thereof—17
US 2018334880 A1Rapid setting in situ cement plugs—13
US 2019241792 A1High temperature resistant portland cement slurry and production method thereof—24
CN 102,531,481 AHigh-strength low-density cement paste adopting fluid loss agent—14
CN 105,884,239 ASulfoaluminate-Portland cement composite system additive, fast-hardening early-strength concrete and preparation method of concrete—18
CN 106,986,584 AA kind of low-temperature high-strength cement slurry and its preparation method and application—24
CN 107,200,520 ADeep well cementing weighted cement slurry system—1
CN 107,244,857 AWell cementation cement slurry and preparation method thereof—20
CN 108,298,902 AA kind of high temperature resistant silicate grout and preparation method thereof—29
CN 108,439,872 AA kind of high intensity low-elasticity-modulus high-density cement mortar of high temperature resistance—8
CN 104,371,678 BA kind of expansion toughness cementing slurry and preparation method thereof20182
CN 108,623,258 AA kind of oil-proof concrete—1
CN 108,706,927 AA kind of high-temperature water mud suspension stabilizer and its high temperature resisting cement grout of preparation—16
CN 108,911,618 AA kind of preparation method of the hollow partition board of excellent in mechanical performance—4
CN 109,437,710 AA kind of high water-cement ratio low cost low-density well cementing cement mortar and preparation method thereof—15
CN 109,943,303 AA kind of oil well cement chlorine-free coagulation accelerating early strength agent and its preparation method and application—4
JP H08104556 ACement accelerating agent and cement composition—9
WO 2020/187742 A1Mineral binder composition for 3d printing—11

Non-Patent Literature (10)

  • CN109811618A Merge with Machine translation.
  • JPH08104556A Merge with Machine trnalstion.
  • Extended European Search Report issued on Feb. 19, 2024 for counterpart European patent application No. 21893705.0 (5 pages).
  • Decision of Rejection issued on Dec. 2, 2022 for counterpart Chinese patent application No. 202011313439.1, along with EN translation.
  • First Office Action and search report issued on Jun. 22, 2022 for counterpart Chinese patent application No. 202011313439.1, along with machine EN translation downloaded from EPO.
  • International Search Report issued for counterpart Chinese patent application No. PCT/CN2021/126618 mailed on Dec. 31, 2021.
  • Lan Bang et al., Research progress in additives for strength reinforcement of Portland cement, Inorganic Chemicals Industry, 2015, vol. 47, No. 11, pp. 15-19.
  • Qing Xiong Shan, Practice Guide for Petroleum Engineering borehole, China University of Petroleum Press, No. 1, p. 390, 2011.
  • Xiuzhen, et al., Composite anti-crack technology of high-performance concrete structure, Jiangsu Building Materials, No. 2, 2009.
  • Yunlong, et al., Production and application technology of dry-mixed gypsum building materials, China Building Materials Industry Press, vol. 1, 2006.