Neodymium-iron-boron magnet material, raw material composition preparation method, and application

0Forward Citations (#3378186 Global)
0.0/yrCitation Velocity (#3378186 Global)
0.00Citation PageRank (#3378186 Global)
14Prior Art Cited
8Claims (1 Indep. · 7 Dep.)
0Drawings / Sheets

Abstract

Provided are a neodymium-iron-boron magnet material, raw material composition, preparation method, and application. The raw material composition of the neodymium-iron-boron magnet material comprises the following mass content components: R: 28-33%; R is a rare earth element, R comprises R1 and R2; R1 is a rare earth element added during smelting, and R1 comprises Nd and Dy; R2 is a rare earth element added during grain boundary diffusion, R2 comprises Tb, the content of R2 is 0.2%-1%; Co: < 0.5%, but not 0; M: ≤ 0.4%, but not 0, and M is one or more of Bi, Sn, Zn, Ga, In, Au, and Pb; Cu: ≤ 0.15%, but not 0; B: 0.9-1.1%; Fe: 60-70%; the percentage is the mass percentage of the mass of each component to the total mass of the raw material composition. The neodymium-iron-boron magnet material has high remanence, coercivity, and good thermal stability.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (8 — 1 Independent, 7 Dependent)

  1. Claim 1Independent Claim

    A neodymium-iron-boron magnet material, which comprises the following components by mass percentage: R: 28-33%; R comprises R1 and R2, R1 comprises Nd and Dy, R2 comprises Tb, the content of R2 is 0.2%-1%; the content of Dy in R1 is 0.05-0.3%; Co: 0.05-0.45%; M: ≤ 0.4%, but not 0, M is at least one element selected from group consisting of Bi, Sn, Zn, Ga, In, Au, and Pb; Cu: ≤ 0.15%, but not 0; B: 0.9-1.1%; Fe: 60-70%; C; and O; the percentage is the mass percentage of the mass of each component to the total mass of neodymium-iron-boron magnet material; the neodymium-iron-boron magnet material comprises Nd 2 Fe 14 B grains and their shells, and two-grain intergranular boundary and grain boundary triangle region adjoining to the Nd 2 Fe 14 B grains; wherein, heavy rare earth elements in R1 are distributed in Nd 2 Fe 14 B grains, R2 is mainly distributed in the shell, two-grain intergranular boundary and grain boundary triangle region, the area proportion of the grain boundary triangle r

  2. Claim 2Depends on #1

    The neodymium-iron-boron magnet material according to claim 1, wherein, the neodymium-iron-boron magnet material satisfies any one of the following schemes: scheme 1: the content of R is 29.5-32.6%; R1 is rare earth element added during smelting; R2 is rare earth element added during grain boundary diffusion, the content of R2 is 0.2%-0.9%; the content of M is 0.35% or less, but not 0, M is at least one element selected from group consisting of Ga, Bi, and Zn; the content of Cu is 0.05-0.15%; the content of B is 0.97-1.05%; the content of Fe is 65-69.5%; the area proportion of the grain boundary triangle region is 1.98-2.78%; the continuity of the two-grain intergranular boundary is 97% or more; the mass proportion of C and O in the grain boundary triangle region is 0.41-0.49%, the mass proportion of C and O in the two-grain intergranular boundary is 0.32-0.41%; in the new phase with the chemical composition of R x (Fe+Co) 100-x-y-z Cu y M z; wherein, R in the R x (Fe+Co) 100-x-y-z Cu

  3. Claim 3Depends on #1

    A magnet steel, which is prepared using the neodymium-iron-boron magnet material according to claim 1.

  4. Claim 4Depends on #1

    The neodymium-iron-boron magnet material according to claim 1, wherein, x is 42.33-43.57, y is 0.23-0.35, z is 0.27-0.41; or, the ratio of the area of the new phase in the two-grain intergranular boundary to the total area of the two-grain intergranular boundary is 0.24-2.2%.

  5. Claim 5Depends on #1

    The neodymium-iron-boron magnet material according to claim 1, wherein, the content of Nd in R1 is 28.5-32.5%; or, R1 further comprises at least one element selected from the group consisting of Pr, Ho, Tb, Gd, and Y; or, R2 further comprises at least one element selected from the group consisting of Pr and Dy; or, Cu has been added to the material during smelting or during grain boundary diffusion.

  6. Claim 6Depends on #5

    The neodymium-iron-boron magnet material according to claim 5, wherein, when R2 comprises Pr, the content of Pr is 0.2% or less, but not 0; or, when R2 comprises Dy, the content of Dy is 0.3% or less, but not 0.

  7. Claim 7Depends on #1

    The neodymium-iron-boron magnet material according to claim 1, wherein, M is at least one element selected from the group consisting of Zn, Ga, and Bi; or, the neodymium-iron-boron magnet material further comprises Al.

  8. Claim 8Depends on #7

    The neodymium-iron-boron magnet material according to claim 7, wherein, the content of Al is 0.3% or less, but not 0.

Technical Overview & Description

The present application is a National Stage of International Application No. PCT/CN2021/077178, filed on Feb. 22, 2021, which claims priority of the Chinese Patent Application No. CN202010121798.0 filed on Feb. 26, 2020, the contents of which are incorporated herein by reference in their entireties. TECHNICAL FIELD The present disclosure relates to a neodymium-iron-boron magnet material, a raw material composition, a preparation method, and application. BACKGROUND Nd — Fe — B permanent magnet material with the advantages of high magnetic performance, small thermal expansion coefficient, easy processing and low price is based on Nd 2 Fe 14 B compound matrix. Since its appearance, Nd — Fe — B permanent magnet material increased at an average rate of 20-30% per year, and it has been the most widely used permanent magnet material. Classified by preparation method, Nd — Fe — B permanent magnets can be divided into three types: sintering, bonding and heat pressure. Herein, sintering magnets account for 80% or more of the total output, and its use is the most widely. With the continuous optimization of the preparation process and magnetic component, the maximum magnetic energy product of sintering Nd — Fe — B magnet is close to the theoretical value. With the booming development of emerging industries such as wind power, hybrid vehicles, and inverter air conditioners in recent years, the demand for high-performance Nd — Fe — B magnets has become greater and greater. At the same time, these high-temperature field uses also put forward higher requirements for performance of the magnets, especially the coercivity. The U.S. patent application U.S. Pat. No. 5,645,651A shows that the curie temperature of Nd — Fe — B magnet increases with the increase of Co content through FIG. 1 . In addition, by the comparison of sample 9 and sample 2, table 1 shows that adding 20 at % of Co to the Nd — Fe

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (14)

PatentTitleYearCitations

Non-Patent Literature (6)

  • English translation of CN 111261355 (originally published Jun. 9, 2020), obtained from PE2E search.
  • English translation of WO 2021244321 (originaly published Dec. 9, 2021), obtained from PE2E search.
  • English translation of Chinese priority application No. 202010121798.0 , filed Feb. 26, 2020.
  • Apr. 29, 2021 International Search Report issued in International Patent Application No. PCT/CN2021/077178.
  • Apr. 29, 2021 Written Opinion of the International Searching Authority issued in International Patent Application No. PCT/CN2021/077178.
  • Chinese priority application No. CN202010121798.0 (not published) , filed Feb. 26, 2020.