Metal nanoparticles in an amorphous bonding layer between a device substrate and carrier substrate
Abstract
A method for manufacturing a semiconductor structure includes: forming a first bonding layer on a device substrate, the first bonding layer including a first bonding sub-layer and a second bonding sub-layer, the first bonding sub-layer including a first metal oxide material in an amorphous state and a plurality of metal nanoparticles, the second bonding sub-layer including a second metal oxide material in an amorphous state; forming a second bonding layer on a carrier substrate, the second bonding layer including a third metal oxide material in an amorphous state; conducting a surface modification process on the first and second bonding layers; bonding the device and carrier substrates to each other through the first and second bonding layers; and annealing the first and second bonding layers to convert the first, second, and third metal oxide materials from the amorphous state to a crystalline state.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 1.
Claims (8)
- Claim 1Independent Claim
A method for manufacturing a semiconductor structure, comprising: forming a first bonding layer on a device substrate formed with a semiconductor device so as to cover the semiconductor device, the first bonding layer including a first bonding sub-layer disposed on the device substrate and a second bonding sub-layer disposed on the first bonding sub-layer opposite to the semiconductor device, the first bonding sub-layer including a first metal oxide material in an amorphous state and a plurality of metal nanoparticles, the second bonding sub-layer including a second metal oxide material in an amorphous state; forming a second bonding layer on a carrier substrate, the second bonding layer including a third metal oxide material in an amorphous state; conducting a surface modification process on the first bonding layer and the second bonding layer; bonding the device substrate and the carrier substrate to each other through the first bonding layer and the second bonding layer; and anneali
- Claim 2Depends on #1
The method according to claim 1, wherein formation of the first bonding layer includes: alternately forming a plurality of metal nanoparticle layers and a plurality of metal oxide layers on the device substrate so as to form a metal oxide-based stack which covers the semiconductor device, an uppermost one of the plurality of metal oxide layers serving as an uppermost layer of the metal oxide-based stack distal from the semiconductor device, each of the plurality of metal nanoparticle layers including a plurality of the metal nanoparticles; and subjecting the uppermost one of the plurality of metal oxide layers to planarization, wherein the uppermost one of the plurality of metal oxide layers serves as the second bonding sub-layer, and the plurality of metal nanoparticle layers and the other ones of the plurality of metal oxide layers collectively serve as the first bonding sub-layer.
- Claim 3Depends on #2
The method according to claim 2, wherein each of the plurality of metal oxide layers is formed by a deposition process conducted at a temperature ranging from room temperature to 300 ° C.
- Claim 4Depends on #2
The method according to claim 2, wherein the uppermost one of the plurality of metal oxide layers includes the second metal oxide material; each of the other ones of the plurality of metal oxide layers includes the first metal oxide material; each of the first metal oxide material, the second oxide material, and the third metal oxide material has a formula of MOx, wherein M is selected from Al, Ti, Mg, Zn, Ni, or combinations thereof and x is a number satisfying the valence of M, and the first metal oxide material, the second oxide material, and the third metal oxide material are the same as or different from one another; M-OH bonds are formed on a surface of the first bonding layer and a surface of the second bonding layer which face toward each other after the surface modification process; and the M-OH bonds polymerize to result in formation of M-O-M bonds and water molecules, the first bonding layer and the second bonding layer being bonded to each other through the M-O-M bonds.
- Claim 5Depends on #1
The method according to claim 1, wherein formation of the first bonding layer includes: alternately forming a plurality of metal nanoparticle layers and a plurality of metal oxide layers on the device substrate so as to form a metal oxide-based stack which covers the semiconductor device, each of the plurality of metal nanoparticles layers including a plurality of the metal nanoparticles; forming an additional metal oxide layer on the metal oxide-based stack opposite to the semiconductor device; and subjecting the additional metal oxide layer to planarization, wherein the metal oxide-based stack serves as the first bonding sub-layer, and the additional metal oxide layer serves as the second bonding sub-layer.
- Claim 6Depends on #5
The method according to claim 5, wherein each of the additional metal oxide layer and the plurality of metal oxide layers of the metal oxide-based stack is formed by a deposition process conducted at a temperature ranging from room temperature to 300 ° C.
- Claim 7Depends on #5
The method according to claim 5, wherein the additional metal oxide layer includes the second metal oxide material; each of the plurality of metal oxide layers of the metal oxide-based stack includes the first metal oxide material; each of the first metal oxide material, the second oxide material, and the third metal oxide material has a formula of MOx, wherein M is selected from Al, Ti, Mg, Zn, Ni, or combinations thereof and x is a number satisfying the valence of M, and the first metal oxide material, the second oxide material, and the third metal oxide material are the same as or different from one another; M-OH bonds are formed on a surface of the first bonding layer and a surface of the second bonding layer which face toward each other after the surface modification process; and the M-OH bonds polymerize to result in formation of M-O-M bonds and water molecules, the first bonding layer and the second bonding layer being bonded to each other through the M-O-M bonds.
- Claim 8Depends on #1
The method according to claim 1, wherein formation of the first bonding layer includes: forming a doped metal oxide layer on the device substrate to cover the semiconductor device, the doped metal oxide layer including a metal oxide matrix and the metal nanoparticles doped into the metal oxide matrix; forming an undoped metal oxide layer on the doped metal oxide layer opposite to the semiconductor device; and subjecting the undoped metal oxide layer to planarization, wherein the doped metal oxide layer serves as the first bonding sub-layer, and the undoped metal oxide layer serves as the second bonding sub-layer.
Technical Overview & Description
BACKGROUND The semiconductor integrated circuit (IC) industry has, over the decades, experienced tremendous advancements and is still undergoing vigorous development. With dramatic advances in technology, the industry pays much attention on the development of small IC devices with high performance and low power consumption. Since substrate is an important component of semiconductor devices, substrate bonding issue, such as heat dissipation issue, needs be solved in order to facilitate manufacturing process of semiconductor devices. BRIEF DESCRIPTION OF THE DRAWINGS Aspects of the present disclosure are best understood from the following detailed description when read with the accompanying figures. It is noted that, in accordance with the standard practice in the industry, various features are not drawn to scale. In fact, the dimensions of the various features may be arbitrarily increased or reduced for clarity of discussion. FIG. 1 is a flow diagram illustrating a method for manufacturing a semiconductor structure in accordance with some embodiments. FIGS. 2 to 21 are schematic views showing some intermediate stages of the method depicted in FIG. 1 . DETAILED DESCRIPTION The following disclosure provides many different embodiments, or examples, for implementing different features of the disclosure. Specific examples of components and arrangements are described below to simplify the present disclosure. These are, of course, merely examples and are not intended to be limiting. For example, the formation of a first feature over or on a second feature in the description that follows may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features may be formed between the first and second features, such that the first and second features may not be in direct contact. In addition, the present disclosure may repeat reference numerals and/or letters in the various examples. This repet
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,702,040 B2 | Low temperature substrate bonding method | 2026 | 0 |
References Cited — Backward Prior Art (5)
| Patent | Title | Year | Citations |
|---|