High aspect ratio dielectric etch with chlorine
Abstract
Various embodiments herein relate to methods and apparatus for etching recessed features on a semiconductor substrate. The techniques described herein can be used to form high quality recessed features with a substantially vertical profile, low bowing, low twisting, and highly circular features. These high quality results can be achieved with a high degree of selectivity and a relatively high etch rate. In various embodiments, etching involves exposing the substrate to plasma generated from a processing gas that includes a chlorine source, a carbon source, a hydrogen source, and a fluorine source. The chlorine source may have particular properties. In some cases, particular chlorine sources may be used. Etching typically occurs at low temperatures, for example at about 25 C or lower.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 80 · Forward citations: 0.
Claims (17 — 1 Independent, 16 Dependent)
- Claim 1Independent Claim
A method of etching recessed features on a substrate, the method comprising: a. providing the substrate on a substrate support in a reaction chamber, the substrate having a stack thereon, the stack comprising one or more layers of a first material comprising a silicon-containing material alternating with one or more layers of a second material, the substrate further comprising a patterned mask layer positioned over the stack; b. flowing processing gas into the reaction chamber and generating a plasma from the processing gas, wherein the processing gas comprises: i. a chlorine source comprising molecules containing only carbon, hydrogen, bromine, and chlorine, or comprising molecules containing only chlorine, carbon, and nitrogen, ii. a carbon source, iii. a fluorine source, and iv. a hydrogen source; and c. exposing the substrate to the plasma to etch recessed features into the stack on the substrate, the recessed features being etched through one or more of the layers of the first material and through one or more of the layers of the second material, wherein the substrate support is maintained at a cryogenic temperature during etching.
- Claim 2Depends on #1
The method of claim 1, wherein the first material comprises silicon nitride and the second material comprises silicon oxide.
- Claim 3Depends on #2
The method of claim 2, wherein the stack further comprises one or more layers of a third material alternating with the one or more layers of the first material comprising silicon nitride and the one or more layers of the second material comprising silicon oxide.
- Claim 4Depends on #3
The method of claim 3, wherein the third material comprises polysilicon.
- Claim 5Depends on #1
The method of claim 1, wherein the first material comprises silicon nitride and the second material comprises polysilicon.
- Claim 6Depends on #1
The method of claim 1, wherein the chlorine source comprises at least one species selected from the group consisting of ClCN, CH 2 BrCl, C 2 H 2 BrCl, and C 2 H 4 BrCl.
- Claim 7Depends on #1
The method of claim 1, wherein the substrate support is maintained at a cryogenic temperature between about − 40 ° C. and − 10 ° C. during etching.
- Claim 8Depends on #1
The method of claim 1, wherein the plasma is a capacitively coupled plasma generated at an RF power between about 10-100 kW.
- Claim 9Depends on #1
The method of claim 1, wherein the hydrogen source comprises at least one material selected from the group consisting of: H 2, CH x F y (where 1 ≤ x ≤ 4, and x+y=4), C x H y F z (where z > 0), and combinations thereof.
- Claim 10Depends on #1
The method of claim 1, wherein the hydrogen source comprises H 2.
- Claim 11Depends on #1
The method of claim 1, wherein the fluorine source comprises at least one material selected from the group consisting of: NF 3, CH x F y (where 0 ≤ x ≤ 3, and x+y=4), C x F y (where y > x), C x H y F z (where z > 0), and combinations thereof.
- Claim 12Depends on #1
The method of claim 1, wherein the carbon source comprises at least one material selected from the group consisting of: CH x F y (where 0 ≤ x ≤ 4, and x+y=4), C x F y (where y > x), C x H y F z (where z > 0), and combinations thereof.
- Claim 13Depends on #1
The method of claim 1, wherein the processing gas comprises Cl 2, H 2, NF 3, CH 2 F 2, CF 4, and at least one of HBr and CF 3 I.
- Claim 14Depends on #1
The method of claim 1, wherein the recessed features that are formed have a 3 σ twist of about 10 nm or less.
- Claim 15Depends on #1
The method of claim 1, wherein the recessed features that are formed have a depth of at least about 4000 nm.
- Claim 16Depends on #1
The method of claim 1, wherein the recessed features that are formed have an ellipticity of about 1.15 or less.
- Claim 17Depends on #1
The method of claim 1, wherein the recessed features that are formed have a maximum critical dimension of about 115 nm or less, and/or a Max − Bottom CD of about 40 nm or less.
Technical Overview & Description
INCORPORATION BY REFERENCE A PCT Request Form is filed concurrently with this specification as part of the present application. Each application that the present application claims benefit of or priority to as identified in the concurrently filed PCT Request Form is incorporated by reference herein in their entireties and for all purposes. BACKGROUND One process frequently employed during fabrication of semiconductor devices is formation of an etched cylinder or other recessed feature in dielectric material. Often the dielectric material includes alternating/repeating layers into which the recessed feature is formed. One example context where such a process may occur is memory applications such as 3D NAND. As the semiconductor industry advances and device dimensions become smaller, such recessed features become increasingly harder to etch in a uniform manner, especially for high aspect ratio features having narrow widths and/or deep depths. The background description provided herein is for the purposes of generally presenting the context of the disclosure. Work of the presently named inventors, to the extent it is described in this background section, as well as aspects of the description that may not otherwise qualify as prior art at the time of filing, are neither expressly nor impliedly admitted as prior art against the present disclosure. SUMMARY Various embodiments herein relate to methods and apparatus for etching recessed features on a semiconductor substrate. For example, in one aspect of the disclosed embodiments, a method of etching recessed features on a substrate is provided, the method including: (a) providing the substrate on a substrate support in a reaction chamber, the substrate having a stack thereon, the stack including one or more layers of a first material including a silicon-containing material alternating with one or more layers of a second material, the substrate further including a patterned mask layer positioned over the stack; (b) flowing
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (80)
Non-Patent Literature (10)
- Chinese First Office Action dated Aug. 22, 2017 issued in Application No. CN 201510543852.X.
- Chinese First Office Action dated Jul. 17, 2019 issued in Application No. CN 201610996940.X.
- Chinese Second Office Action dated Feb. 25, 2020 issued in Application No. CN 201610996940.X.
- International Preliminary Report on Patentability dated Oct. 13, 2022, in PCT Application No. PCT/US2021/021752.
- International Search Report and Written Opinion dated Jun. 29, 2021, in PCT Application No. PCT/US2021/021752.
- Japanese First Office Action dated Jun. 5, 2019 issued in Application No. JP 2015-167336.
- Korean First Office Action dated Nov. 27, 2019 issued in Application No. KR 10-2013-0076689.
- KR Office Action dated Feb. 28, 2022, in Application No. KR1020150121582 with English translation.
- Nishino et al. (1993)
- “