Method to form narrow slot contacts
Abstract
In method of patterning a substrate, a first relief pattern is formed based on a first layer deposited over a substrate. Openings in the first relief pattern are filled with a reversal material. The first relief pattern is then removed from the substrate and the reversal material remains on the substrate to define a second relief pattern. A fill material is deposited over the substrate that is in contact with the second relief pattern, and sensitive to a photo-acid generated from a photo-acid generator in the second relief pattern. Selected portions of the second relief pattern are exposed to a first actinic radiation to generate the photo-acid in the selected portions of the second relief pattern. The photo-acid are driven from the selected portions of the second relief pattern into portions of the fill material so that the portions of the fill material to become soluble to a predetermined developer.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 0.
Claims (20 — 2 Independent, 18 Dependent)
- Claim 1Independent Claim
A method of patterning a substrate, the method comprising: forming a first relief pattern including openings based on a first layer deposited over a substrate; filling the openings in the first relief pattern with a reversal material, containing a resin and a photo-acid generator, the resin being insoluble to a predetermined developer without any post-deposit treatment, and the resin being further insensitive to a photo-acid generated from the photo-acid generator in that the resin remains insoluble to the predetermined developer when the resin is in contact with the photo-acid without any post-deposit treatment; forming, on the substrate, a second relief pattern being an inverse pattern of the first relief pattern; depositing a fill material over the substrate and sensitive to the photo-acid generated from the photo-acid generator in that portions of the fill material that are in contact with the photo-acid become soluble to the predetermined developer; generating the photo-acid in selected portions of the second relief pattern via selective exposure to a light source, the photo-acid causing the portions of the fill material to become soluble to the predetermined developer.
- Claim 2Depends on #1
The method of claim 1, further comprising removing the portions of the fill material by using the predetermined developer so as to form a third relief pattern uncovering an underlying layer that is positioned between the substrate and the fill material.
- Claim 3Depends on #2
The method of claim 2, further comprising: transferring the third relief pattern into the underlying layer through an etching process.
- Claim 4Depends on #1
The method of claim 1, wherein the portions of the fill material to become soluble to the predetermined developer are caused by diffusing the photo-acid a predetermined distance into the fill material by a diffusion process through the interfaces between the selected portions of the second relief pattern and the fill material.
- Claim 5Depends on #1
The method of claim 1, wherein the forming the first relief pattern includes exposing the first layer to a second actinic radiation that forms a latent pattern, and developing the latent pattern through a developer to form the first relief pattern.
- Claim 6Depends on #1
The method of claim 1, wherein the first layer is a layer of photoresist.
- Claim 7Depends on #1
The method of claim 1, wherein the filling the openings in the first relief pattern includes depositing an overburden of the reversal material and removing the overburden of the reversal material.
- Claim 8Depends on #1
The method of claim 1, wherein the fill material is free of the photo-acid generator.
- Claim 9Depends on #1
The method of claim 1, wherein the portions of the fill material to become soluble to the predetermined developer are caused by applying a thermally activated diffusion process to drive the photo-acid.
- Claim 10Depends on #9
The method of claim 9, wherein the thermally activated diffusion process includes heating the substrate at a predetermined temperature and for a predetermined duration.
- Claim 11Depends on #1
The method of claim 1, wherein the fill material includes a de-protection group that causes the fill material to become soluble in a presence of the photo-acid.
- Claim 12Independent Claim
A method of patterning a substrate, the method comprising: forming a first relief pattern that including openings based on a first layer deposited over a substrate; filling the openings in the first relief pattern with a resin being insensitive to a solubility-changing agent in that the resin remains insoluble to a predetermined developer when the resin is in contact with the solubility-changing agent without any post-deposit solubility-neutralizing treatment; forming a second relief pattern being an inverse pattern of the first relief pattern; depositing a fill material on the second relief pattern, and sensitive to the solubility-changing agent generated from a generator compound in that portions of the fill material that are in contact with the solubility-changing agent become soluble to the predetermined developer; exposing selected portions of the second relief pattern to generate the solubility-changing agent in the selected portion of the second relief pattern; and driving the solubility-changing agent generated in the selected portions of the second relief pattern to diffuse from the selected portions of the second relief pattern into portions of the fill material through interfaces between the selected portions of the second relief pattern and the fill material, the solubility-changing agent causing the portions of the fill material to become soluble to the predetermined developer.
- Claim 13Depends on #12
The method of claim 12, wherein the solubility-changing agent includes a photo-acid.
- Claim 14Depends on #12
The method of claim 12, wherein the solubility-changing agent includes a photo destructive base.
- Claim 15Depends on #13
The method of claim 13, wherein the generator compound is a photo acid generator (PAG) that generates the photo-acid in response to exposure to an actinic radiation.
- Claim 16Depends on #14
The method of claim 14, wherein the generator compound is a photo destructive base generator that generates the photo destructive base in response to exposure to an actinic radiation.
- Claim 17Depends on #12
The method of claim 12, wherein the driving the solubility-changing agent generated in the selected portions of the second relief pattern to diffuse from the selected portions of the second relief pattern into the portions of the fill material includes applying a thermally activated diffusion process by controlling an average diffusion length of the solubility-changing agent.
- Claim 18Depends on #12
The method of claim 12, wherein the generator compound includes a thermal acid generator (TAG).
- Claim 19Depends on #18
The method of claim 18, wherein the thermal acid generator comprises sulfonate esters that are derived from oximes, imides and benzyl alcohols.
- Claim 20Depends on #12
The method of claim 12, wherein the fill material is free of the generator compound.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS This application is a continuation of U.S. application Ser. No. 17/221,416 filed on Apr. 2, 2021, now U.S. Pat. No. 11,682,559, which is based upon and claims the benefit of priority from U.S. Provisional Application No. 63/037,798 filed on Jun. 11, 2020, the entire contents of which are incorporated herein by reference. FIELD OF THE INVENTION This invention relates to microfabrication including microfabrication of integrated circuits as well as processes involved in patterning semiconductor substrates. BACKGROUND In material processing methodologies (such as photolithography), creating patterned layers typically involves the application of a thin layer of radiation-sensitive material, such as photoresist, to an upper surface of a substrate. This radiation-sensitive material is transformed into a patterned mask that can be used to etch or transfer a pattern into an underlying layer on a substrate. Patterning of the radiation-sensitive material generally involves exposure by a radiation source through a reticle (and associated optics) onto the radiation-sensitive material using, for example, a photolithographic exposure system. This exposure creates a latent pattern within the radiation-sensitive material which can then be developed. Developing refers to dissolving and removing a portion of the radiation-sensitive material to yield a relief pattern (topographic pattern). The portion of material removed can be either irradiated regions or non-irradiated regions of the radiation-sensitive material depending on a photoresist tone and/or type of developing solvent used. The relief pattern can then function as a mask layer defining a pattern. Preparation and development of various films used for patterning can include thermal treatment or baking. For example, a newly applied film can receive a post-application bake (PAB) to evaporate solvents and/or to increase structural rigidity or etch resistance. Also, a post-exposure bake (PEB)
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (15)
| Patent | Title | Year | Citations |
|---|
Non-Patent Literature (4)
- International Search Report and Written Opinion of the International Searching Authority issued Aug. 25, 2021 in PCT/US2021/030927, citing documents AA-AJ therein, 8 pages.
- Japanese Office Action issued Dec. 10, 2024 in Japanese Patent Application No. 2022-575929 (with English Translation), citing references 1 and 15-16 therein, 17 pages.
- Korean Office Action dated Jul. 28, 2025, in Korean Patent Application No. 10-2023-7000237, filed Jan. 3, 2023, w/English translation, 18 pages.
- Office Action issued Apr. 15, 2025 in Japanese Patent Application No. 2022-575929 with English translation, 4 pages.